I saw a post from you in 2018 that said you fire many different types of pottery together. I did that and now I am completely unsure of what is my low fire and what is my stoneware. Some of it I can tell apart bc I can see the grog but some of the stoneware doesn’t have grog! I don’t know what to do. I don’t know what I was thinking. I could tell them apart by the color when they were wet. Most of my pieces are utilitarian. Thank you so much.
- Show previous comments 1 more
-
This is a conundrum! I've run into a similar situation. I use low fire white clay and mid-range porcelain and have bisque fired them together. I can tell the difference before but not always after! I'm doing my best to keep them separate but I don't always trust my memory.
A couple of solutions I just thought of would be to
1. photograph what's what or
2. somehow indiscriminately mark one from the other.
Just my two cents.
-
@MADcrafter Maybe come up with a system of symbols that you can carve into the bottom of your pieces next to your signature to differentiate them
-
You could try the "stick the tongue on" test and the low temp clay should not "stick" so much as it is now not so porous.