Glaze firing started yesterday, kiln open on low at 5pm, 8pm closed with no plugs at high, 12am backed to 3/4, checked at 3am,up at 7 to check , ^6 nearly down-turned all to high, 7:20 am ^6 is down, kiln cut back to 30% turn off soon by noon.
-
When do you sleep?
-
Wen to bed at 12 am, woke to check the kiln at 3, back to bed til 7.