Posts
12,066 -
Joined
-
Last visited
Reputation Activity
-
Mark C. got a reaction from Callie Beller Diesel in In my 50 years this has never happened.
So last night I got a message on facebook from a fellow Board member (art show board)
Seems a hoarder with money passed away and their is an estate sale this weekend. The photos show a few huge tables of packed to the gills with my work as well as a large floor area . The Estate guy was posting lots of photos of tons of collected stuff as this women had passed away and collected huge volumes of work . I called him an hour after the post went up to ask whats the deal. He said he was in a huge time crunch to emepty the house . He was not autioning it but hoping to sell it piece by piece ,nothing is priced. I let him know i made all that pottery . Looks to be about 8-12 boxes full. I said if the price was right I'll take it all. He siad any reasonable offer he would take. Now In all my ceramics life I =have never bought my work back from anyone. The pots look all new and not used as there was too much volume to use -she was collecting not using. He said since you are the maker how about coming a day early and see what you want so today at noon I'm going. My plan is buy it for about 25%of retail tops. . Then just put it into my inventory . I have a pile of cash to sweeten the deal. Tbis may all go south today just as easy so its far from a done deal but its one heck of a strange deal. The forms are glasses ,mugs and bowls of all sizes from stacks of large serving to cereal bowls. I can see few pots that are not mine (not interested in) in the mix as well. I'll post the outcome.
This is the most work of any one single customer by far and it looks like it was mostly bought at my gallery outlets.I can tell by the colors (some now discontinued) and color combos of when the work was made. I had no idea anyone custiomer pould ever own this much stuff from me. I'm hoping I may have known her as well. we shall see today-its a strange world out there.
-
Mark C. got a reaction from Callie Beller Diesel in In my 50 years this has never happened.
Ok I showed up at noon and others where walking thru house buying up stuff. Looks like a small amount of my work had sold . . But the tables where still stuffed.I told the fellow for me its all or nothing deal. I made a quik rough list and and down sized my offer to 450 $ cash. I said I have the boxes and paper and will take only my work as there was other ceramics mixed in especailly on the floor under tables (not in the photos)He took the offer which is about 16 mugs for me sales wise these days. I boxed it into 6 Banana boxes full and dollyed it out feeling great. The womans sister spoke to me and said the lady (her sister) had a stroke and was in full time care now in North Caralina.I said she had the most work of any customer I ever knew of and gave her my card to thank the sister . I have never met here as 99% of all the work was from a few outlets and they all had the price labels and cards inside of them. Not my own show price labels but those of my Eureka outlets. The largest amout of stuff was from a co-op organic market I pulled out of a year ago as I am slowing it down with a plan. I put a care and feeding tag in every pot then and all those where still in every pot. Now I have a nearly a 35 cubic feet whole kiln worth of new old stock. Its insane really. In my 50 years I never in my dreams would expect this to happen. I'm selling the stock twice this time without having to make or glaze or fire it. Of couse prices have risen since I sold this originally so I'm really ahead . I'm making 4 dinner plates for the friend who sent me the info last night. She really came thru for me.
There where two tables of pots like the one photo as well as a bunch on the floor
Just when you think you have seen or heard it all -boom something new surfaces .
-
Mark C. got a reaction from Roberta12 in In my 50 years this has never happened.
So last night I got a message on facebook from a fellow Board member (art show board)
Seems a hoarder with money passed away and their is an estate sale this weekend. The photos show a few huge tables of packed to the gills with my work as well as a large floor area . The Estate guy was posting lots of photos of tons of collected stuff as this women had passed away and collected huge volumes of work . I called him an hour after the post went up to ask whats the deal. He said he was in a huge time crunch to emepty the house . He was not autioning it but hoping to sell it piece by piece ,nothing is priced. I let him know i made all that pottery . Looks to be about 8-12 boxes full. I said if the price was right I'll take it all. He siad any reasonable offer he would take. Now In all my ceramics life I =have never bought my work back from anyone. The pots look all new and not used as there was too much volume to use -she was collecting not using. He said since you are the maker how about coming a day early and see what you want so today at noon I'm going. My plan is buy it for about 25%of retail tops. . Then just put it into my inventory . I have a pile of cash to sweeten the deal. Tbis may all go south today just as easy so its far from a done deal but its one heck of a strange deal. The forms are glasses ,mugs and bowls of all sizes from stacks of large serving to cereal bowls. I can see few pots that are not mine (not interested in) in the mix as well. I'll post the outcome.
This is the most work of any one single customer by far and it looks like it was mostly bought at my gallery outlets.I can tell by the colors (some now discontinued) and color combos of when the work was made. I had no idea anyone custiomer pould ever own this much stuff from me. I'm hoping I may have known her as well. we shall see today-its a strange world out there.
-
Mark C. got a reaction from Jeff Longtin in In my 50 years this has never happened.
Ok I showed up at noon and others where walking thru house buying up stuff. Looks like a small amount of my work had sold . . But the tables where still stuffed.I told the fellow for me its all or nothing deal. I made a quik rough list and and down sized my offer to 450 $ cash. I said I have the boxes and paper and will take only my work as there was other ceramics mixed in especailly on the floor under tables (not in the photos)He took the offer which is about 16 mugs for me sales wise these days. I boxed it into 6 Banana boxes full and dollyed it out feeling great. The womans sister spoke to me and said the lady (her sister) had a stroke and was in full time care now in North Caralina.I said she had the most work of any customer I ever knew of and gave her my card to thank the sister . I have never met here as 99% of all the work was from a few outlets and they all had the price labels and cards inside of them. Not my own show price labels but those of my Eureka outlets. The largest amout of stuff was from a co-op organic market I pulled out of a year ago as I am slowing it down with a plan. I put a care and feeding tag in every pot then and all those where still in every pot. Now I have a nearly a 35 cubic feet whole kiln worth of new old stock. Its insane really. In my 50 years I never in my dreams would expect this to happen. I'm selling the stock twice this time without having to make or glaze or fire it. Of couse prices have risen since I sold this originally so I'm really ahead . I'm making 4 dinner plates for the friend who sent me the info last night. She really came thru for me.
There where two tables of pots like the one photo as well as a bunch on the floor
Just when you think you have seen or heard it all -boom something new surfaces .
-
Mark C. got a reaction from Roberta12 in In my 50 years this has never happened.
Ok I showed up at noon and others where walking thru house buying up stuff. Looks like a small amount of my work had sold . . But the tables where still stuffed.I told the fellow for me its all or nothing deal. I made a quik rough list and and down sized my offer to 450 $ cash. I said I have the boxes and paper and will take only my work as there was other ceramics mixed in especailly on the floor under tables (not in the photos)He took the offer which is about 16 mugs for me sales wise these days. I boxed it into 6 Banana boxes full and dollyed it out feeling great. The womans sister spoke to me and said the lady (her sister) had a stroke and was in full time care now in North Caralina.I said she had the most work of any customer I ever knew of and gave her my card to thank the sister . I have never met here as 99% of all the work was from a few outlets and they all had the price labels and cards inside of them. Not my own show price labels but those of my Eureka outlets. The largest amout of stuff was from a co-op organic market I pulled out of a year ago as I am slowing it down with a plan. I put a care and feeding tag in every pot then and all those where still in every pot. Now I have a nearly a 35 cubic feet whole kiln worth of new old stock. Its insane really. In my 50 years I never in my dreams would expect this to happen. I'm selling the stock twice this time without having to make or glaze or fire it. Of couse prices have risen since I sold this originally so I'm really ahead . I'm making 4 dinner plates for the friend who sent me the info last night. She really came thru for me.
There where two tables of pots like the one photo as well as a bunch on the floor
Just when you think you have seen or heard it all -boom something new surfaces .
-
Mark C. got a reaction from Rae Reich in In my 50 years this has never happened.
So last night I got a message on facebook from a fellow Board member (art show board)
Seems a hoarder with money passed away and their is an estate sale this weekend. The photos show a few huge tables of packed to the gills with my work as well as a large floor area . The Estate guy was posting lots of photos of tons of collected stuff as this women had passed away and collected huge volumes of work . I called him an hour after the post went up to ask whats the deal. He said he was in a huge time crunch to emepty the house . He was not autioning it but hoping to sell it piece by piece ,nothing is priced. I let him know i made all that pottery . Looks to be about 8-12 boxes full. I said if the price was right I'll take it all. He siad any reasonable offer he would take. Now In all my ceramics life I =have never bought my work back from anyone. The pots look all new and not used as there was too much volume to use -she was collecting not using. He said since you are the maker how about coming a day early and see what you want so today at noon I'm going. My plan is buy it for about 25%of retail tops. . Then just put it into my inventory . I have a pile of cash to sweeten the deal. Tbis may all go south today just as easy so its far from a done deal but its one heck of a strange deal. The forms are glasses ,mugs and bowls of all sizes from stacks of large serving to cereal bowls. I can see few pots that are not mine (not interested in) in the mix as well. I'll post the outcome.
This is the most work of any one single customer by far and it looks like it was mostly bought at my gallery outlets.I can tell by the colors (some now discontinued) and color combos of when the work was made. I had no idea anyone custiomer pould ever own this much stuff from me. I'm hoping I may have known her as well. we shall see today-its a strange world out there.
-
Mark C. got a reaction from Bam2015 in In my 50 years this has never happened.
Ok I showed up at noon and others where walking thru house buying up stuff. Looks like a small amount of my work had sold . . But the tables where still stuffed.I told the fellow for me its all or nothing deal. I made a quik rough list and and down sized my offer to 450 $ cash. I said I have the boxes and paper and will take only my work as there was other ceramics mixed in especailly on the floor under tables (not in the photos)He took the offer which is about 16 mugs for me sales wise these days. I boxed it into 6 Banana boxes full and dollyed it out feeling great. The womans sister spoke to me and said the lady (her sister) had a stroke and was in full time care now in North Caralina.I said she had the most work of any customer I ever knew of and gave her my card to thank the sister . I have never met here as 99% of all the work was from a few outlets and they all had the price labels and cards inside of them. Not my own show price labels but those of my Eureka outlets. The largest amout of stuff was from a co-op organic market I pulled out of a year ago as I am slowing it down with a plan. I put a care and feeding tag in every pot then and all those where still in every pot. Now I have a nearly a 35 cubic feet whole kiln worth of new old stock. Its insane really. In my 50 years I never in my dreams would expect this to happen. I'm selling the stock twice this time without having to make or glaze or fire it. Of couse prices have risen since I sold this originally so I'm really ahead . I'm making 4 dinner plates for the friend who sent me the info last night. She really came thru for me.
There where two tables of pots like the one photo as well as a bunch on the floor
Just when you think you have seen or heard it all -boom something new surfaces .
-
Mark C. got a reaction from LouiseD in Extremely stupid and ignorant to hazards with working with clay
This is not my first time about hearing about lead use in England. Its still in use there for some .
Google is your friend and learning about being around it or NOT
-
Mark C. got a reaction from shawnhar in In my 50 years this has never happened.
Ok I showed up at noon and others where walking thru house buying up stuff. Looks like a small amount of my work had sold . . But the tables where still stuffed.I told the fellow for me its all or nothing deal. I made a quik rough list and and down sized my offer to 450 $ cash. I said I have the boxes and paper and will take only my work as there was other ceramics mixed in especailly on the floor under tables (not in the photos)He took the offer which is about 16 mugs for me sales wise these days. I boxed it into 6 Banana boxes full and dollyed it out feeling great. The womans sister spoke to me and said the lady (her sister) had a stroke and was in full time care now in North Caralina.I said she had the most work of any customer I ever knew of and gave her my card to thank the sister . I have never met here as 99% of all the work was from a few outlets and they all had the price labels and cards inside of them. Not my own show price labels but those of my Eureka outlets. The largest amout of stuff was from a co-op organic market I pulled out of a year ago as I am slowing it down with a plan. I put a care and feeding tag in every pot then and all those where still in every pot. Now I have a nearly a 35 cubic feet whole kiln worth of new old stock. Its insane really. In my 50 years I never in my dreams would expect this to happen. I'm selling the stock twice this time without having to make or glaze or fire it. Of couse prices have risen since I sold this originally so I'm really ahead . I'm making 4 dinner plates for the friend who sent me the info last night. She really came thru for me.
There where two tables of pots like the one photo as well as a bunch on the floor
Just when you think you have seen or heard it all -boom something new surfaces .
-
Mark C. got a reaction from Kelly in AK in In my 50 years this has never happened.
So last night I got a message on facebook from a fellow Board member (art show board)
Seems a hoarder with money passed away and their is an estate sale this weekend. The photos show a few huge tables of packed to the gills with my work as well as a large floor area . The Estate guy was posting lots of photos of tons of collected stuff as this women had passed away and collected huge volumes of work . I called him an hour after the post went up to ask whats the deal. He said he was in a huge time crunch to emepty the house . He was not autioning it but hoping to sell it piece by piece ,nothing is priced. I let him know i made all that pottery . Looks to be about 8-12 boxes full. I said if the price was right I'll take it all. He siad any reasonable offer he would take. Now In all my ceramics life I =have never bought my work back from anyone. The pots look all new and not used as there was too much volume to use -she was collecting not using. He said since you are the maker how about coming a day early and see what you want so today at noon I'm going. My plan is buy it for about 25%of retail tops. . Then just put it into my inventory . I have a pile of cash to sweeten the deal. Tbis may all go south today just as easy so its far from a done deal but its one heck of a strange deal. The forms are glasses ,mugs and bowls of all sizes from stacks of large serving to cereal bowls. I can see few pots that are not mine (not interested in) in the mix as well. I'll post the outcome.
This is the most work of any one single customer by far and it looks like it was mostly bought at my gallery outlets.I can tell by the colors (some now discontinued) and color combos of when the work was made. I had no idea anyone custiomer pould ever own this much stuff from me. I'm hoping I may have known her as well. we shall see today-its a strange world out there.
-
Mark C. got a reaction from Rae Reich in What’s the hottest temperature that I can safely unload a bisque kiln?
The trick for quick cooling is no let cold air in. No matter what typoe of kiln.Electrics are easier as they are essentially sealed up. The lid lets the heat up and. out -I keep the plugs in and cover any holes and open the lid with gloves.
-
Mark C. got a reaction from oldlady in In my 50 years this has never happened.
So last night I got a message on facebook from a fellow Board member (art show board)
Seems a hoarder with money passed away and their is an estate sale this weekend. The photos show a few huge tables of packed to the gills with my work as well as a large floor area . The Estate guy was posting lots of photos of tons of collected stuff as this women had passed away and collected huge volumes of work . I called him an hour after the post went up to ask whats the deal. He said he was in a huge time crunch to emepty the house . He was not autioning it but hoping to sell it piece by piece ,nothing is priced. I let him know i made all that pottery . Looks to be about 8-12 boxes full. I said if the price was right I'll take it all. He siad any reasonable offer he would take. Now In all my ceramics life I =have never bought my work back from anyone. The pots look all new and not used as there was too much volume to use -she was collecting not using. He said since you are the maker how about coming a day early and see what you want so today at noon I'm going. My plan is buy it for about 25%of retail tops. . Then just put it into my inventory . I have a pile of cash to sweeten the deal. Tbis may all go south today just as easy so its far from a done deal but its one heck of a strange deal. The forms are glasses ,mugs and bowls of all sizes from stacks of large serving to cereal bowls. I can see few pots that are not mine (not interested in) in the mix as well. I'll post the outcome.
This is the most work of any one single customer by far and it looks like it was mostly bought at my gallery outlets.I can tell by the colors (some now discontinued) and color combos of when the work was made. I had no idea anyone custiomer pould ever own this much stuff from me. I'm hoping I may have known her as well. we shall see today-its a strange world out there.
-
Mark C. got a reaction from Pres in In my 50 years this has never happened.
So last night I got a message on facebook from a fellow Board member (art show board)
Seems a hoarder with money passed away and their is an estate sale this weekend. The photos show a few huge tables of packed to the gills with my work as well as a large floor area . The Estate guy was posting lots of photos of tons of collected stuff as this women had passed away and collected huge volumes of work . I called him an hour after the post went up to ask whats the deal. He said he was in a huge time crunch to emepty the house . He was not autioning it but hoping to sell it piece by piece ,nothing is priced. I let him know i made all that pottery . Looks to be about 8-12 boxes full. I said if the price was right I'll take it all. He siad any reasonable offer he would take. Now In all my ceramics life I =have never bought my work back from anyone. The pots look all new and not used as there was too much volume to use -she was collecting not using. He said since you are the maker how about coming a day early and see what you want so today at noon I'm going. My plan is buy it for about 25%of retail tops. . Then just put it into my inventory . I have a pile of cash to sweeten the deal. Tbis may all go south today just as easy so its far from a done deal but its one heck of a strange deal. The forms are glasses ,mugs and bowls of all sizes from stacks of large serving to cereal bowls. I can see few pots that are not mine (not interested in) in the mix as well. I'll post the outcome.
This is the most work of any one single customer by far and it looks like it was mostly bought at my gallery outlets.I can tell by the colors (some now discontinued) and color combos of when the work was made. I had no idea anyone custiomer pould ever own this much stuff from me. I'm hoping I may have known her as well. we shall see today-its a strange world out there.
-
-
Mark C. got a reaction from Roberta12 in Extremely stupid and ignorant to hazards with working with clay
Buy your own mask.treat lead exposure seriously -Read up on precautions -Google is your friend
-
Mark C. reacted to Min in Extremely stupid and ignorant to hazards with working with clay
Frits containing lead are safer for the potter while using the raw glaze but once a glaze is melted it depends on the glaze chemistry just the same as if using a raw lead glaze.
If this studio is allowing and asking employees to spray lead glazes with inadequate PPE and practices I have to wonder what other infractions are happening. Where is the exhaust going? Landing up in the environment? What temperature are they firing it to? (lead volatilizes over 1170C) Silica dust control etc. Is there excessive copper being used in any of the lead glazes? (copper increases lead release) and so on.
-
Mark C. got a reaction from Rae Reich in Amaco Bisque Fix on Greenware?
It works on both but best on bisque- If the item is green use your own clay fines to fill the crack. (mix your own clay fines with a bit of vinagar and water and fill greenware cracks. I fill the crack once bisqued and let it dry and sand it smooth then glaze. The line (where it is) is white so I usually cover with a dark glaze. This product works well but do not expect miracles .I never rebisque it -just let it dry sand smooth glaze and fire.If you need to glue it on use Aztec high fire cement. Mix it with your own clay body in small doses.
Used Bisque fix for many many years. They once made a greenware fix but took it off market years ago-that stuff was great .
I also use it a filler in a say a hole or chip missing piece. Good stuff but the price went up recently like all things.
-
Mark C. got a reaction from Kelly in AK in QotW: How savvy are your customers about pottery?
Its a huge mix from knowing a lot to clueless-like putting a teapot on open flame ( and breaking it the day he bought it) to heating bake ware up with oven and lasting decades.
The public is a petri dish of good bad and the down right clueless
As I slow it down with the public I will never miss the clueless ones.Only the ones who are aware .
-
Mark C. got a reaction from LouiseD in Extremely stupid and ignorant to hazards with working with clay
Buy your own mask.treat lead exposure seriously -Read up on precautions -Google is your friend
-
Mark C. got a reaction from Hulk in QotW: How savvy are your customers about pottery?
Its a huge mix from knowing a lot to clueless-like putting a teapot on open flame ( and breaking it the day he bought it) to heating bake ware up with oven and lasting decades.
The public is a petri dish of good bad and the down right clueless
As I slow it down with the public I will never miss the clueless ones.Only the ones who are aware .
-
Mark C. got a reaction from GEP in QotW: How savvy are your customers about pottery?
Its a huge mix from knowing a lot to clueless-like putting a teapot on open flame ( and breaking it the day he bought it) to heating bake ware up with oven and lasting decades.
The public is a petri dish of good bad and the down right clueless
As I slow it down with the public I will never miss the clueless ones.Only the ones who are aware .
-
Mark C. got a reaction from Pres in QotW: How savvy are your customers about pottery?
Its a huge mix from knowing a lot to clueless-like putting a teapot on open flame ( and breaking it the day he bought it) to heating bake ware up with oven and lasting decades.
The public is a petri dish of good bad and the down right clueless
As I slow it down with the public I will never miss the clueless ones.Only the ones who are aware .
-
Mark C. got a reaction from Rae Reich in QotW: How savvy are your customers about pottery?
Its a huge mix from knowing a lot to clueless-like putting a teapot on open flame ( and breaking it the day he bought it) to heating bake ware up with oven and lasting decades.
The public is a petri dish of good bad and the down right clueless
As I slow it down with the public I will never miss the clueless ones.Only the ones who are aware .
-
Mark C. got a reaction from Kelly in AK in AAARGH SHIMPO you changed EVERYTHING!
I did a demo workshop on about 8 of the wispers-they are quiet and thats all they are -they can be slowed down easy with a medium amount of clay and the splash pans are cheesy and will break over time. The cords are to light duty as well. Thats my take-oh ya they do not have good fast service/parts like Brands made in this country
a pancake motor is like Naan bread only made on a charcoal fire a low heat-when done its a low torque flavor that is really quiet and small
-
Mark C. got a reaction from Pres in Amaco Bisque Fix on Greenware?
It works on both but best on bisque- If the item is green use your own clay fines to fill the crack. (mix your own clay fines with a bit of vinagar and water and fill greenware cracks. I fill the crack once bisqued and let it dry and sand it smooth then glaze. The line (where it is) is white so I usually cover with a dark glaze. This product works well but do not expect miracles .I never rebisque it -just let it dry sand smooth glaze and fire.If you need to glue it on use Aztec high fire cement. Mix it with your own clay body in small doses.
Used Bisque fix for many many years. They once made a greenware fix but took it off market years ago-that stuff was great .
I also use it a filler in a say a hole or chip missing piece. Good stuff but the price went up recently like all things.