Thanks for the advice Neil. But I'm 100% sure that the pieces were completely dry. They were produced 1 month ago.
Yes, I will definitely preheat for the next firings. But if this problem persists, do you suggest contacting a technician?
thank you again.
Amanda
Hello @neilestrick!
Oh big explosions! The pieces literally exploded completely.
My first thought was: - probably the temperature range up too fast? but on the second firing it happened again and I think maybe it's a cooling problem?
Today I will do a glaze firing test with the pieces that have survived the last 2x bisque firings.
Thank you,
Amanda
Thank you so much for your answer Kelly!
I will definitely try to use a pre-heat program. By the way, I don't have a vent, so I keep my first peephole open. With a pre-heat program, should I continue like this? Or do you suggest anything else?
Also thought it might be a coolingdown issue but let's see the next chapter Lol. thank you again!
Hello guys!
I finally got my first kiln. It's a Skutt electric kiln. I have already did 2x bisque firings and unfortunately it was not a success.
I programmed my bisque firing using CONE 04 - NO PRE-HEAT - NO HOLD, and for the second time I lost large pieces that I put in the same place inside the kiln.
Any tips or suggestions for my third firing? What should I do to not lose some pieces again?
Thank you, Amanda! =)