Pres reacted to Mark C. in Purchasing a kiln for home studio use
If this is in the UK? then we need to know more on what the electrical voltage is in the UK. Maybe some UK potters can chine in with this tec info
-
Pres reacted to neilestrick in Purchasing a kiln for home studio use
Only very small kilns will run on 120V service. Any kiln of functional size will need 220/240 volts. The smallest kiln I would consider is an 18" wide model. But ideally a 23" wide model would be the most functional, as you can fit plates and serving bowls in it much easier. First thing to do is to take a look at the web sites of some kiln manufacturers in your area to get an idea of what's out there, and see what the electrical requirements are for the size of kiln you want. Then have an electrician check out your system to see what size circuit your system can handle. Minimum you'll need a 30 amp breaker, on up to 50 or 60 amps depending on the size of kiln you want. At £800 you'll have to buy used, but looking at the new ones will give you an idea of what you'll need to do as far as hooking it up. If the kiln is indoors, it will need to be vented, or at the very least have 2 windows that can create a cross draft with fans.
-
Pres reacted to Dick White in Purchasing a kiln for home studio use
The OP shows a location in the UK and price limits in pounds. The standard electric service there is 230V. In the US, standard residential electric service is 120/240V, where the normal household receptacle is 120V and other special purpose receptacles are 240V. Thus, in the US, there are a variety of kilns designed for either 120V or 240V service. I don't think there will be any 120V kilns in the UK, but I could be wrong.
-
Pres reacted to Mark C. in Purchasing a kiln for home studio use
I bet they made some small hobby doll kilns and the like in the UK that ran on 120 like they did here
-
Pres reacted to davidh4976 in QotW: Have you had to reformulate any clays or glazes due to a shortage of materials?
I've had to reformulate over half of our pottery glazes, both cone 6 and cone 10 to accommodate the end of Gerstley Borate, Custer, and Texas Talc. Using frits for GB, Mahavir Potash Feldspar for Custer, and dolomite/whiting for talc. Of course, all of the recipes needed changes to amounts of silica, kaolin, etc.
The tough ones seem to be the recipes that were "breaking" glazes or used some sort of lithium. Those took some tweaking and testing to get to a similar match to the old glazes.
Our local supplier has switched from Custer to G-200EU in their clay body mixes without any noticeable difference.
-
Pres reacted to GEP in QotW: Have you had to reformulate any clays or glazes due to a shortage of materials?
I have been spending a lot of time and energy replacing my Gerstley Borate glazes. The new ones are coming along, but they just don’t have the same glow and magic. I am trying to push the limits of “how much boron can I get away with?”
The good news is that switching to Fabi Talc in place of Texas Talc has been seamless.
-
Pres got a reaction from Rae Reich in QotW: Have you had to reformulate any clays or glazes due to a shortage of materials?
I have a favorite glaze that uses talc, and up until lately have had quite a bit to use in glazes that I bought several years ago. However this last glaze batch found me with none left. Last year I had heard about a shortage of talc, and believed I would have to reformulate my glaze to work with a different component, maybe dolomite. Imagine my surprise when I found Fabi Talc listed at SC. So I will be ordering some to use in my glaze. However, it makes me wonder if anyone has had to reformulate glazes or clay bodies due to a lack of materials?
QotW: Have you had to reformulate any clays or glazes due to a shortage of materials?
best,
Pres
-
Pres reacted to Hulk in QotW: Have you had to reformulate any clays or glazes due to a shortage of materials?
The clays I like from "nearby" vendor (about a hundred miles) have been reformulated.
The whitish stoneware seems about the same, the red behaves a bit differently.
My intent was (still is!) to look into alternatives this year; I've enough Gerstley, Custer, and Texas Talc to last a few years, however, years go quickly...
-
Pres reacted to Dick White in QotW: Have you had to reformulate any clays or glazes due to a shortage of materials?
All the time now. Gerstley is gone and Gillespie is not a perfect match. 3134 requires a complete rewrite of the recipe. Custer is gone from the market, but I still have some. G200EU might be ok, haven’t tried it yet. Still have some old Amtal talc, but some Fabi is in my future. What’s next?
-
Pres got a reaction from Hulk in QotW: Have you had to reformulate any clays or glazes due to a shortage of materials?
I have a favorite glaze that uses talc, and up until lately have had quite a bit to use in glazes that I bought several years ago. However this last glaze batch found me with none left. Last year I had heard about a shortage of talc, and believed I would have to reformulate my glaze to work with a different component, maybe dolomite. Imagine my surprise when I found Fabi Talc listed at SC. So I will be ordering some to use in my glaze. However, it makes me wonder if anyone has had to reformulate glazes or clay bodies due to a lack of materials?
QotW: Have you had to reformulate any clays or glazes due to a shortage of materials?
best,
Pres
-
Pres reacted to neilestrick in Gritty wheel head
First, why vinegar in the throwing water?
Usually when we see black on the wheel head it is simply a tiny bit of the aluminum abrading from the clay. Could just be the abrasion of the bat against the wheel. Does wiping it down not remove it?
-
Pres reacted to Callie Beller Diesel in QotW: Talisman, Bucket or other type of sieve for glaze mixing?
I use a talisman at work, and while it’s great for 10 gallon batches of glaze, it would be wildly impractical in my home studio. The cleanup of the brushes is a pain.
I have a smaller sieve that sits in a 5 gallon pail at home, and I use a large round sash brush to push the glaze through. It works pretty fast and cleans up very easily.
-
Pres got a reaction from Rae Reich in Glazed pieces hung out at 800F degrees - ok?
@ABlancBest bet here is to assess the kiln problem, fix it, and then re-fire the load to ^6. Check your elements to make certain none of them has broken first. If they are in good shape, then the problem is probably in the lead boxes. Is this kiln run on a cone setter or a programmable controller? If in a setter was the cone in the setter still as if unused?
best,
Pres
-
Pres reacted to neilestrick in Bisque firing frustrations
Pack the middle the tightest.
Have you tried just using the cone 08 preprogrammed firing schedule?
-
Pres got a reaction from Callie Beller Diesel in Bisque firing frustrations
Density of the load has an effect on the way heat moves in the kiln. Kilns are heated by 3 different forms of heat transfer: Radiant, Conduction, and Convection. Understanding these will help you to understand the need to pack the kiln consistently. Radiant heat is occurs first in the kiln as the elements radiate heat to heat up the air and the pottery. The pottery on the outer edges will heat up to radiate heat towards the center of the kiln. Please note that while Radiant heat is going on Convection is also occurring in the kiln as air heats up and begins to move to the top of the kiln forcing cooler air downward. Overly tight loads will inhibit the movement of air in the kiln causing areas that do not get air to not reach expected cones. However, as this is going on Conduction, where heat is moving through a solid, is taking place, Conduction is a slower process but it allows the pots to heat up from the outside to the inside, and the kiln from the inside to the outside. This good reason to have proper distance from the kiln to outside walls or other materials that could ignite.
Hope this helps to answer some of you concerns.
best,
Pres
-
Pres got a reaction from Hulk in QotW: Talisman, Bucket or other type of sieve for glaze mixing?
Hi folks, we covered this a few years ago, but I was mixing glazes yesterday with my plastic bucket sieve, and a brush to run the glaze through the sieve into a spare bucket, and then back into the rinsed out original bucket. I have often wondered about buying a Talisman sieve, but in the long run the cost scares me away, and I really get along fine with my bucket sieve. I will pick up a digital scale as the cost of them has come down.
QotW: Talisman, Bucket or other type of sieve for glaze mixing?
bestg,
Pres
-
Pres reacted to Gonepotty in Bisque firing frustrations
Thanks Min, yes it only has 1 thermocouple. I'll make note of this info for my next bisque firing
-
Pres got a reaction from Babs in Bisque firing frustrations
Density of the load has an effect on the way heat moves in the kiln. Kilns are heated by 3 different forms of heat transfer: Radiant, Conduction, and Convection. Understanding these will help you to understand the need to pack the kiln consistently. Radiant heat is occurs first in the kiln as the elements radiate heat to heat up the air and the pottery. The pottery on the outer edges will heat up to radiate heat towards the center of the kiln. Please note that while Radiant heat is going on Convection is also occurring in the kiln as air heats up and begins to move to the top of the kiln forcing cooler air downward. Overly tight loads will inhibit the movement of air in the kiln causing areas that do not get air to not reach expected cones. However, as this is going on Conduction, where heat is moving through a solid, is taking place, Conduction is a slower process but it allows the pots to heat up from the outside to the inside, and the kiln from the inside to the outside. This good reason to have proper distance from the kiln to outside walls or other materials that could ignite.
Hope this helps to answer some of you concerns.
best,
Pres
-
Pres got a reaction from Min in Bisque firing frustrations
Density of the load has an effect on the way heat moves in the kiln. Kilns are heated by 3 different forms of heat transfer: Radiant, Conduction, and Convection. Understanding these will help you to understand the need to pack the kiln consistently. Radiant heat is occurs first in the kiln as the elements radiate heat to heat up the air and the pottery. The pottery on the outer edges will heat up to radiate heat towards the center of the kiln. Please note that while Radiant heat is going on Convection is also occurring in the kiln as air heats up and begins to move to the top of the kiln forcing cooler air downward. Overly tight loads will inhibit the movement of air in the kiln causing areas that do not get air to not reach expected cones. However, as this is going on Conduction, where heat is moving through a solid, is taking place, Conduction is a slower process but it allows the pots to heat up from the outside to the inside, and the kiln from the inside to the outside. This good reason to have proper distance from the kiln to outside walls or other materials that could ignite.
Hope this helps to answer some of you concerns.
best,
Pres
-
Pres reacted to Mark C. in QotW: Talisman, Bucket or other type of sieve for glaze mixing?
I should add I put my large shallow porcelain sink and water setup with high ball valve pipe and hose setup in studio from a salvage yard in 1973. The sink is shallow but large.That was 51 years ago. Lot of water thru the screens since then.
-
Pres reacted to Min in QotW: Talisman, Bucket or other type of sieve for glaze mixing?
I used to use a Talisman but switched over to using a cordless drill with a brush attachment and a regular plastic sieve that sits in the glaze bucket . WAY easier to clean up!!! Can clean the brush attachment in a small basin or pail of water or under a running tap. Takes seconds and no big sink needed. I have one sieve for clear and light coloured glazes and the other for the dark glazes.
I sold my Talisman.
To give credit where credit is due this idea is from @liambesaw
-
Pres reacted to Mark C. in QotW: Slip, Slip with vinegar, Magic Water: What is your choice, and why?
I feel that whatever works for you with slip use that . If it works use it. I will add that in my clay body and calc class back in collage we tested all types of attachments (long before magic water ) and what was leaned that scoring and slip make for stronger bonds. It's a night and day difference so score and slip . If you are not that you are making weaker bonds.
-
Pres got a reaction from Hyn Patty in QotW: Slip, Slip with vinegar, Magic Water: What is your choice, and why?
I'm sure we have had this discussion a few years back, but good to return to it for those newbies out there. Over the years I have used all three, and found that I prefer the Magic Water. When teaching HS in the early years, I had used slip as that is what I learned to work with. If you you were diligent about your scoring, and your paddling/compressing the seams along with regular gap filling and smoothing you would have a good seam with no problems. However, being lax in any way could leave a seam that would split, or leave and ugly hole to be noticed even after glaze firing. Students took a long time to discover diligence. Vinegar was the addition that I started adding to my slip containers, as the mild acid did help to work the seams better. However, I came to believe that it was too easy for students to cover up a bad seam with slip of any sort than to get the seam right. Along came Magic Water, and when I started using it myself, I knew that I had to start using it in the classroom. It did not change everything, but worked wonders with making seams and at the same time it was hard to hide a bad seam.
QotW: Slip, Slip with vinegar, Magic Water: What is your choice, and why?
best,
Pres
-
Pres reacted to Callie Beller Diesel in Are exhibitions or juried art shows worth entering?
Juried exhibitions or invitationals through galleries have never netted me any sales. They can be a nice ego rub, which has its own value, but that value isn’t monetary IME.
Juried fairs or markets however, are a good thing. Juries can help put together a crowd of compatible artists and quality of work, which helps get it in front of people who are interested in such things.
-
Pres reacted to neilestrick in Are exhibitions or juried art shows worth entering?
Juried gallery exhibitions may get you one or two sales beyond the piece you have in the show, but mostly it's just a resume builder that may help you get into other galleries or build your social media account a little. Art fairs will definitely build sales, because you can show so much more work to so many more people.