idahogem Posted October 14, 2020 Report Share Posted October 14, 2020 I am new first post so I hope I am in the right place. So my mom had a shop for over 25 years she did ceramics and porcelain. She was a master and did wonderful work. She did a lot of lusters and fine metals. She has become blind and I am tasked with Selling her things. I found a Box with 45 bottles of HANOVIA lusters and gold nost unopened in over 15 different colors including white gold mother of pearl gold essence halo gold.... I did some research and came up with very little I got the history of the company was unable to find when it closed other than a forum post from 2007 mentioning these were no longer available and only about 3 on the web for sale. my understanding is this was the artists choice at the time. So these are over 10 years old always stored in the house. My question is are these still usable or valuable. I have nothing to compare to I was hoping to find something to value them or someone who wants them or a correct forum where I could find more information. Here is the list thank you for your consideration. HANOVIA 1/2OZ MOTHER OF PEARL 7 OPAL 2 GOLD ESSENSE 2 HALO ROSE RED 1 HALO GOLD 6 LUSTER WHITE 3 HALO LUSTER TOPAZ 1 SLATE GREY 1 2 GMS MICRO PT (CANT READ) 1 BRIGHT PLATINUM #05 7 BRONZE #16 1? COPPER 3696 3 BRIGHT GOLD #N 2 1/4 OZ BLUE 1 IRRIDECENT LIGHT BLUE 1 TOURQUOISE BLUE 1 GREEN 3 LUSTER GREEN 1 LUSTER BROWN 3 Quote Link to comment Share on other sites More sharing options...
Mark C. Posted October 14, 2020 Report Share Posted October 14, 2020 These are old luster and generally do not go bad unless stored in high heat areas (evaporation) Most are just not made anymore and have not much value They tend to stay just fine for long periods in terms of value the gold still has some value as well as the paltinum the others are less so. I would try to sell the whole lot as one so you do not get stuck with the lesser ones Quote Link to comment Share on other sites More sharing options...
Purplelilac Posted October 24, 2020 Report Share Posted October 24, 2020 How do you use Hanovia lusters. I just bought some at an estate sale. Can they be used on stained glass? Do you have to mix them with something? If fired to what temp? Quote Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted October 24, 2020 Report Share Posted October 24, 2020 Usually lustres are fired at cone 020-018, roughly in the same neighbourhood as slumping temperatures. So it depends what you want to do with them. The might be compatible with some stained glass, but some glass colours will change at those temperatures. Quote Link to comment Share on other sites More sharing options...
liambesaw Posted October 24, 2020 Report Share Posted October 24, 2020 Keep in mind that gold lustres also contain a strong flux, so if glass is slumping at 018, it may slump extra in areas with lustre. I've never heard of using gold resin lustre on glass. But I'm sure there must be some kind of gilding product specific for glass. Quote Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted October 24, 2020 Report Share Posted October 24, 2020 Bel Decal’s instructions say that their metallic and china paint decals can be used on glass. So I assume it can be done. But I also know that some stained glass doesn’t do well with heat. Check what the glass manufacturer says about the specific colour way you’re using. liambesaw 1 Quote Link to comment Share on other sites More sharing options...
Sasglass Posted February 17, 2021 Report Share Posted February 17, 2021 Did you sell them? I have used the gold on glass to good effect. Quote Link to comment Share on other sites More sharing options...
Patriot Posted March 31, 2021 Report Share Posted March 31, 2021 On 10/14/2020 at 1:30 PM, idahogem said: I am new first post so I hope I am in the right place. So my mom had a shop for over 25 years she did ceramics and porcelain. She was a master and did wonderful work. She did a lot of lusters and fine metals. She has become blind and I am tasked with Selling her things. I found a Box with 45 bottles of HANOVIA lusters and gold nost unopened in over 15 different colors including white gold mother of pearl gold essence halo gold.... I did some research and came up with very little I got the history of the company was unable to find when it closed other than a forum post from 2007 mentioning these were no longer available and only about 3 on the web for sale. my understanding is this was the artists choice at the time. So these are over 10 years old always stored in the house. My question is are these still usable or valuable. I have nothing to compare to I was hoping to find something to value them or someone who wants them or a correct forum where I could find more information. Here is the list thank you for your consideration. HANOVIA 1/2OZ MOTHER OF PEARL 7 OPAL 2 GOLD ESSENSE 2 HALO ROSE RED 1 HALO GOLD 6 LUSTER WHITE 3 HALO LUSTER TOPAZ 1 SLATE GREY 1 2 GMS MICRO PT (CANT READ) 1 BRIGHT PLATINUM #05 7 BRONZE #16 1? COPPER 3696 3 BRIGHT GOLD #N 2 1/4 OZ BLUE 1 IRRIDECENT LIGHT BLUE 1 TOURQUOISE BLUE 1 GREEN 3 LUSTER GREEN 1 LUSTER BROWN 3 Quote Link to comment Share on other sites More sharing options...
Patriot Posted March 31, 2021 Report Share Posted March 31, 2021 Do you still have Hanovia halo gold for sale? Quote Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted March 31, 2021 Report Share Posted March 31, 2021 @Patriot The OP hasn’t been on the forum since February. If you check a person’s profile, it’ll show when they last checked in. You might try direct messaging them. Unless you turn the option off in your profile, people get an email when you dm them. Quote Link to comment Share on other sites More sharing options...
Loralei Posted August 16, 2021 Report Share Posted August 16, 2021 If you still have these I'd be interested.. Quote Link to comment Share on other sites More sharing options...
Jasmine Posted October 6, 2021 Report Share Posted October 6, 2021 Hello, I have some hanovia opal #850 that I want to use on ceramic bisque. I'm planning on firing cone 18, but I'm not sure of the temp. High/low, how long on each setting etc. Any help would be greatly appreciated! Quote Link to comment Share on other sites More sharing options...
Min Posted October 7, 2021 Report Share Posted October 7, 2021 Hi Jasmine and welcome to the forum. Lustres are an overglaze so it's best not to use your Hanovia Opal on bisque. I would suggest using a gloss glaze on it first then applying your lustre and firing to the recommended cone, gold lustres are usually fired to cone 018 and mother of pearl lusters to cone 020. Lustres take on the finish of the underlying glaze so a matte glaze will give a matte result, gloss will give gloss. You really need to work outdoors if possible and if not then work in a really well ventilated space, either way you also must wear a respirator rated for vapours not just dusts. For firing, load the kiln loosely and keep it well ventilated, just your regular glaze firing should be fine but obviously you will be firing much much cooler. (That zero at the front of the cone 018 is important!) Quote Link to comment Share on other sites More sharing options...
Bonnie Anderson Posted October 21, 2021 Report Share Posted October 21, 2021 pottersaddict@gmail.com could I fire MOP and Gold at the same time? Quote Link to comment Share on other sites More sharing options...
Chilly Posted October 23, 2021 Report Share Posted October 23, 2021 On 10/21/2021 at 9:14 PM, Bonnie Anderson said: could I fire MOP and Gold at the same time? Check the firing temps and cones. should be on the labels Quote Link to comment Share on other sites More sharing options...
Started Late Posted December 5, 2021 Report Share Posted December 5, 2021 On 10/21/2021 at 1:14 PM, Bonnie Anderson said: pottersaddict@gmail.com could I fire MOP and Gold at the same time? What is MOP? Quote Link to comment Share on other sites More sharing options...
Mark C. Posted December 5, 2021 Report Share Posted December 5, 2021 Man Over Pottery? just a guess Chilly 1 Quote Link to comment Share on other sites More sharing options...
Min Posted December 5, 2021 Report Share Posted December 5, 2021 2 hours ago, Started Late said: What is MOP? Mother of Pearl. It looks a bit like the inside of an abalone shell but much lighter. Roberta12 and Chilly 2 Quote Link to comment Share on other sites More sharing options...
M.Carter Posted June 22, 2022 Report Share Posted June 22, 2022 Hello. So I was clearing out some of my fathers estate. And I found a pencil case, with gold leafing and a bottle of Hanovia Opal #850. There's about 1/3 left. He was a glass painter, so I guess thats what he may of used it for. Would anyone like it? I might kept the gold leafing, but it someone can use the opal, all I'm asking is that you pay the postage. Cheers M.Carter (South Australia) Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.