davidh4976 Posted April 21 Report Share Posted April 21 Does the mesh level of dolomite make any difference in glazes? Pottery suppliers seem to offer both 200 and 325 mesh, but I've never heard of a difference for using either one. Quote Link to comment Share on other sites More sharing options...
neilestrick Posted April 21 Report Share Posted April 21 I'd go with the 325 unless it's really expensive compared to the other. The finer it is the easier it will enter the melt. Callie Beller Diesel and Mark C. 2 Quote Link to comment Share on other sites More sharing options...