Camping, kayaking, family, travel, Art in general. I have a small studio in my garage. Two electric kilns, two wheels, wedging table etc. I am primarily interested in cone 6 Ox. but like to see what is going on at all ranges. Read about ceramics voraciously and love the feel of the clay and throwing. Have to admit that my greatest joy is in the making, not the glazing. That said I do mix my own glazes, some of my own formulas, some borrowed. Retired from teaching art, in 2009 after 36 years, taught ceramics 34 of those years.
Posted answers to Potters Quiz of the week 3, Sorry I was late, but yesterday was tiring with lots of driving and a 3am turn off of the glaze firing. At least it got me out of the house until today-no peeking.