Marcia Selsor got a reaction from Pyewackette for a gallery image, Cone 9 Celedon Glaze
Celedon ^9 reduction using burnt umber for a colorant.This was the color I wanted for ^6 Ox.
I did many tests and came up with the recipe posted in the previous Faux celedon example.
-
Marcia Selsor got a reaction from Pyewackette for a gallery image, newly learned throwing technique
I tried a technique I saw on youtube. Using a heat gun, which I already use on the outing of pot for the crackled surface, the inside walls stiffen enough to really puch pulling up and forming with great control.
-
Marcia Selsor got a reaction from oldlady for a gallery image, Cone 9 Celedon Glaze
Celedon ^9 reduction using burnt umber for a colorant.This was the color I wanted for ^6 Ox.
I did many tests and came up with the recipe posted in the previous Faux celedon example.
-
Marcia Selsor got a reaction from oldlady for a gallery image, rakuhorserainbowsm
tested some new glazes. I like this one.
-
Marcia Selsor got a reaction from Pieter Mostert for a gallery image, From Sept. workshop and home firings 2015
-
Marcia Selsor got a reaction from rakukuku for a gallery image, Obvara Looking Up From Sept. workshop and home firings 2015
obvara firing on a smooth terra sig surface
-
-
Marcia Selsor got a reaction from rakukuku for a gallery image, obvarabrsq copy
One of the newest pieces of Obvara. 11" x 10.5"
-
-
Marcia Selsor got a reaction from Min for a gallery image, newly learned throwing technique
I tried a technique I saw on youtube. Using a heat gun, which I already use on the outing of pot for the crackled surface, the inside walls stiffen enough to really puch pulling up and forming with great control.
-
-
-
-
-
-
-
-
-
Marcia Selsor got a reaction from ChenowethArts for a gallery image, obvarabrsq copy
One of the newest pieces of Obvara. 11" x 10.5"
-
Marcia Selsor got a reaction from rayaldridge for a gallery image, rakuhorserainbowsm
tested some new glazes. I like this one.
-
Marcia Selsor got a reaction from Sallyd for a gallery image, Cone 9 Celedon Glaze
Celedon ^9 reduction using burnt umber for a colorant.This was the color I wanted for ^6 Ox.
I did many tests and came up with the recipe posted in the previous Faux celedon example.
-
Marcia Selsor got a reaction from Sara for a gallery image, obvara3 3:15copy
A few pieces from my first Obvara firing of the year.
-
Marcia Selsor got a reaction from Sara for a gallery image, Obvara6 3:15copy
A few pieces from my first Obvara firing of the year.
-
Marcia Selsor got a reaction from Sara for a gallery image, obvara12.3:15copy
A few pieces from my first Obvara firing of the year.
-
-
-
Marcia Selsor got a reaction from Babs for a gallery image, texturedpotsmall
working on potential pieces for an obvert firing
-
-
-