Tyler Miller Posted June 17, 2014 Report Share Posted June 17, 2014 Terra sigillata is why I got into ceramics. I'm a fan of classical Greek and Roman art and learning to throw pots "like them" has been a goal of mine ever since I began playing with clay. But I'm bad at the classical style. "Athenian Vase Construction," by Toby Schreiber has been a great help in learning technique. But it's also really hard, especially the gloss. On ancient examples, it's like a glaze, the level of shine is so high. Check out this kylix, it's perfection: http://webapps.fitzmuseum.cam.ac.uk/explorer/index.php?oid=166270 I'd love to know how you guys approach pre-application surface treatment, application of the terra sig., and even firing (max cone range?) to get the glossiest finishes possible. I've got some articles from CAD and elsewhere, but I still can't seem to make it work that well. Link to comment Share on other sites More sharing options...
Wyndham Posted June 17, 2014 Report Share Posted June 17, 2014 Here's a guess, based on what the early pioneers did for dirt floors, Milk. After the floor was compacted, at which point I'm not sure, they poured milk from the cows(goats, sheep ?)onto the floor and polished them( don't know this part). In another thread, this is mentioned for sealing earthenware pieces(after firing). The oil and protein of milk might be what did it I think this might be a path you might look into. Wyndham Link to comment Share on other sites More sharing options...
Tyler Miller Posted June 17, 2014 Author Report Share Posted June 17, 2014 Cool! I'll bet your right that it's the oil and milk protein. I'll definitely give it a try. Link to comment Share on other sites More sharing options...
Min Posted June 17, 2014 Report Share Posted June 17, 2014 I have a friend from Hungary who used rendered elk fat when she lived there. Now she buys suet and renders that down to rub onto the fired pots. Pots are shiny but not overly so. A bit of an ick factor when I found out what she used. (her pots are decorative only) Link to comment Share on other sites More sharing options...
neilestrick Posted June 17, 2014 Report Share Posted June 17, 2014 I had a studio mate a long time ago who did nice glossy terra sig pots. He would put on 3 layers (if I remember right) of sig, burnishing with a stone between layers. The last layer was burnished with lard before firing. There was some historical reference for using the lard, and it lubricated the burnishing process. The firing was quite low, like maybe 1650F, to prevent the polish from burning off. The fired pots he then waxed and buffed, although they were quite glossy before waxing. Link to comment Share on other sites More sharing options...
Bob Coyle Posted June 18, 2014 Report Share Posted June 18, 2014 The pueblo potters out this way use a little fat and burnish the heck out of the pot till it has an almost mirror like finish. Then they do a reduction pit fire. seldom gets higher then maybe 1400F from what I read from people who inserted thermocouples into the pit. Ends up looking pretty much like your picture. Link to comment Share on other sites More sharing options...
Colby Charpentier Posted June 18, 2014 Report Share Posted June 18, 2014 We use mineral oil in the community studio when burnishing pots for pit fire. Might be a good substitution for pig fat, milk or some of that other stuff. Link to comment Share on other sites More sharing options...
Tyler Miller Posted June 18, 2014 Author Report Share Posted June 18, 2014 Thanks for the help guys. I'll give the lubricated burnishing method a try. Link to comment Share on other sites More sharing options...
Venicemud Posted June 18, 2014 Report Share Posted June 18, 2014 Years ago I took a workshop with Juan Quezada in Mata Ortiz and there we burnished with baby oil. I asked Juan why he used baby oil and he said (via a translater) because it smells better. Link to comment Share on other sites More sharing options...
JLowes Posted June 18, 2014 Report Share Posted June 18, 2014 Although I am quite certain this has no historic basis, I got nice results from the following method. I apply three coats of terra sigillata. I have burnished between coats and not, but always using the unprinted parts of a grocery store plastic bag. A friend uses a favorite bit of sweatshirt. We both get a high shine on the last coat. Then you bisque the pot. I have bisqued as high as cone 04 (not knowing any better), but cone 010 or 08 will keep more shine. Here comes the definitely non-historic part; wrap the pot round and round with cheap toilet tissue, keeping as close to the form as you can. Then wrap the pot and tissue in a layer or two of aluminum foil and seal it up tight. I fire this up to 1000 F (although paper burns at 451 F this gets it going better in my opinion), outside in a raku kiln (it can get smoky), and shut down the kiln, remove the pot, and let it sit and burn until the paper is exhausted and cool. I only found this picture as an example, but it shows the color and shine. John Link to comment Share on other sites More sharing options...
Bob Coyle Posted June 18, 2014 Report Share Posted June 18, 2014 Here is a vid of Maria at work. very basic technique but effective. Link to comment Share on other sites More sharing options...
Tyler Miller Posted June 19, 2014 Author Report Share Posted June 19, 2014 Bob, thanks for tracking down that wonderful video! I watched it all the way through last night and enjoyed it for a lot more than just the burnishing technique. Link to comment Share on other sites More sharing options...
Tyler Miller Posted June 27, 2014 Author Report Share Posted June 27, 2014 terrasigmystery.pdf I found this photo in Athenian Vase Construction I thought I'd share. I formatted it as a pdf because it gives better detail for its file size. If this is a problem, let me know and I'll shrink the phot and repost as a jpeg or rescan at greater detail and crop. It's of a kylix foot that broke off, revealing that the potter had used terra sig to join the stem to the bowl instead of conventional slip. The slip is glossy and black from reduction, despite it not being burnished. It appears there's more to Greek gloss than just burnishing. The gloss is in the slip itself. Puzzling, eh? terrasigmystery.pdf Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 27, 2014 Report Share Posted June 27, 2014 We did terra sig orange and black at the potters Council tour in Tuscany. We did not use any fat, stones nor spoons to burnish.First we formed the pieces and smoothed the surface with a wooden rib and metal rib. We applied thin layer to dried surface and polished with a soft sponge. Did it again and if desired, one more time. Let the surface dry in between coats and polishing.Note the sponge in the first picture. That is what we used for burnishing. this was one of two hands-on workshops as part of the Potters Council Tuscany Tour IV.this past year. Link to comment Share on other sites More sharing options...
Tyler Miller Posted June 27, 2014 Author Report Share Posted June 27, 2014 Marcia, thank you for explaining the process, those pieces are beautiful! Link to comment Share on other sites More sharing options...
Babs Posted June 27, 2014 Report Share Posted June 27, 2014 A piece of lambs wool rug works nicely Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 28, 2014 Report Share Posted June 28, 2014 The orange sig fluxes at 857 degrees C. All clays vary. This particular clay comes from the garden area at La Meridiana. two years ago we did numerous tests to nail down the exact temperature of the fluxing. That means that is won't take carbon when smoked in sawdust. The black is a more porrous slip. ball clay could be used. You have to test to get these effects. Marcia Link to comment Share on other sites More sharing options...
Tyler Miller Posted June 28, 2014 Author Report Share Posted June 28, 2014 Ah, I see. It occurs to me that we're talking about different things then. I'm interested in the historical method used in particular on Greek and Roman gloss. It's well known that the effect was achieved with one kind of slip, treated in two different ways. While I'm greatly appreciative of all the generous help all of you've offered, I did feel like there was still something missing. I spent the night last night researching the process and I think I've just about got it down. Testing to be sure. In the interest of sharing, I'll post what I've learned. FIrstly the black/red effect of Greek pottery comes from an oxidation, reduction, reoxidation firing schedule, with the peak temp achieved in reduction. The black sinters enough that it will not return to orange in oxidation. The surface treatment process as I had already known it from Toby Schreiber's book is that the pot was smoothed with a rib, then metal, then an iron-enhanced slip called miltos was added. The potter would then burnish the pot. The design was applied with a scraper or charcoal, then the "mystery slip" that later turns black was applied. Schreiber describes a process of using 80% ash water to 20% iron bearing clay, stirring it vigorously, pouring off the finest particles of clay and then evaporating the slip with heat until it was the consistency of cream. This is what I understood to be modern terra sigillata, however, in my experience they don't behave the same. I can get a warm, shiny glow with terra sig, but I can't get the level of gloss of Greek red-figure. It is truly like a glaze. I welcome correction, but I've never seen a modern terra sigillata get that level of mirror polish, John Lowes' example above is the closest I've seen. However, the broken kylix bottom I posted above also gets a truly high polish comparable to JLowes' with nothing more than basic slip-joining technique. So, I spent tonight feeling a little at a loss, despite my appreciation for how much information has been offered up. I did quite a lot of reading and I think I've come to some conclusions about the process that may be of interest. Firstly, I have a feeling the ash water in the slip is doing more than simply levigating the particles, I think there's a level of alkali high enough to increase the level of sintering to a nearly non-porous surface. Then, illite is repeatedly mentioned in articles as a key component of Greek gloss. It's not universally present in modern, commercially produced clays, and I think this has somethign to do with the difference between warm, shiny glow of modern terra sig. and the high polish of unburnished Greco-Roman gloss. I welcome correction on any of the conclusions I've come to, and I will be testing my theory with a oxy-red-ox firing in late July/August. I will post results here. Thanks again for all the help. I apologize if I've caused any confusion in what I'm after. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 28, 2014 Report Share Posted June 28, 2014 No confusion. I am aware of the many theories of red and black pottery from the Ancients. In this case the tradition from the first use of controlling the atmosphere to re-oxidize to get the red (orange) to turn orange again does use the similar idea of one that sinters, i..e fluxes enough to seal and the other remaining porous. I have a good book called "Looking at Greek Vases" by Rasmussen and Spivey from Cambridge University press.1991 At any rate, one uses the kiln atmosphere and the other uses the kiln to reach the sintering temperature and then post reduction. Interesting that both give the same coloration but use different reduction process. I don't think it is caused from milk, lard, etc. It is done with the firing process and the knowledge of the sintering temps of the slips. Marcia Link to comment Share on other sites More sharing options...
Angie Days Posted June 29, 2014 Report Share Posted June 29, 2014 There are two things you have to take into account: first, the photo is retouched and the lighting design is made with perfection. Have you ever seen a Kylix in a Museum? The brightness is silky, not as shinny as in the photo. Second, some natural red clays produces it’s own shine even without polishing, the brightness is lower but it’s still there. Terra sigillata has a rule: higher temperature, less luster. Try working with a very plastic natural clay with low fire temperature and see the difference. P.S. In the book the photo is not as shinny as it looks in your photocopied page. some links you'll find interesting: http://books.google.com.mx/books?id=L-DYdyXXMy8C&printsec=frontcover&source=gbs_ge_summary_r&cad=0#v=onepage&q&f=false http://www.jstor.org/stable/497642 http://iweb.tntech.edu/wpitelka/professional/terra_sig.htm I just found this amazing information: NEW EVIDENCE FOR THE NATURE OF THE ATTIC BLACK GLOSS http://www.ims.demokritos.gr/archae/publication_pdf/attic/black/archaeometry.pdf Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 29, 2014 Report Share Posted June 29, 2014 Great resources, Angie. I'd like to add Ann Shepherd's Ceramics for the Archeologist and Fred Matson's Ceramics and Man. Matson's disciples continue to present Current Research on Ceramic Materials at the AM. Anthropological Association Meetings annually. I have given several papers at these meetings on my research in Spain and Central Asia. his book is a bible for current research in the last quarter of the 20th century. Marcia Selsor Link to comment Share on other sites More sharing options...
Tyler Miller Posted June 29, 2014 Author Report Share Posted June 29, 2014 Marcia, I get the feeling I may have trod on some toes with my reply. If this is the case, I deeply apologize. I do see where you're coming from now. My concern was that you were advocating your post reduction method as historical. It was my impression that the three stage firing was universally accepted as how it was done, and I had misunderstood the kernel of your posts--the importance of the sinter was what you were getting at, rather than the importance of the colour. The confusion was mine. I was thinking you were advocating it as an historical technique, and my post was based on thinking you had got the sintered/non-sintered portions and the means of achieving colour backwards. I do greatly respect your opinion. I will definitely make an attempt to track down the books you recommend in your most recent post. I've found Ann Shepherd's book in pdf format. Thank you for the recommendation. Ceramics and Man, however, seems to be out of print and my usual sources such as abebooks.com etc. don't seem to yield any results. Perhaps you could summarize the relevant portions or recommend a book seller? I have read through "Looking at Greek Vases" and I'm not sure there's anything out of keeping with what I've said in it. It mentions post-firing colours, however I interpreted this to mean paint. The illitic comments I made came from this article: http://onlinelibrary.wiley.com/doi/10.1111/j.1475-4754.1982.tb00994.x/abstract Angie, I've handled kylices in person--a professor of mine had a small collection bequeathed to him in the late 1960s by a private collector while he was at Oxford. I can assure you that they can be that glossy. I also highly doubt that the previously linked amphora photographed in a museum setting was photoshopped. You can almost make out the reflection of the photographer in the black gloss. (link here: http://en.wikipedia.org/wiki/Red-figure_pottery#mediaviewer/File:Neck-amphora_swordsman_Louvre_G216.jpg) I also own Athenian Vase Construction. See? I can assure you that the photograph of the broken kylix bottom is quite shiny. But my point wasn't about the level of shine per se, but rather the fact that it achieved a shine at all, given that the slip would have been applied with no more care than what I would put into applying a jug handle. I found that fact alone remarkable. I do appreciate the links you've posted. I've seen the JSTOR article before as well as the link on terra sigillata, they both have gone into my efforts with terra sig, and into my posts on this thread as well, even if I've not been properly articulate. I'm afraid I cannot view your last link, it comes up as a 404 not found. I do appreciate you guys taking the time to reply. Again, thank you for your help and if I've bruised an egos or stepped on any toes, I deeply apologize. Terra sigillata is certainly the turf of "ye twain," and I yield to your expertise. -Tyler Link to comment Share on other sites More sharing options...
PeterH Posted June 29, 2014 Report Share Posted June 29, 2014 Tyler, Try www.bookfinder.com for Fred Matson's Ceramics and Man, they list several copies, Link to comment Share on other sites More sharing options...
CarlCravens Posted June 29, 2014 Report Share Posted June 29, 2014 I just bought Ceramics and Man (paperback) through Amazon for $8 (including shipping). Link to comment Share on other sites More sharing options...
Tyler Miller Posted June 29, 2014 Author Report Share Posted June 29, 2014 Yeah, I feel a little stupid. I didn't get any results because I was looking for "Cermics and Man" by Batson. Ordered a copy via Amazon. Thanks for pointing that out, guys. Link to comment Share on other sites More sharing options...