Started a firing last night, something told me no right. I turned it off and waited til it cooled but, not before I noticed top coil was not firing. Later found that the SC-20 fuse on the right side on top layer was blown! No replacements until this morning with a walk to Ace Hardware. Firing now
- Show previous comments 1 more
-
I am glad you listen to your gut, I get gut feeling also. I almost lost a lot of money not listening to my gut. It was a big decorating job of a well know local celebrity. They had fired the decorator and wanted me to take over the job. I didn't want to do it but friends and relatives talked me into it. Before I had any time or money invested in it they decided to give the last decorator another chance. I was so relieved, later in the year I found out that they didn't pay any of their subcontractors. I could have lost $50,000 on a job like that. I don't let anyone talk me in to something I have a bad gut feeling about anymore. Happy birthday, I will be 67 October 15. Denice
-
8 pm, Kiln dropping ^5 right now,
best,
Pres