Chilly reacted to Callie Beller Diesel in Reglazing Using a Propane Torch
I would also expect the spot use of a blow torch to cause enough thermal discrepancy through the piece to crack it entirely. +1 for what Bill said. Either have it reglazed professionally or replace it.
-
Chilly reacted to Bill Kielb in Reglazing Using a Propane Torch
Very, very unlikely. Lowfire glazes melt about 2000 degrees. Fired on enameled porcelain is usually a mix of Frits and fires in the range of 1400 degrees. That’s probably the tip temperature of a propane torch, plus if cast iron - you need to heat the whole vessel. My thought is very very unlikely, removing to a restore shop possible but I am guessing replacement probably more economical.
-
Chilly got a reaction from Callie Beller Diesel in Pottery Wheel for Beginner
Can't give much advice, other than - buy a real wheel from a pottery supply company - do not buy a "toy" wheel - try Scarva who are (I believe) based on your island. If looking at second hand, try before your buy, make sure the wheel runs and accelerates smoothly, starts and stops when asked.
.
-
Chilly got a reaction from Rae Reich in Pottery Wheel for Beginner
Can't give much advice, other than - buy a real wheel from a pottery supply company - do not buy a "toy" wheel - try Scarva who are (I believe) based on your island. If looking at second hand, try before your buy, make sure the wheel runs and accelerates smoothly, starts and stops when asked.
.
-
Chilly got a reaction from Hulk in Pottery Wheel for Beginner
Can't give much advice, other than - buy a real wheel from a pottery supply company - do not buy a "toy" wheel - try Scarva who are (I believe) based on your island. If looking at second hand, try before your buy, make sure the wheel runs and accelerates smoothly, starts and stops when asked.
.
-
Chilly got a reaction from Pyewackette in Slip Casting Handles
I use an extruder, horizontally, next to a corner wall. Use the side wall to push the handle in. I tried it upside down, pushing handle on floor, but that was not good. Also tried right way up, pushing handle up against greenhouse bench, but that lifted the bench !
Similar to this.
-
Chilly reacted to Kelly in AK in Partial glazing of large pot in soda fire
While it’s not quite the same as what you have to deal with, it is fun to watch these old potters glaze big pots. And they glazed them green, which is wild to think about too.
Isaac Button glazing some big crocks (around 4:30):
Burlon Craig glazing a crock and a bottle (around 2:00):
-
Chilly got a reaction from Hulk in QotW: Are you Dipper, Pourer, Sprayer, sponger, squirter, or Brusher?
Brusher, followed by pouring in/out. Never use enough of amy glaze to justify quantity needed for dipping.
-
Chilly got a reaction from Rae Reich in QotW: Are you Dipper, Pourer, Sprayer, sponger, squirter, or Brusher?
Brusher, followed by pouring in/out. Never use enough of amy glaze to justify quantity needed for dipping.
-
Chilly got a reaction from Callie Beller Diesel in troubleshooting glaze color without buying all of the glazes in the world....
There is a Facebook group....... https://www.facebook.com/groups/potterschoiceex
-
Chilly reacted to Dick White in What could cause this (hard panning)
What @PeterH said. Neph sye is a known bad boy in the glaze chem world. It is very high in sodium, which is why it is popular. It is also slightly soluble. Sodium is an alkaline deflocculant, which results in hard panning. The sodium slowly leaches out of the neph sye and at some indeterminate point deflocs the glaze slurry and it hard pans.
Also understand clay is the only material that can be flocculated to create a suspended glaze slurry. Materials such as feldspars or feldspathic materials (neph sye), other minerals such as whiting, etc., or frits do not respond to the alkaline or acidic conditions in the slurry to deflocculate or flocculate, respectively. Only clay responds to the deflocculation/flocculation process. A recipe with little or no clay, such as your recipe with a mere 5% EPK, needs a few additional percent of bentonite (a super clay) upon which to cause flocculation (if needed) by adding a mild acid such as epsom salts. And then after some time, the alkaline sodium leaches out of the neph sye and neutralizes whatever acidity in the slurry has been keeping the clay suspended, and boom, without warning it all falls down. The bentonite is not enough to stop this from happening. Dig it out and remix it with some epsom salts or vinegar to neutralize the excess alkalinity and restore the suspension.
As for the Magma product that folks above recommend, it does not chemically flocculate the slurry. It is an artificial gum additive that mechanically suspends the glaze solids. It is unaffected by the soluble leached sodium from the neph sye. It also has other attributes, so read the cautionary statements on the label. Otherwise, it floats bricks.
-
Chilly got a reaction from Hulk in Partial glazing of large pot in soda fire
Personally, I think he's talking out of his .....sit-upon.
I do think not glazing both inside and out can cause glaze fit issues, but implode......
Test (in your own kiln) by making a small vessel, glaze as you want, put into a saggar and fire it.
-
Chilly got a reaction from Pres in QotW: Sit or Stand, and on what type of Surface/Furniture?
I don't throw, but stand when hand-building. I use the highest table at the community centre, and often work on top of boxes to raise my work, and my benches in my greenhouse (studio) are high too.
I fidget, and am short in the body, and find sitting for most tasks is not comfortable. I did evening classes working with glass - fusing, copper foiling, leading and was the only one in the class who stood for 3-4 hours.
The only stuff I do sitting is textile based - spinning, sewing, knitting, although for spindle spinning it's easier to stand, same for weaving.
I think it's important to be at the right height, and comfortablewhatever you're doing.,
-
Chilly got a reaction from Rae Reich in Partial glazing of large pot in soda fire
Personally, I think he's talking out of his .....sit-upon.
I do think not glazing both inside and out can cause glaze fit issues, but implode......
Test (in your own kiln) by making a small vessel, glaze as you want, put into a saggar and fire it.
-
Chilly got a reaction from Rae Reich in QotW: Sit or Stand, and on what type of Surface/Furniture?
I don't throw, but stand when hand-building. I use the highest table at the community centre, and often work on top of boxes to raise my work, and my benches in my greenhouse (studio) are high too.
I fidget, and am short in the body, and find sitting for most tasks is not comfortable. I did evening classes working with glass - fusing, copper foiling, leading and was the only one in the class who stood for 3-4 hours.
The only stuff I do sitting is textile based - spinning, sewing, knitting, although for spindle spinning it's easier to stand, same for weaving.
I think it's important to be at the right height, and comfortablewhatever you're doing.,
-
Chilly got a reaction from Magnolia Mud Research in QotW: Sit or Stand, and on what type of Surface/Furniture?
I don't throw, but stand when hand-building. I use the highest table at the community centre, and often work on top of boxes to raise my work, and my benches in my greenhouse (studio) are high too.
I fidget, and am short in the body, and find sitting for most tasks is not comfortable. I did evening classes working with glass - fusing, copper foiling, leading and was the only one in the class who stood for 3-4 hours.
The only stuff I do sitting is textile based - spinning, sewing, knitting, although for spindle spinning it's easier to stand, same for weaving.
I think it's important to be at the right height, and comfortablewhatever you're doing.,
-
Chilly got a reaction from Pyewackette in Partial glazing of large pot in soda fire
Personally, I think he's talking out of his .....sit-upon.
I do think not glazing both inside and out can cause glaze fit issues, but implode......
Test (in your own kiln) by making a small vessel, glaze as you want, put into a saggar and fire it.
-
Chilly got a reaction from Min in Partial glazing of large pot in soda fire
Personally, I think he's talking out of his .....sit-upon.
I do think not glazing both inside and out can cause glaze fit issues, but implode......
Test (in your own kiln) by making a small vessel, glaze as you want, put into a saggar and fire it.
-
Chilly reacted to Callie Beller Diesel in Refiring
If the metal itself is already brittle, firing it more will make it worse. You may be better advised to look into cold process reinforcements, like maybe clear epoxy.
-
Chilly reacted to oldlady in Burning out candle wax in kiln?
after many, many years of using used candles, i have learned a thing or two. #1 do not use any added decorated candles with "snow". toss them!! #2, read #1. or, you may end up with a mess spread all through the entire kiln load by the fumes. read #1.
i find that mixing a red into the usual clear or white melted wax allows me to see exactly where the wax is and how far up the edge it goes. i single fire nearly everything so scraping off any splashes or whatever is easy since the clay is removed with the mistake. if done on a bisqued piece, re-bisquing removes the wax.
wiping the bottom on the interior edge of the hot pan immediately removes enough wax that the burn-out smell is hardly noticable. my hot pan is set at 350, and i wait until it is that hot to attempt to wax bottoms. the amount used is just enough to cover the foot.
the best part of using hot wax is that it is almost instantly dry. some brush on wax needs hours to dry.
-
Chilly reacted to Min in Porcelain slip over a Raku clay
Instead of using a porcelain I would use some of the raku body made into a slip then sieved to get the grog out of it. (60 mesh sieve should be fine enough) Get the slip on the outside of the pot as soon as possible to avoid issues with the slip shelling off or cracking.
edit: I looked up white raku clays in Australia and a quick search brought up this one, might be worth a try if the one you are using isn't white.
-
Chilly reacted to PeterH in My pieces collapsed
I don't think that firing within the manufacturer's guidelines guarantees that your form won't slump.
Probably only an issue with forms outside the usually pottery shapes, as previously observed by Hulk.
Think of a sheet of printer paper. Hold it by the short edge and it flops about. Tape the long edges together and it forms quite a strong cylinder. Compound curves are probably even better at resisting deformation.
I suspect that during firing sheets of clay bend easily, unless the bending requires local stretching or compression of the sheet.
-
Chilly reacted to Callie Beller Diesel in My pieces collapsed
Having a look at the glaze and clay information, it’s definitely not the clay being over fired. So +1 to what Peter said. The piece needs support, or a different design.
-
Chilly reacted to ronfire in Slump Mold
Finally got the mold slump mold made and a platter from it finished. It worked well and I can finally get to make more of these platters.
-
Chilly got a reaction from Callie Beller Diesel in QotW: How do you finish the lips of you vertical pieces?
I don't throw, therefore make few vessel type pots, but when I do, I think about this:
However...... I have two favourite mugs. One of them I can fill with hot drink, and carry it upstairs in total darkness and put it down without spilling a dropl The other sloshes around and I have to put a light on and carry it with total concentration. Mug 1 is shaped like #6 with a narrower neck than body, mug 2 is like #2 but more pronounced - it is a "gardener's mug and shaped like a plant pot.