  1. Finally going to be firing with my power burner tomorrow, had a month with no free time at all :( let's hope it works.

    1. Show previous comments  8 more
    2. High Bridge Pottery

      High Bridge Pottery

      Had it open and I managed to crack about 25% of the pots. It did go from room temp to 400c in 30 min on the lowest setting. I need a smaller burner for the very start I think. All cone 9's and 10's down except right at the flue where cone 10 was starting to go.

    3. Joseph Fireborn

      Joseph Fireborn

      stinks about the pots cracking but part of testing! how did the ones that didn't crack turn out? Wonderful stuff? You will figure out the firing stuff, look how far you have came!

    4. glazenerd

      glazenerd

      Joel- consider yourself a Trekkie- boldly going where no potter has gone before.

×
×