This is a collection of all our member's albums. Click on the album name to see larger images. Click on the member name to go to a member's profile page to see all of the albums created by that member.
Local clay from my area. Porous at cone 04, vitreous at 03, slumping and bloating at 02. Glazed on the inside, the exterior is bare clay with terra sigillata (made from the same clay). The darker pieces are reduction cooled. Blacks are from reduced iron, not carbon or smoke.
Equine artist working in 3D fine art sculpture. I both sculpt, mold, and cast my own pieces in earthenware and am working towards producing my own sculpture also in English fine bone china here in the USA. Since 2003 I have been custom glazing equine ceramics sculpted by other artists and produced in various ceramic media. See more of my work at hynpatty.com .
English fine bone china 'Crusher' sculpted by Kitty Cantrell and produced by the Horse Gallery of Horsing Around of England. Claybody customized to add mane, braid, stud bridle and shoes myself, then under glazed to a dappled grey. Finished in satin glaze with low fired yellow gold buckles and white gold bit and shoes by Hyn Patty, 2006. Piece measures approximately 8 inches tall by 10 inches long - Private collection, sold for just under $4k at public auction. 2007 Realistic Equine Sculpture Society Best Custom Glazed Ceramic and People's Choice Awards.