Sort of an oddball thing but Crayola washable liquid paint works as a floc, I add it to small glaze amounts for spraying. (I don't always need to floc a whole bucket)
this stuff





How did you happen on that Min?

#22 Min

Min

    Advanced Member

  • Members
  • PipPipPip
  • 1,524 posts
  • LocationCanada

Posted 29 March 2017 - 05:58 PM

Hi Babs,

 

Accidentally discovered it. I had run out of food colouring and was spraying a glaze with a white slurry onto a white pot. My girls were younger at the time and I raided their craft cupboard. I wasn't trying to flocculate the glaze, just tint it a bit so I could see it on the pots. In a hurry it makes a really good floc, no lumps or floating bits, just stirs right in but it's kind of a pricey way to do it.