samnus Posted March 18, 2014 Report Share Posted March 18, 2014 I'm interested in the many ways that potters use to sign their pots...on greenware or bisqueware, carving name & filling with oxides or stains, just brush signing...and the details. Also, whether or not to include the date. Thanks Link to comment Share on other sites More sharing options...
TJR Posted March 18, 2014 Report Share Posted March 18, 2014 I sign all my work with a brush and oxide-but I also decorate all my work with brush and oxide. I do not write the date, as there is always some ckunker hiding in a box that you can sell. If people think that it is old work, they wonder why it didn't sell. Tom. Link to comment Share on other sites More sharing options...
neilestrick Posted March 18, 2014 Report Share Posted March 18, 2014 I have a stamp, made of of clay and bisque fired. I put a little BB of clay on the pot and stamp it down. Link to comment Share on other sites More sharing options...
ChenowethArts Posted March 18, 2014 Report Share Posted March 18, 2014 I have a stamp that identifies a series/class of work, but just about everything carries my initials and a crosshatch pattern on the bottom...stained with red iron oxide after bisque fire: Link to comment Share on other sites More sharing options...
clay lover Posted March 18, 2014 Report Share Posted March 18, 2014 I made a stamp from my signature and bisque it for the basic things. For larger, more spendy pieces, I hand sign. Link to comment Share on other sites More sharing options...
Chilly Posted March 18, 2014 Report Share Posted March 18, 2014 There's been a couple of threads recently: http://community.ceramicartsdaily.org/topic/2390-hangtags/?hl=%2Bsigning+%2Bpots&do=findComment&comment=17999 http://community.ceramicartsdaily.org/topic/4964-ooopsi-forgot-to-sign-my-pot/?hl=%2Bsign+%2Bbottom+%2Bpot Link to comment Share on other sites More sharing options...
Tarheeler Posted March 18, 2014 Report Share Posted March 18, 2014 I use a stylus to put in my initials after I trim. Eventually I'll get around to making a stamp for it. Link to comment Share on other sites More sharing options...
Brian Reed Posted March 18, 2014 Report Share Posted March 18, 2014 I follow the Leach tradition (I know it is really a Japanese, but I learned if from Leach) of making a stamp and bisque firing it. I then use it to press into leather hard clay. I make sure that when I glaze no glaze touches the stamped area. Link to comment Share on other sites More sharing options...
Mark C. Posted March 19, 2014 Report Share Posted March 19, 2014 I'm the odd man out as I use the dull end of a metal pro needle tool (the butt end) to sign the work right after triming or sponging. I did date them randomly thru1969-1986 Now I do not date them. I have two signatures as well. One is Cort which is very fluid the other is LHP all letters combined as a studio signature Like to keep the folks guessing Mark Link to comment Share on other sites More sharing options...
Pres Posted March 19, 2014 Report Share Posted March 19, 2014 I use a pencil or wooden rib to sign through a piece of plastic shopping bag-no burr. I also stamp an Old English "R" from letter press. I date everything, but then don't worry about sales that much. I can see how dating -dates your stuff. No one wants last year, or 10 years ago unless of course they are a collector, or just like your work. Lately I have been getting fancier with the signature with an incised line with interlaced squiggles at the ends forming a spot for the "R". Link to comment Share on other sites More sharing options...
Benzine Posted March 19, 2014 Report Share Posted March 19, 2014 Pres, they will need the dated work, for future editions of Antique Roadshow.... I sign my work, usually with a wooden thumb tool, or if I don't have it on hand, the point of a needle or wood tool. Link to comment Share on other sites More sharing options...
PSC Posted March 19, 2014 Report Share Posted March 19, 2014 I use my needle tool, i don't date it as some shoppers seem to think its the pot's expiration date but i have found it handy to put the cone i am going to fire it to on the bottom then i don't get my low fire and high fire bisque mixed up. I started to add the cone after hurricane charley destroyed my studio in 2004. My shelves collapsed and i couldn't tell the lowfire from high fire from each other in the pile that survived the fall. When i started making again 3 years later i started adding the cone. Link to comment Share on other sites More sharing options...
Babs Posted March 19, 2014 Report Share Posted March 19, 2014 Old biro when I trim, on larger stuff i use a fine line pen with black slip inside. Is time consuming so I may go to a stamp soon. Link to comment Share on other sites More sharing options...
ayjay Posted March 19, 2014 Report Share Posted March 19, 2014 I've made a couple of stamps, but rarely use them, my usual method is to initial the bottom just after trimming - I use a Porcupine quill, it lives with my trimming tools so I don't have to use a needle which will then get left in the wrong place. Link to comment Share on other sites More sharing options...
samnus Posted March 21, 2014 Author Report Share Posted March 21, 2014 Thanks for the input and variety of ways to approach signing a pot...I guess I was making it harder than it needed to be...by scribing, sanding, filling with underglaze and then wiping off the excess ;o( Link to comment Share on other sites More sharing options...
claygram Posted March 21, 2014 Report Share Posted March 21, 2014 I have some pieces of lead type saved from when my Dad had a one-man printing business in our home. He set all his type by hand--this was 75 years ago and he had learned from his father when he was young. I have my two initials and a small design that I just press into the clay when I finish trimming. It always brings back good memories and keeps him part of my life. Link to comment Share on other sites More sharing options...
Rebekah Krieger Posted March 21, 2014 Report Share Posted March 21, 2014 I use the rubber sculpting blending tool thing (not sure the name)… this week at nceca somebody mentioned that they put a black spot of slip in the bottom of their pots, and then carve out their name (write with needle tool probably) Link to comment Share on other sites More sharing options...
Biglou13 Posted March 22, 2014 Report Share Posted March 22, 2014 Sharpened pencil After trimming I've used a stamp in past For now it feels more personal to actually "sign" with my mark Sometimes need to be hit with diamond pad to smooth down after bisque I usually just hold my pots and dip leaving finger marks. Some get covered sometime not. I ve been doing this x3 on bottom of most pieces The 5 lines while minimalist are my initials. LEC While not as bold part of the inspiration came from koie ryoji, where his bold signature sometimes part of the decoration of pot. Link to comment Share on other sites More sharing options...
clayshapes Posted March 22, 2014 Report Share Posted March 22, 2014 I just started using Designer Liner (Mayco) to cursively sign my work. It's pigment only, so doesn't stick to the kiln shelf when you fire it. Link to comment Share on other sites More sharing options...
Guest JBaymore Posted March 23, 2014 Report Share Posted March 23, 2014 For high end work...... this etching and inlaying slip and such samnus mentions is the kind of stuff that adds that "little extra" pizazz. WELL worth the little extra time and fussing. For some of the higher end pieces I make, I sometimes also use painted overglaze enamel or burnish gold luster. Has to "fit" the nature of the piece. I use JBaymore in script almost all the time for this kind of thing. For a lot of stuff, I sign my name in the leatherhard clay with a DULL pencil, or a ball point pen. Prominent and readable. Sharp points like needle tools tend to leave a "harsh" quality to the mark after work is fired. On some pieces I use a stone hanko (stamp) that I carved in Mashiko, Japan in 1996 (over a lot of sake with a potter friend). It is a stylized JB. I press it into the clay or into a small wet wad of clay. For my Chadogu (formal teawares) it varies by the type of piece. Chawan and mizusashi and things like kogo and furo and serving pieces usually get JBaymore in the leatherhard clay outside the footring (never inside). Chaire (being very small) often get a stamped JB or an overglaze or gold one usually on the lower sidewall near the foot. Chadogu almost always also get a signed (in black ink) wooden box, with my ceramic hanko, my legal signature hanko (last name in Kanji) and the kiln name hanko in red ink. They also get a yellow-orange wrapping cloth for the piece with the same three hanko in red. best, ..................john PS: At the 2014 NCECA fund raising cup sale I donated a Chawan (with box, etc.). I set it at 1/2 of my usual price. Everything sold....... so .......did anyone here happen to get that piece? Curious. BTW... the cup sale raised almost $25,000 for scholarships in only a few hours of actual sales. NICE! Link to comment Share on other sites More sharing options...
Stellaria Posted March 24, 2014 Report Share Posted March 24, 2014 I made a wooden stamp by carving with a dremel, and use that somewhere on my pieces. It's a celtic spiral design that resembles a raven. It's big, though, and tends to deform my work if I'm not careful, so I need to figure out how to make a smaller one. I'll probably carve one from clay, even though carving clay tends to piss me off. I don't like to sign my pots. I'm not entirely sure why. I always get the feeling I'm "doing it wrong" which is really stupid, I know. Writing my name on the bottom feels weird, and I think my signature looks too plain anyway. So far, the only pieces that get marked consistently are mugs, because I stamp into the fishtail join on the handle...which, incidentally, looks pretty dang cool. Link to comment Share on other sites More sharing options...
Rebekah Krieger Posted March 24, 2014 Report Share Posted March 24, 2014 For high end work...... this etching and inlaying slip and such samnus mentions is the kind of stuff that adds that "little extra" pizazz. WELL worth the little extra time and fussing. For some of the higher end pieces I make, I sometimes also use painted overglaze enamel or burnish gold luster. Has to "fit" the nature of the piece. I use JBaymore in script almost all the time for this kind of thing. For a lot of stuff, I sign my name in the leatherhard clay with a DULL pencil, or a ball point pen. Prominent and readable. Sharp points like needle tools tend to leave a "harsh" quality to the mark after work is fired. On some pieces I use a stone hanko (stamp) that I carved in Mashiko, Japan in 1996 (over a lot of sake with a potter friend). It is a stylized JB. I press it into the clay or into a small wet wad of clay. For my Chadogu (formal teawares) it varies by the type of piece. Chawan and mizusashi and things like kogo and furo and serving pieces usually get JBaymore in the leatherhard clay outside the footring (never inside). Chaire (being very small) often get a stamped JB or an overglaze or gold one usually on the lower sidewall near the foot. Chadogu almost always also get a signed (in black ink) wooden box, with my ceramic hanko, my legal signature hanko (last name in Kanji) and the kiln name hanko in red ink. They also get a yellow-orange wrapping cloth for the piece with the same three hanko in red. best, ..................john PS: At the 2014 NCECA fund raising cup sale I donated a Chawan (with box, etc.). I set it at 1/2 of my usual price. Everything sold....... so .......did anyone here happen to get that piece? Curious. BTW... the cup sale raised almost $25,000 for scholarships in only a few hours of actual sales. NICE! I was very close to buying your bowl. IT was gorgeous! I came back mid sale and noticed that my cup was still there so I vowed not to go back in case i would see my cup as the last remaining one… that was my biggest fear. Link to comment Share on other sites More sharing options...
alabama Posted April 2, 2014 Report Share Posted April 2, 2014 Hey, I sign my name and date backwards with a fine needle tool, homemade from a blow gun dart. On the left of the bottom, I put the cone its fired to and on the right of the bottom I put the pounds needed to make the vessel. If the vessel is a copy of something colonial, then I put the country and date it would have been used...i.e. Germany 1675 or Belgium 1550 or British 1725..just whatever the archaeological date is. If the pottery is not a referenced copy then my name and date (backwards), cone, and pounds are incised on the bottom. After the pottery is bisqued, the bottom it is stained with a wash of black iron oxide. On American Indian replicas I just sign my name regular and date on the inside of the vessel sice they aren't glazed.. I just wanted to sign differently on two types of pottery. And this works for me. :>) See you all later, Alabama Link to comment Share on other sites More sharing options...
Nancy S. Posted April 3, 2014 Report Share Posted April 3, 2014 I carved a "sigil" that incorporates my initials into a plaster bat, then pressed a bit of clay into that to form a stamp that was bisque fired. The past few years I've used a date (also a bisqued stamp that I made from carved plaster), but obviously that necessitates a new date stamp every year, so I'm pondering that a lot lately. I don't sell a lot; most of what I make is for me and my family. And they don't really care when it was made anyway! I like using the stamp, because it makes for a clean, incised line that is also consistent. I started out hand-carving the sigil, but sometimes it didn't come out right, sometimes it was too deep or too shallow, etc. Link to comment Share on other sites More sharing options...