Rebekah Krieger Posted November 4, 2023 Report Share Posted November 4, 2023 My zinc has been a huge problem. I have used a mortar and pestal by hand for small amounts but I have a decent amount. Is there an easier way to process this at home without having any special equipment? Quote Link to comment Share on other sites More sharing options...
Min Posted November 4, 2023 Report Share Posted November 4, 2023 Whiz it in a blender. Either dry then wait for the dust to settle before opening the blender or with some water then pour it out and add a bit more water to get the residuals. Rae Reich and Magnolia Mud Research 2 Quote Link to comment Share on other sites More sharing options...
Dick White Posted November 4, 2023 Report Share Posted November 4, 2023 The easiest way I have discovered to process it is... don't. Head on over to the big river in S. America dot com and order cosmetic grade zinc oxide in 4 lb bags. It is already finely ground. Upon opening, store it in an airtight jar. Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Pres Posted November 5, 2023 Report Share Posted November 5, 2023 I use a stick blender with a plastic cover seal, wait until the dust settles, and will be fine. best, Pres Rae Reich 1 Quote Link to comment Share on other sites More sharing options...
Mark C. Posted November 5, 2023 Report Share Posted November 5, 2023 I have a thrift store blender in. shop for this-works like charm Pres and Rae Reich 2 Quote Link to comment Share on other sites More sharing options...
JohnnyK Posted November 5, 2023 Report Share Posted November 5, 2023 I have also found that a small coffee grinder works pretty well. Pres 1 Quote Link to comment Share on other sites More sharing options...