neilestrick got a reaction from ChrisC in Kiln identification
If you measure the resistance of the elements you can calculate the amperage draw. AFAIK it's not a Paragon, although the color is different. Pacific Kiln is a company in California, which may or may not be the same company. Their web site doesn't show any studio size kilns, but it might be worth sending them an email.
-
neilestrick got a reaction from HenryBurlingame in L&L vs Cone Art Kilns
You can't go wrong with either one. They are very similar in construction aside from the element holders. Both have zone control, neither one requires element pins. The L&L will be easier to replace bricks, but if you're careful with your kiln you won't need to do that.
There's very little reason to fire to cone 10 in an electric kiln unless you're doing crystalline work. Glazes won't turn out the same as if fired in a gas kiln to cone 10, because most cone 10 glazes are made to fire in reduction. If your'e firing in oxidation, cone 6 is a much smarter way to go. Your kiln will last longer, your elements will last longer, and your firing and maintenance costs will be much lower. If you are going to do crystalline work, then the L&L JH model is the way to go. It's rated to cone 12, is built with K26 bricks, and has type S thermocouples, so it can handle the high temps much better.
Shop around for best pricing. 'Packages' aren't always the best deal. Since you're in Washington, I highly recommend calling Rob Battey at Northwest Potter's Supply if you go with the L&L. He's a great guy and has been providing tech support for L&L for years.
-
neilestrick got a reaction from HenryBurlingame in Gas or Electric Kiln For Starting Out
As I mentioned in your other thread, cone 10 in a gas kiln is not the same as cone 10 in an electric kiln. It's about atmosphere, not temperature. There is no difference between cone 6 electric and cone 10 gas in terms of durability or quality of work. There are a small handful of glaze types that require a reduction atmosphere for them to work, and therefore need a gas kiln, but other than that you can do just as much in an electric kiln. Cone 6 has the benefit of more stability with colors, and a lot more options with commercially available glazes. If you really like shino and tenmoku glazes, you need cone 10 reduction. They will not work in an electric kiln. If you don't have experience in firing a gas kiln, it's going to be a long hard learning curve, and a lot more expensive to get started. If you want faster success and a simpler process, go electric.
-
neilestrick got a reaction from Rae Reich in Is my bat the problem?
Also make sure your bat pins are tight.
-
neilestrick got a reaction from Rae Reich in Is my bat the problem?
The knocking is likely from the bat slipping. The oblong hole is not ideal, but that's how Brent makes them. There are other bats on the market that do not have oblong holes, like Northstar, but another solution is a BatMate or Bat Gripper. There's a few on the market but I know Xiem and Bailey both have a version. It's a think piece that sits under the bat and gives it more grip. My students love them.
-
neilestrick got a reaction from Magnolia Mud Research in Is my bat the problem?
Also make sure your bat pins are tight.
-
neilestrick got a reaction from Piedmont Pottery in Kiln trips breaker after replacing elements and power plug, but...
@davidh4976 Sounds like you got it figured out.
For future reference, and for others that may read this:
1. When the breaker trips immediately when the elements turn on, then there's a short in the system somewhere. Usually it's in the kiln, like a relay has melted out or a wiring connection has fried and there's a bare wire making contact with the kiln body, or it wasn't wired properly when you repaired it. In rare instances the short could be in the outlet or the wires from the outlet to the breaker.
2. When the breaker trips after the kiln has been on for a few minutes (or longer), then it's a breaker issue. Either the breaker is the wrong size, or it's old and worn out.
-
neilestrick reacted to davidh4976 in Kiln trips breaker after replacing elements and power plug, but...
I figured out what was causing this, but wanted to allow for a lot of firings to make sure. It turns out that inside the digital controller that I added, the 'wire-end' of the compression terminal on one of the internal wires was a bit too close to the controller's metal housing. I disassembled the controller (which was bought in one preassembled piece), and found signs of arcing. I put a good bend into the terminal, put everything back together, and have had no problems now over many, many firings.
-
neilestrick got a reaction from Roberta12 in High fire clear glaze over under glaze - cloudiness
Many commercial underglazes just don't hold up at cone 10. They start to flux out and that causes them to behave poorly when you put a glaze over them. If you're just looking for black or blue, you'd probably be better off making your own underglaze or slip. If you do want to use commercial underglazes, each color will need to be tested to see how it holds up and cone 10 and with your clear glaze.
-
neilestrick got a reaction from Pres in Purchasing a kiln for home studio use
Only very small kilns will run on 120V service. Any kiln of functional size will need 220/240 volts. The smallest kiln I would consider is an 18" wide model. But ideally a 23" wide model would be the most functional, as you can fit plates and serving bowls in it much easier. First thing to do is to take a look at the web sites of some kiln manufacturers in your area to get an idea of what's out there, and see what the electrical requirements are for the size of kiln you want. Then have an electrician check out your system to see what size circuit your system can handle. Minimum you'll need a 30 amp breaker, on up to 50 or 60 amps depending on the size of kiln you want. At £800 you'll have to buy used, but looking at the new ones will give you an idea of what you'll need to do as far as hooking it up. If the kiln is indoors, it will need to be vented, or at the very least have 2 windows that can create a cross draft with fans.
-
neilestrick got a reaction from Callie Beller Diesel in High fire clear glaze over under glaze - cloudiness
Many commercial underglazes just don't hold up at cone 10. They start to flux out and that causes them to behave poorly when you put a glaze over them. If you're just looking for black or blue, you'd probably be better off making your own underglaze or slip. If you do want to use commercial underglazes, each color will need to be tested to see how it holds up and cone 10 and with your clear glaze.
-
neilestrick got a reaction from Callie Beller Diesel in Dolomite mesh?
I'd go with the 325 unless it's really expensive compared to the other. The finer it is the easier it will enter the melt.
-
neilestrick got a reaction from Mark C. in Dolomite mesh?
I'd go with the 325 unless it's really expensive compared to the other. The finer it is the easier it will enter the melt.
-
neilestrick got a reaction from Kelly in AK in Beginner question re saggar firing
Another way to get some great colors is to use salt. Soak wood chips in a saturated salt water, let them dry, then use them in the saggar. It can give great red, yellow, and orange colors.
-
neilestrick got a reaction from Kelly in AK in Bisque firing frustrations
It's not about temperature, it's about heatwork, which is what cones measure. Setting it at 950C doesn't necessarily mean cone 08. It depends on the rate of climb of the final 100C degrees. If it's not hitting the cone, then it could be due to the rate of the final ramp, or simply that the system needs to be calibrated. You can do a thermocouple offset which will affect all temperatures, or a cone offset to change the final temp of a specific cone. Using the pre-programmed firing schedule (I'd use Medium speed) will give you a better idea of how accurately the system is firing compared to a custom schedule.
-
neilestrick reacted to Mark C. in Bread kloche bisque vs cone 6?
Laguna now sells a flameware body so you can get a 25# at Laguna/Aftosa location in Fl
-
neilestrick reacted to Kelly in AK in Bread kloche bisque vs cone 6?
Damn @neilestrick!!!
Best low fire work I’ve seen in a long time. So good I could eat it.
To @Biglou13, bisque anything will tolerate that kind of abuse better than a clay close to maturity. Lots of grog, kyanite, or even spodumene (gotten a bit expensive lately) will help. Unglazed flameware sounds better than any other clay body, but I haven’t tried that.
It can be done in the studio, ordinary clay products that handle the extreme temperature swings of cooking, but that’s far from saying it should be. I’ve made several earthenware pots that survive the stovetop, experimenting with clay formulations and bisque temperatures. Though I used them regularly, the maintenance was unforgiving (mold will not be denied if given a habitat to grow), and sooner or later they will fall apart despite all best practices. You didn’t bring this up, but I would never try to sell such a thing. Too complicated.
Pottery used for cooking is largely disposable, in places it’s actually used. Manufacturers like Le Creuset and Wiliams-Sonoma create ceramic ware that’s functional in a contemporary kitchen, but they are carefully engineered first world conveniences. If people can afford to use metal they do.
I’ll confess, I’ve never had better beans than those I cooked in clay pots. I don’t want to discourage anybody, I just think they should know what they’re in for.
-
neilestrick got a reaction from Hulk in Bread kloche bisque vs cone 6?
Hi @Biglou13 A flameware body would be your best bet for this. 500F is pretty hot for a clay dish, especially since you'll be dropping wet, room temp dough onto a hot, flat surface. It's a lot to ask of any clay body besides flameware. The other option is to just buy a cheap cast iron dutch oven on Amazon. It works great, and you don't have to worry about it cracking. My dutch oven is preheating in my oven as I type this!
My loaf from last week. 25% whole wheat, 80% hydration:
-
neilestrick got a reaction from Hulk in Clay breaking in kiln
That's a steam explosion from firing too fast for the thickness of the piece, or the piece still being too wet. Let the piece dry completely, do a preheat for a couple hours. Be sure to vacuum out all the clay crumbs from the elements.
-
neilestrick got a reaction from Kelly in AK in Bread kloche bisque vs cone 6?
Thanks @Babs! My bread game drastically improved during Covid lockdown. My 2 teenage boys and I were home every day for 3 months, and we went through 3 loaves a week. I figured out a lot with all that practice.
-
neilestrick got a reaction from Kelly in AK in Bread kloche bisque vs cone 6?
Hi @Biglou13 A flameware body would be your best bet for this. 500F is pretty hot for a clay dish, especially since you'll be dropping wet, room temp dough onto a hot, flat surface. It's a lot to ask of any clay body besides flameware. The other option is to just buy a cheap cast iron dutch oven on Amazon. It works great, and you don't have to worry about it cracking. My dutch oven is preheating in my oven as I type this!
My loaf from last week. 25% whole wheat, 80% hydration:
-
neilestrick got a reaction from Rae Reich in Gritty wheel head
First, why vinegar in the throwing water?
Usually when we see black on the wheel head it is simply a tiny bit of the aluminum abrading from the clay. Could just be the abrasion of the bat against the wheel. Does wiping it down not remove it?
-
neilestrick got a reaction from Pres in Gritty wheel head
First, why vinegar in the throwing water?
Usually when we see black on the wheel head it is simply a tiny bit of the aluminum abrading from the clay. Could just be the abrasion of the bat against the wheel. Does wiping it down not remove it?
-
neilestrick got a reaction from Callie Beller Diesel in Why does my Bone China have a Green tint?
I'm voting iron as well. I think that also accounts for the pinkish tint in low fire bisque pieces. If we were able to have a slab that thick of our clear glazes we would also see it to varying degrees. Window glass is also green for that reason. It look pretty darn clear when we look through it, but if you put some paint on it you'll see just how much color it really has. They make super clear glass, of course, but it's expensive. If I remember correctly they call it Water White glass. Standard plate glass and such is quite green. I worked for a glass shop for a few years after grad school, and we would occasionally have to replace opaque colored glass panels on buildings that were no longer available from the original supplier, so we just had to paint the backsides. Getting an accurate color match was nearly impossible due to the tinting effect of the green. You couldn't just have the paint color matched to the old panel.
-
neilestrick got a reaction from PeterH in PID small kiln
It's rate to just above cone 6, which means it'll only get to cone 6 maybe 50 times max before the elements need to be changed. Probably a lot less than that given the quality of the elements they are likely using. So to get any sort of real life from the elements you'll probably want to limit this to cone 2 at the most. Really we consider cone 6 kilns to be best suited for low fire work. I would definitely check to see if you can even get replacement elements for it.
It appears to be on angle iron legs, but they're not very tall. Most kilns have 8" legs, so this kiln is on the short side and it should definitely need to be placed on something fireproof. If it were mine, I wold put it higher up on some bricks to give more air flow under it, with a fireproof floor below.