Marcia Selsor got a reaction from Pyewackette for a gallery image, cone 6 Faux Celedon
Selsor Faux Celedon ^6 Oxidation
Whiting 18.5
Neph Syen 25.8
EPK 18.8
Silica 31.1
Gerstley B 4.6
98.8
Copper carb 0.3
Mason #6600 Black 0.02
-
Marcia Selsor got a reaction from Mark_H for a gallery image, FoilSagerLargedetail
Detail of the large orb's surface.
I keep firing them until I am happy with the results.
-
-
-
-
Marcia Selsor got a reaction from Shelly M for a gallery image, cone 6 Faux Celedon
Selsor Faux Celedon ^6 Oxidation
Whiting 18.5
Neph Syen 25.8
EPK 18.8
Silica 31.1
Gerstley B 4.6
98.8
Copper carb 0.3
Mason #6600 Black 0.02
-
-
-
-
Marcia Selsor reacted to Biglou13 for a gallery image, image
Slightly modified 12d* clay, Wood fired plate with; tuna, yellowtail, eel, white tuna aka escolar.......
-
Marcia Selsor reacted to Biglou13 for a gallery image, Zen practice/6/18/14.
I ve been away from wheel for a few weeks. Struggled with a few bowls a few days ago. I needed to go back and "practice". The first five were a struggle, some were a fight. I struggled with centering, I crashed a few on purpose, I crashed a few due to bad technique. Cylinders 6 - 17 found the zone they .........flowed.....they just. Happened!!
-
-
-
Marcia Selsor got a reaction from ChenowethArts for a gallery image, FoilSagerLargedetail
Detail of the large orb's surface.
I keep firing them until I am happy with the results.
-
Marcia Selsor got a reaction from ChenowethArts for a gallery image, obvara tan pair
two crackle surfaces
-
-
Marcia Selsor got a reaction from Denice for a gallery image, cone 6 Faux Celedon
Selsor Faux Celedon ^6 Oxidation
Whiting 18.5
Neph Syen 25.8
EPK 18.8
Silica 31.1
Gerstley B 4.6
98.8
Copper carb 0.3
Mason #6600 Black 0.02
-
Marcia Selsor reacted to Marc McMillan for a gallery image, ferric chloride with miracle grow fuming
-
Marcia Selsor reacted to meghanmuir for a gallery image, Vase
Burnished and pit-fired, different view
-
Marcia Selsor got a reaction from Babs for a gallery image, ObvaraBigcracks copy
experimenting with textured surfaces for Obvara firings
-
Marcia Selsor got a reaction from Babs for a gallery image, Obvaracracklesurface copy
experimenting with textured surfaces for Obvara firings
-
-
-
Marcia Selsor got a reaction from Cuny for a gallery image, Obvarainvertedlip copy
fired 8/27 Obvara on crackled porcelain
-
Marcia Selsor reacted to thirdcareer for a gallery image, New pieces May2013
It's always a great day when everything comes out of the kiln in good shape!
-
Marcia Selsor got a reaction from Claypple for a gallery image, legacy.jpg
Shell form modeled from a sand washed shell picked up on the beach. I made this piece in response to the BP oil spill in the Gulf©
-
Marcia Selsor got a reaction from Pompots for a gallery image, legacy.jpg
Shell form modeled from a sand washed shell picked up on the beach. I made this piece in response to the BP oil spill in the Gulf©
-
Marcia Selsor got a reaction from Marc McMillan for a gallery image, foilsaggarsmall copy
more ferric chloride, manganese and copper with some sugar granules and silver nitrate granules.
-
-
Marcia Selsor got a reaction from Marc McMillan for a gallery image, Obvara cylinder
Fired to 1650 and reduced in a liquor flour, sugar yeast brew 3 days old.Rinsed and cooled in water.
-
-