  1. I will try programming it this way
  2. https://www.desertcart.ae/products/425093753 This is the clay I am using. around 1hr and a half to cool dowm
  3. This is my first time firing my mug in a kiln (I use Mid fire clay) I used these segment: C1 (160c) 60min C2 (500c) skip C3 ( 1240c) 20 min C4 (room temperature) Each time I use my kiln my mug breaks Do you have any advice?
  4. I tried firing it today at 1240c but my mug broke I put the Kiln in my garage and it is on a ceramic floor
  5. Can’t thank you enough
  6. Thank you, I will try
  7. No it did not come with a manual and I do not really know how to program the controller( the controller just specifies Pv and Sv
  8. Hello, It is my first time making pottery and I got a small electrical kiln and I dont have any clue of how to use the controller to glaze fire. https://www.desertcart.ae/products/528588673 please help
×
×