Custom glazed 'Carlito' in traditional scale fine bone china, sculpted by Brigitte Eberl and glazed to a black homozygous tobiano with sunburnt tips to his mane and tail. Blue eyes, ergots, wrinkles, sweat wrinkles, subtle hair pattern, etc and all fired in the kiln with satin finish and glossed eyes/hooves.  Lots of hair texture on this boy that I painstakingly hand painted into his blacks. There may be a hint of it showing in these photos but ultimately I just had to give up trying to find the right adjustment to make it pop well in my photos.  All work fired in the kiln between cones 04 and 016 using underglazes, china paints, and enamels by Hyn Patty, 2024.