Advice on buying a used kiln


  • Please log in to reply
11 replies to this topic

#1 jemenfous5

jemenfous5

    Member

  • Members
  • PipPip
  • 10 posts

Posted 10 February 2013 - 07:11 PM

Hello-

I found a kiln on craigslist I'd like to purchase, however, I'd have to drive several hundred miles to pick it up. (It's a very good deal. $850 for an L&L Easy Fire E23-S-3 along with a slab roller and shimpo 1/3 hp M250 wheel). Therefore, I want to be sure its in working order before I drive all that way. I've attached a photo of the interior of the kiln. Can anyone tell me if the condition of the brick and elements looks up to par? This is my first kiln so I'm not exactly sure how it should look.

Thanks,
Kyle

Attached Files



#2 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,682 posts
  • LocationNorthern Virginia

Posted 10 February 2013 - 07:55 PM

You can't tell by looks alone, although the elements seem to show no signs of glaze drips or other issues and the brick work looks to be in good shape. You'll only really know when you plug it in and fire it up. I'd ask the owner for a copy of his kiln log; that would show you the number of times fired, to what cone, etc. which will be helpful in figuring out how much life is left to the elements and other replaceable parts.

#3 Denice

Denice

    Advanced Member

  • Members
  • PipPipPip
  • 1,229 posts
  • LocationWichita, Kansas

Posted 10 February 2013 - 08:02 PM

It sounds like a good deal with all of the other equipment your getting with the kiln you could afford to have someone rewire it for you. A used kiln in that good of shape would cost about 600 dollars here and you still might need to rewire it after you spent 600 for it. There are no guarantees in life but I would buy that combo in a heart beat. Denice

#4 atanzey

atanzey

    -

  • Members
  • PipPipPip
  • 147 posts
  • LocationSouth-Central Pennsylvania

Posted 10 February 2013 - 08:06 PM

Honestly, for that price, buy it and change the elements! Great deal, if the electronics work. I bought a used L&L and didn't even try the elements that were in it - I immediately change them. It was pretty easy, and gave me an opportunity to make sure the element holders were cleaned out and all was well with the bricks. I did replace one or tow pyrometers, a couple of element holders and a couple of bricks.

Alice

#5 jemenfous5

jemenfous5

    Member

  • Members
  • PipPip
  • 10 posts

Posted 10 February 2013 - 08:06 PM

It sounds like a good deal with all of the other equipment your getting with the kiln you could afford to have someone rewire it for you. A used kiln in that good of shape would cost about 600 dollars here and you still might need to rewire it after you spent 600 for it. There are no guarantees in life but I would buy that combo in a heart beat. Denice


Thanks, I'm leaning toward buy it. The equipment belonged to her deceased mother, so she doesn't have a 6-50 outlet to plug it into. I have to off looks alone.

#6 justanassembler

justanassembler

  • Members
  • PipPipPip
  • 248 posts
  • LocationBaton Rouge, LA

Posted 10 February 2013 - 08:32 PM


It sounds like a good deal with all of the other equipment your getting with the kiln you could afford to have someone rewire it for you. A used kiln in that good of shape would cost about 600 dollars here and you still might need to rewire it after you spent 600 for it. There are no guarantees in life but I would buy that combo in a heart beat. Denice


Thanks, I'm leaning toward buy it. The equipment belonged to her deceased mother, so she doesn't have a 6-50 outlet to plug it into. I have to off looks alone.


Based on the model # and voltage you could look up on L&L's www site the proper resistance for the elements and check them with a meter when you get there--its simple and a good excuse to buy an inexpensive multi-meter and learn to use it--its really easy. This will @ least tell you if the elements are good or not.

#7 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,212 posts
  • LocationRed Lodge, Montana

Posted 11 February 2013 - 08:20 AM

sounds like a great deal and the kiln bricks look like they are in good shape.
Download a manual online. Have the correct wiring installed. Then you can check it out and replace anything necessary.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#8 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,908 posts
  • LocationGrayslake, IL

Posted 11 February 2013 - 11:13 AM

Those elements are most likely worn out. When the coils start laying over on each other it's a very good sign that they are done. Plan on replacing them. It's still a good deal, even with new elements. A new set will cost around $200.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#9 Mossyrock

Mossyrock

    Advanced Member

  • Members
  • PipPipPip
  • 203 posts
  • LocationHigh Point, NC

Posted 12 February 2013 - 11:07 AM

Just curious....why would the kiln have three exhaust vent tubes coming out of it? I have an L&L and it has only one.
Brenda Moore
Mossy Rock Creations
High Point, NC

#10 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,908 posts
  • LocationGrayslake, IL

Posted 12 February 2013 - 11:31 AM

Just curious....why would the kiln have three exhaust vent tubes coming out of it? I have an L&L and it has only one.


No clue about all the ducts. Very odd.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#11 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 3,030 posts
  • LocationCentral, PA

Posted 12 February 2013 - 01:10 PM

Hello-

I found a kiln on craigslist I'd like to purchase, however, I'd have to drive several hundred miles to pick it up. (It's a very good deal. $850 for an L&L Easy Fire E23-S-3 along with a slab roller and shimpo 1/3 hp M250 wheel). Therefore, I want to be sure its in working order before I drive all that way. I've attached a photo of the interior of the kiln. Can anyone tell me if the condition of the brick and elements looks up to par? This is my first kiln so I'm not exactly sure how it should look.

Thanks,
Kyle


Kiln body looks to be in good shape, the element holders show that the kiln has been used heavily(coloration as compared to new from vitrification of holders), the elements definitely look like they are heavily oxidized. Considering the price, size and condition, I would go for it if it matches your needs.
Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . . http://picworkspottery.blogspot.com/

#12 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 12 February 2013 - 04:31 PM

Don't listen to them! It's an awful deal! Get out of it while you can. Please let me know how I can contact them.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.