Would anybody be interested in sharing success / good experience with the commercial glazes?
I have a lot of them; mostly Coyote, Potters Choice, Amaco, Laguna.
It takes a lot of experimental firings to find out when they look the best.
I do realize that it also depends on the type of the clay we use, the firing schedule, etc., but there are definitely some things we could share with each other so we would not "discover America" with every new glaze we use.

As an example and as the first person to share: This is Coyote Butterscotch Shino MBG086 ^6
It looks the best on a rough surface. You can see the difference: inside the surface was smooth, but outside I used some slip to create a texture.
The dark brown strip is just a thin layer of a Potters Choice glaze. Slow firing to ^6.


Attached File  100_2106.JPG   508.98KB   76 downloads

#2 Diane Puckett

Diane Puckett

    Advanced Member

  • Members
  • PipPipPip
  • 398 posts
  • LocationAsheville, NC

Posted 04 July 2013 - 06:20 AM

Great idea! I would be especially interested in photos of layered glazes, including the ones that did not turn out well.

Nice pot, BTW.
Diane Puckett
Dry Ridge Pottery

#3 Claypple

Claypple

    Advanced Member

  • Members
  • PipPipPip
  • 261 posts
  • LocationReno, NV

Posted 04 July 2013 - 10:07 AM

I would be especially interested in photos of layered glazes, including the ones that did not turn out well.


Here is some layering: Attached File  100_2079.JPG   436.14KB   46 downloads
Coyote Croc Blue MBG 009 over Coyote Red MBG 019. Next time I will make a much wider overlap.

#4 Nancy S.

Nancy S.

    My day job pays for my clay habit

  • Members
  • PipPipPip
  • 232 posts
  • LocationHarrisburg area, PA

Posted 06 July 2013 - 11:32 AM

I have added glazing info to my pottery gallery online, if anyone's interested -- it's mostly Coyote Glazes, but I'll be adding more Amaco and Mayco colors soon (once I test them and get photos)!

 

http://smg.photobuck...html?sort=6&o=0



#5 Pugaboo

Pugaboo

    Lifetime artist 3rd year potter

  • Members
  • PipPipPip
  • 1,039 posts
  • LocationHelen, GA

Posted 06 July 2013 - 11:51 AM

Very nice pictures on your site. I'll definitely be back to visit it again.
The world is but a canvas to the imagination - Henry David Thoreau

#6 Nancy S.

Nancy S.

    My day job pays for my clay habit

  • Members
  • PipPipPip
  • 232 posts
  • LocationHarrisburg area, PA

Posted 06 July 2013 - 03:52 PM

Very nice pictures on your site. I'll definitely be back to visit it again.

Thank you!! I just added a few more I found. :)



#7 Claypple

Claypple

    Advanced Member

  • Members
  • PipPipPip
  • 261 posts
  • LocationReno, NV

Posted 06 July 2013 - 04:36 PM

Thank you Nancy! That is just perfect!



#8 kathleenMK

kathleenMK

    Newbie

  • Members
  • Pip
  • 4 posts
  • LocationTexas

Posted 06 July 2013 - 05:39 PM

I've had good luck at school with the Amaco Potter's Choice  and Coyote glazes. As you  know they have to be thickly coated. (The kid who made the biggest mess actually made one of the best bowls we donated to the Empty Bowls project.)

Try layering those Coyote Shinos over the black for some interesting effects.

 

These cones 6 oxidation glazes make me in less of a hurry to built a gas-fired kiln.



#9 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 07 July 2013 - 01:10 AM

I'm moving away from commercial glazes....
But was quite pleased with coyote shino. Over potters choice tenmoku

LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#10 Roberta12

Roberta12

    Advanced Member

  • Members
  • PipPipPip
  • 469 posts
  • LocationColorado

Posted 08 July 2013 - 01:48 PM

I'm moving away from commercial glazes....
But was quite pleased with coyote shino. Over potters choice tenmoku

I mostly mix my own but I do like Coyote Goldenrod shino.  It is so nice over a speckly clay body.  I will see if I can get some pics loaded.   I have not been able to find a recipe to replicate Goldenrod.  So that is one I still purchase. 



#11 Roberta12

Roberta12

    Advanced Member

  • Members
  • PipPipPip
  • 469 posts
  • LocationColorado

Posted 08 July 2013 - 01:54 PM

I hope this picture loads correctly.   The glaze on the interior of this piece is Goldenrod shino.  The rim is one I mixed and sprayed over it on the rim.  

Attached Files



#12 Bill T.

Bill T.

    member

  • Members
  • PipPipPip
  • 78 posts
  • LocationGilmer, Texas

Posted 08 July 2013 - 09:13 PM

I mostly use Coyote and Amaco Potters Choice along with some I mix and a few from Opulence.  My favorite from Coyote is Red Gold.  Started buying it in bulk and find it gives different effects by dipping.  The bird house is floating blue over red gold on the top and Potters choice Albany slip on the bottom (brushed)

Attached Files



#13 Claypple

Claypple

    Advanced Member

  • Members
  • PipPipPip
  • 261 posts
  • LocationReno, NV

Posted 08 July 2013 - 10:29 PM

Ah, both are gorgeous! Thanks for sharing!

 

 

 



#14 Roberta12

Roberta12

    Advanced Member

  • Members
  • PipPipPip
  • 469 posts
  • LocationColorado

Posted 08 July 2013 - 11:32 PM

I mostly use Coyote and Amaco Potters Choice along with some I mix and a few from Opulence.  My favorite from Coyote is Red Gold.  Started buying it in bulk and find it gives different effects by dipping.  The bird house is floating blue over red gold on the top and Potters choice Albany slip on the bottom (brushed)

Oh my gosh! Beautiful combo!  I have some red gold in a bucket, but never thought about putting floating blue over it like that.  I really like it.  Thanks for sharing.  Was that a floating blue that you made yourself?

 

Roberta



#15 Bill T.

Bill T.

    member

  • Members
  • PipPipPip
  • 78 posts
  • LocationGilmer, Texas

Posted 09 July 2013 - 09:31 PM

 

I mostly use Coyote and Amaco Potters Choice along with some I mix and a few from Opulence.  My favorite from Coyote is Red Gold.  Started buying it in bulk and find it gives different effects by dipping.  The bird house is floating blue over red gold on the top and Potters choice Albany slip on the bottom (brushed)

Oh my gosh! Beautiful combo!  I have some red gold in a bucket, but never thought about putting floating blue over it like that.  I really like it.  Thanks for sharing.  Was that a floating blue that you made yourself?

 

Roberta

 

Yes, just one of the standard recipies. 



#16 Claypple

Claypple

    Advanced Member

  • Members
  • PipPipPip
  • 261 posts
  • LocationReno, NV

Posted 31 July 2013 - 08:55 PM

Laguna "Desert Sand" and "Peacock"

Duncan "Sephia Brown"

Coat&Stroke "Java Bean" and "Blue Grass"

Coyote "Red Gold"

 

No overlaying. 

Attached Files



#17 weeble

weeble

    Advanced Member

  • Members
  • PipPipPip
  • 121 posts
  • LocationOregon Coast

Posted 01 August 2013 - 05:23 AM

Claypple, which of Laguna's 'Peacock' glazes are you using?  They've got two in the cone 5-6 line, I've used MS#27 a lot.  Its a crazy glaze, over some clay it is more green, over the Laguna B-mix it goes blue-green, on "Frost" porcelain it is straight blue.  (Someone with more glaze formulation knowledge could probably say exactly what's going on, but I'm stuck using commercial glazes.)  A layer of white under it does some fabulous texture things... I've used "Colonial White" under, with the MS#27 over and got a really crazy roiling water look.  


Maryjane Carlson

Whistling Fish Pottery

#18 Claypple

Claypple

    Advanced Member

  • Members
  • PipPipPip
  • 261 posts
  • LocationReno, NV

Posted 01 August 2013 - 09:06 AM

I am using MS-95. On the vase I showed it is in the very center over Speckled Buff clay and it looks like a deep water of Tahoe.

It is interesting what you said. I will try it over the white glaze now.

I, too, wish there were a way to find out what are the ingredients in the commercial glazes.

Some of them are very unique and beautiful. 



#19 ayjay

ayjay

    Advanced Member

  • Members
  • PipPipPip
  • 492 posts
  • LocationHampshire, UK.

Posted 03 November 2013 - 10:59 AM

This is one from my most recent firing that I quite like.

 

On white stoneware, Amaco Potters Choice  - alternate stripes of Ironstone and Waxy White in the diagonal grooves and then two alternate coats each of Toasted Sage and Ancient Jasper, (in that order), and a little Jen's Juicy Fruit  (not Amaco) on the rim.

 

Attached File  IMG_2971-c-r.jpg   588.41KB   15 downloads

 

 

 

 



#20 nancylee

nancylee

    Advanced Member

  • Members
  • PipPipPip
  • 435 posts
  • LocationUpstate NY

Posted 03 November 2013 - 12:22 PM

This is my favorite: hobbit under and blue snowflake on top. It is best on cone 6 clay we call 60, but is good on B mix also. Attached File  image.jpg   207.98KB   19 downloadsAttached File  image.jpg   207.98KB   19 downloadsAttached File  image.jpg   115.2KB   9 downloads

Attached Files


Nancy
Northern Woods Pottery
www.northernwoodsstudio.blogspot.com




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users