Pagan Clay Posted December 1, 2023 Report Share Posted December 1, 2023 Hi y’all! Beginner ceramist here! I have some over glaze decals and lusters I want to try, but I’m in a community studio that won’t fire that low (come 018-019). I have however found a friend at the studio with a personal kiln willing to fire this low. However she uses bars instead of cones. How can I convert the cones to bars so that she knows how to fire them? Is there even a way to do this? Here’s the decal for reference- https://www.chinaclayart.com/collections/overglazedecal/products/gold-bee Thanks in advance for your time, help, and input! Quote Link to comment Share on other sites More sharing options...
Dick White Posted December 1, 2023 Report Share Posted December 1, 2023 The mini-cones and pyrometric bars are more-or-less equivalent. Some would argue that the bars are more accurate, in that they cannot be shifted to one end or the other to slightly change the outcome, but if her bars are 018 or 019, they will be fine for your work. Pres 1 Quote Link to comment Share on other sites More sharing options...
PeterH Posted December 2, 2023 Report Share Posted December 2, 2023 (edited) Looking at the table Orton Cone Chart I'm surprised/confused that the heating rate assumed for small cones is so much faster than for regular ones. https://www.ortonceramic.com/_files/ugd/7c9d79_11dd303c800c46b08d3a05178a02d99c.pdf Small at 300°C/hr and regular at 15°C/hr, 60°C/hr & 150°C/hr. Is there a simple explanation? I note that a footnote states the small cones were fired in a gas kiln, while bars are typically used in a electric kilnsitter. Edited December 2, 2023 by PeterH Quote Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted December 2, 2023 Report Share Posted December 2, 2023 (edited) The blurb on the right says (incorrect information - see Hulk's next post) Quote Temperatures shown for small cones were determined using a heating rate of 300C/hr (540F/hr) in a gas fired kiln. Small cones will come close to duplicating the results of self-supporting cones if mounted upright, properly simulating the position of a self-supporting cone. Typically, small cones will deform 7-10 degrees C earlier than a self-supporting cone, so the temperature values for a self-supporting cone can be used to determine an equivalent small cone temperature by subtracting 7-10 degrees C (or 12-18 degrees F). Edited December 3, 2023 by High Bridge Pottery Rae Reich and PeterH 2 Quote Link to comment Share on other sites More sharing options...
Hulk Posted December 2, 2023 Report Share Posted December 2, 2023 There had been discrepancies in Orton's online materials regarding small cone deformation temperatures*. I used small cones for the kiln sitter (prior kiln), and I like them. They are a tiny bit cheaper. Here's an excerpt from the message I received from Orton Engineer (circa March 2020): Dear Sir, Thank you for contacting Orton to draw our attention to some incorrect information on our website. The small cones do in fact deform after the large cones. We have updated the information on the website. See also this thread (start at the bottom/end) Kiln Sitter cone for witness cone - Studio Operations and Making Work - Ceramic Arts Daily Community *There still are! The 2016 cone charts are all "backward" See the small cone page, SMALL CONES | Orton Ceramic "Small Cones used on the kiln shelf deform at about 9°F after Large or Self-Supporting Cones of the same number." It's just because the small ones are smaller - the cones are same material; same reason a large candle will slump in hot weather before a small one. Rae Reich, Magnolia Mud Research, High Bridge Pottery and 1 other 4 Quote Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted December 6, 2023 Report Share Posted December 6, 2023 I was told that another part of the reason for the small cones deforming later is that they have the weight from the kiln sitter arm applied to them, where self supporting and regular cones don’t. So the later melt is to help compensate for that, as they’re being used as a shutoff. Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.