High Bridge Pottery reacted to Jessica2023 in Electrician cut off my brand new kiln plug without asking…
So here’s the new plug, you can see how they shaved off the cord exterior. The original plug was obviously the same color as the cord, not black. Talked to the business I bought the kiln from and they agreed the electricians had no reason to do this and should take responsibility for it. The owner of the electrician business bought me a new skutt kiln power cord and is ordering the correct receptacle and will install both on Monday. Thank you for your insights, very much appreciated!! Still can’t believe they cut my plug off lol!!
-
High Bridge Pottery reacted to elenab in Kiln is not reaching cone 6 temperature
Hi High Bridge and everyone! I am back with good news! last week I did firing with the new elements we made and my kiln reached cone 6 temperature in 4.5 hr, yay...
I didn't buy 12 g wire, it was too expensive, instead, I bought 14 g, cut enough wire to make 8 ohms for each element, winded it, then stretched it to the length we needed, and installed it. Accidentally, the rod I was winding the wire on had a perfect size and fit perfectly. Later I realized that if the rod was bigger I would not be able to insert the elements in the grooves.
Changing the elements was so much simpler than I feared. I probably was reading F.Olsen's book too much, lol. But after all the self-doubt I made my kiln work, and thank you for your support!
Elena
-
High Bridge Pottery reacted to Callie Beller Diesel in Slip Base by Susan Feagin question
If you’re wanting to mix a large master batch that then gets divided out, leave out the dry mixing entirely, but weigh the water. If you know how much water went into the batch you can divide it out evenly. If you keep to metric measurements, this will be easier, because 1 ml of water weighs 1 gram. It doesn’t work like that for all fluids, but it does for water. If you are used to using a measuring cup, check how accurate it is by filling it to a given measurement line and weighing it to make sure it’s close enough for your purposes.
For instance, if you add 2500 g of water to your 5000g batch, the whole thing will weight 7500g, so a quantity of slip that weighs 1500g will contain 1000g of slip base. (Numbers made up off the top of my head for ease. You may have to play with your water additions to get your consistency right. Just record what you did.)
From there, you can add your colourants to portions of your master batch. To mix thoroughly, you will need to use a stick blender that rotates really fast. If you use something slower like a jiffy mixer, you’ll have to let it mix a lot longer to get everything distributed properly. For some colourants that don’t break up easily, you may have to sieve the mix again.
-
High Bridge Pottery reacted to Bill Kielb in Was it a mistake to pass on an old kiln?
From what I can see, these tests appear to not report false positive below 1mg / cm2 with 95% confidence. I guess we need to define “trace” amounts that would constitute not having lead.
Some info from the EPA https://www.epa.gov/lead/hazard-standards-and-clearance-levels-lead-paint-dust-and-soil-tsca-sections-402-and-403
Allowable levels of dust are fairly low with an emphasis to not aerosolize lead by heating, scraping etc…..
-
High Bridge Pottery got a reaction from KellySnider in Confused Newbie w/new Skutt 818-3
If you put a cone04 in a cone5 firing you will probably end up with it sticking to the shelf unless you are making a cone pack with a bit to catch the melted cones in. Turned out useful for problem solving this time but I wouldn't normally include an 04 unless you make something to catch the melting cone that's not your shelves.
-
High Bridge Pottery reacted to Bill Kielb in Was it a mistake to pass on an old kiln?
I think in the states 1mg per cm2 for surface transfer limits so test kits are likely to detect in this range. Correlating surface transfer to absorption likely extremely difficult though. I am not aware of any amount of lead though that folks would say is fine after polluting the whole planet with low levels of the stuff. The argument at that time for a time evolved to is it is such a “tiny amount” …… See link above for an interesting accounting IMO
-
High Bridge Pottery reacted to Callie Beller Diesel in Was it a mistake to pass on an old kiln?
@High Bridge Potterymostly they’re meant for things like antique/vintage housewares and detecting lead paint. They measure anything you can dissolve with the reagent supplied. So if there’s some lead there but it doesn’t dissolve, or if it’s below a certain amount, you could get a false negative from the home kits. They’re only meant for a quick yes/ no answer.
-
High Bridge Pottery got a reaction from Rae Reich in Confused Newbie w/new Skutt 818-3
If you put a cone04 in a cone5 firing you will probably end up with it sticking to the shelf unless you are making a cone pack with a bit to catch the melted cones in. Turned out useful for problem solving this time but I wouldn't normally include an 04 unless you make something to catch the melting cone that's not your shelves.
-
High Bridge Pottery got a reaction from Babs in Confused Newbie w/new Skutt 818-3
It sounds like you are saying the 04 firing cones are not right but they sound bent the right amount to me. Are you sure you did a cone5 firing and not cone05 as having the 04 start to bend sounds like you did cone05 by mistake.
-
High Bridge Pottery got a reaction from KellySnider in Confused Newbie w/new Skutt 818-3
It sounds like you are saying the 04 firing cones are not right but they sound bent the right amount to me. Are you sure you did a cone5 firing and not cone05 as having the 04 start to bend sounds like you did cone05 by mistake.
-
High Bridge Pottery got a reaction from Callie Beller Diesel in Help with choosing my first kiln!
I could certainly get by with a 4 segment program and £400~ extra just for more segments seems like a rip off unless it has more extra features.
My typical bisque would be 200c per hour to 100c then hold at 100c for 30 min. 150c per hour to 1000c then hold at 1000c for 20 min which would be the 4 segments.
A glaze firing doesn't really need the first hold so for a cone 10 firing it would be 250c per hour to 1180c then 60c per hour to 1280c and a 20 min hold at 1280c. You don't have to hold at the end but they can help to even out the temperature in the kiln. You would change the last ramp segment depending on which cone you want as cones are specified as a rate of climb (either 60c per hour or 150c per hour) for the last 100c of firing to a certain temperature.
250c per hour to 1180c may be too much for thick work or large platters and end up cracking them so something like 100-150c per hour would be better.
You could even add a controlled cool to the glaze firing as my example above is only 3 segments. Cooling slower than just turning the kiln off is good for crystal growth, if you are looking to get into proper crystaline glazes then I would probably go with the 20 segment. Not something I have tried myself but I have read they need very particular firing profiles on the way up and down to get big crystals.
In the end it all depends on how you like to fire. More segments will give you more ways to try and solve issues with your clay and glazes but from my experience you never need the firings to be overly complicated with different ramp rates and holds.
-
High Bridge Pottery reacted to PeterH in Cress B23H kiln 240 V element questions
Looks like it's here http://www.cressmfg.com/wp-content/uploads/B23H-240-VAC.pdf
PS Broken link showed as
... and a google search for "B23H 240" (with the quotes) found it (even though access to the enclosing directory https://www.cressmfg.com/wp-content/uploads/ is forbidden).
-
High Bridge Pottery got a reaction from Hulk in Confused Newbie w/new Skutt 818-3
It sounds like you are saying the 04 firing cones are not right but they sound bent the right amount to me. Are you sure you did a cone5 firing and not cone05 as having the 04 start to bend sounds like you did cone05 by mistake.
-
High Bridge Pottery reacted to k77 in White raised bumps after glaze firing
Hi all,
A quick update. I sanded the pots and refired. The bumps were white and hard in texture. Somewhat difficult to remove. I was able to cover them with glaze, but the finished results (where my brush strokes are visible) are not to my liking.
I have put a fresh load in the kiln today (that I glazed a few days ago). I noticed when putting them in that there were some hard dots on one of the plates. These wouldn't bother me in a dipping glaze (they would melt and blend in) but I'm wondering if in Stroke and Coat, with its lack of movement, these are the culprit? Maybe they are bits of dry glaze that I've picked up during a long painting session? Maybe they are small pieces of dry glaze from the bottle (I do try and get every last bit out!)
So, my working theory for now is that these lumps may actually be from the glaze. This time I've rubbed them out with my finger before firing. Hopefully I'll see better results after this firing!
K
-
High Bridge Pottery got a reaction from Hulk in White raised bumps after glaze firing
I think it's just an optical illusion making them look like craters. If you look at the rim in the lower right the light source is also coming from that direction and the rim is casting a shadow onto the plate.
They don't particularly look like blisters to me. I am guessing you would have noticed all the bumps when glazing if it was some chunks in the glaze but worth sieving through 120mesh just to make sure. Maybe you caught a kiln brick putting a shelf in and knocked some debris onto the ware? You could try sanding them, might give you an idea if they are solid chunks or filled with air?
-
High Bridge Pottery got a reaction from JohnnyK in Forums page layout
I think it looks a lot better, less cluttered and better formatted giving you the 5 most recently updated topics instead of 5 newest posts which could all be in the same topic.
-
High Bridge Pottery got a reaction from LeeU in Forums page layout
I think it looks a lot better, less cluttered and better formatted giving you the 5 most recently updated topics instead of 5 newest posts which could all be in the same topic.
-
High Bridge Pottery got a reaction from Kelly in AK in Mason Stains in Porcelain Slip
In my recent glaze tests I have found 20% kaolin 80% frit will suspend really well for at least a few weeks to a month whereas 10% kaolin 90% frit will be trying to hard pan in about 12 hours.
-
High Bridge Pottery reacted to Hulk in Forums page layout
Ah!
Thanks Johnny, thanks HB!
How's it look now?
The Activity Stream has been replaced by a Topics widget/thingy.
-
High Bridge Pottery reacted to neilestrick in Custom Single-Page Underglaze Transfer?
I spent a couple of hours yesterday morning running some screen printing tests. I'm using a 110 mesh screen, Speedball underglazes, and raw Xuan paper. My findings:
- Speedball underglazes come fairly thick in the bottle, so with no modification they actually print pretty well for 1-2 prints. However, by the third print the underglaze would stop going through the screen and it would just print water. The thicker the underglaze the worse it got. If I washed off and dried the screen, then it would print again. I think the underglaze must be sealing up the screen.
- I don't have any guar gum or dextrin in the studio, but I do have CMC gum and Veegum T, which together are fabulous for suspending glazes and making them brushable. Typically I would make a syrup out of them, but I didn't want to add too much water to the underglaze so I mixed it up like thick snot- 2 tablespoons of CMC and 1 tablespoon of VGT to 1 1/2 pints of hot water (normally would use 1 gallon of water). Let it soak (overnight if you have time), and mix it with a stick blender.
I added 1 teaspoon of the snot to a pint of underglaze and ran a dozen prints without any problems. I also thinned out the underglazes a bit and was much happier with the thickness on the paper. No need to let them stiffen up at all. In fact, Speedball underglazes are a bit too thick in the bottle. I'd seen people say it should thicken up to a toothpaste consistency, but I didn't find that to be necessary or desirable.
- I was concerned that the CMC gum would make it more difficult to transfer, since in a typical application the gum makes the underglaze hard and resists water (which is why I always recommend applying underglazes to leather hard and bisque firing before glazing if you're working with dipping glazes). With the transfers they worked much, much better with the added gum. Great release from the paper. I lay the transfer on the leather hard pot, dab it with a wet sponge, then lightly roll it with a little brayer. I'm doing some bold patterns, not thin line work, so it's easy to control how complete the image transfers by how long I leave the transfer on the pot.
- The raw Xuan paper is very fragile when wet. You have to be very careful about rubbing it when it's sitting wet on the pot. I've got some half raw coming and I'll see if that holds up better.
EDIT: Forgot to add- I have tried making the transfers with newsprint before, but I don't like how much the paper wrinkles as it dries. The underglaze was also more likely to flake off when dry. I'll try it again with the new gum-added version later this week and see if it behaves any better. The good thing about the newsprint is that it's much more durable than the Xuan paper.
-
High Bridge Pottery reacted to Kelly in AK in Haptic Ceramics
All functional pottery is haptic. Feedback by touch.
-
High Bridge Pottery got a reaction from Callie Beller Diesel in Confused Newbie. Cone 6 base matte not firing as expected
FeO is certainly a much more powerful flux but Fe2O3 can help with melting. I don't think you are missing anything entirely, there's quite a fine line/small area of chemistry that will make a good matte glaze as you have found out by removing the iron oxide.
All the B2O3 Fe2O3 Al2O3 oxides are a bit weird and can act as fluxes and stabilisers. Can be called intermediate oxides or amphoteric oxides.
-
High Bridge Pottery got a reaction from Callie Beller Diesel in Unglazed pots and raku absorbed cigarette smell
Dunno if it would work but you could put them in a box with an ozone generator, just be careful not to breathe the O3.
-
High Bridge Pottery reacted to Bill Kielb in Confused Newbie. Cone 6 base matte not firing as expected
Nice! 0.3:0.7 is often considered an ideal range for likely durability. When the ratio departs significantly especially for excess alkali >0.3 it may not be durable. Some reading here: https://www.ceramicmaterialsworkshop.com/uploads/5/9/1/2/59124729/nceca_2012- @High Bridge Pottery (the glass former / flux debate emerges again)
So in and around that ideal range …..generally a decent ratio. 0.16 boron at cone 6 also good as shown by Katz and Dr Bill Carty, pretty linear findings below:
https://www.ceramicmaterialsworkshop.com/uploads/5/9/1/2/59124729/katz_tf_boroninglazes_0912.pdf
The Gloss line
Or matte line, in Stull which is relative - is a Si:Al of ratio of around 5:1 or less and is regional within Stull, trending toward gloss for his glaze at 7:1 and for him highest gloss.
so pretty good picks thus far, my question and caution was very high alumina levels and how did you get there. Things melt by composition though so as the alumina increases so likely does the cone it melts at. I could only find two similar mattes at 0.7 alumina so yours is interestingly high, higher than these and may not melt effectively at cone 6. Old forge below, Si:Al in the 4:1 range and 0.62 alumina.
so nice work, the worry would be its just under melted and testing it to cone 7 or 8 would yield a better melt. Still wondering how you got to 0.74 though.
Old Forge
Only two maybe three similar at 0.7 Al @ cone 6
-
High Bridge Pottery got a reaction from Bill Kielb in Confused Newbie. Cone 6 base matte not firing as expected
FeO is certainly a much more powerful flux but Fe2O3 can help with melting. I don't think you are missing anything entirely, there's quite a fine line/small area of chemistry that will make a good matte glaze as you have found out by removing the iron oxide.
All the B2O3 Fe2O3 Al2O3 oxides are a bit weird and can act as fluxes and stabilisers. Can be called intermediate oxides or amphoteric oxides.