Jump to content

Anchorage Wild Clay

Anchorage Wild Clay

Local clay from my area. Porous at cone 04, vitreous at 03, slumping and bloating at 02. Glazed on the inside, the exterior is bare clay with terra sigillata (made from the same clay). The darker pieces are reduction cooled. Blacks are from reduced iron, not carbon or smoke. 

  • Album created by Kelly in AK
  • Updated
  • 13 images
  • 1 image comment
  • 184 views
×
×