How could I find the name of the guy in the Pacific Northwest that is doing the acrylic like flow glazing? My results so far are quite mediocre and I could use whatever guidance I could get from him
-
My old dentist bought some of his plates in a gift shop in Cannon Beach Or.-she has since moved to Idaho. I also saw his work at a show I was at 10 years ago-
You can add acrylic binder as MMR said or do it with colored slips as in thew video
Even if you found this artist he may not be willing to share Doc-not all are open to that idea of sharing info.
-
There is an Oregon Potters Association and a Washington State ceramics association as well. You might contact them.
The Oregon association has a very large show in April, more than 100 potters, I think. There are probably illustrated rosters.