This is my first time firing my mug in a kiln (I use Mid fire clay)
I used these segment:
C1 (160c) 60min
C2 (500c) skip
C3 ( 1240c) 20 min
C4 (room temperature)
Each time I use my kiln my mug breaks
Do you have any advice?
Hello,
It is my first time making pottery and I got a small electrical kiln and I dont have any clue of how to use the controller to glaze fire.
https://www.desertcart.ae/products/528588673
please help