Callie,
a story which has information about a clay in water:
long long ago, but not to far away, I was still assigned to the refinery when one of the plant cooling systems was changed from deep clean cold water wells to river water that had a small but visible amount of yellow river clay suspended. Shortly after the switch to river water, the plant heat exchangers began to plug with clay and the exchangers had to go off line to be cleaned (not an easy or low cost task).The lab was trying to find why the plugging was taking place and they were not finding anything about why the system was being plugged.
A lab technician had put a bottle of the river water in the window to watch it over time. After month nothing had changed, the clay in the bottle of water was still suspended. Later on, someone decided to clean the window shelf and set the bottle of river water into the sink which had some warm water flowing through. When the someone picked up the bottle to it back to the window shelf, he noted that all the clay was now at the bottom of the bottle and the water was clear; and he came upstairs to tell me what he had found.
my recommendation is to heat the slop water a little bit and see what happens.
if your clays are like my south Texas river clays, boiling is probably not needed.LT
-
When we produce a ceramic material that allows "light" to pass through that material we are working with a "glass" even though us potters call the material a clay body or a glaze.Todays "Ceramic-Tech-Today" article: Colored glass: From alchemy to empirical chemical design
https://ceramics.org/ceramic-tech-today/education/colored-glass-from-alchemy-to-empirical-chemical-design/
has some useful information and background that might help determining why the bone-china pots show a color when seen in a light source. Remember that the source of the "light" is also an important variable.LT
-
you will often get a greenish shine from a light on window glass at an angle.
small amounts of iron in the glass is mostly the reason, but the source of the light and thickness of the glass are also a variables.take a look at:
https://physics.stackexchange.com/questions/247939/why-is-glass-green
question:
When I look at a glass block at an angle the edges appear green, but when I look at the edge sideways, so that is directly in front of my eyes it appears transparent. Why?
answer:
Most glass contains iron oxide as an impurity which gives the glass a slightly green hue. When you're looking straight through a pane of glass you don't notice it because the glass is so thin. But when you look down the side it becomes apparent because of the thickness.
LT -
I've been there. and learned to ignore the "official methods" and simply crushed the dry clay as small as possible using a hammer and kitchen screen utensils to get rid of the "big" rocks.
Mix the clay with water to make a slurry that is somewhere between the buttermilk and the milk level (or a little less). Let the mixture set for a while to let the heavy particles to sink, and then pour the liquid into a separate container which will contain most of the sig. Stir up the original container again and let it set a while, and repeat pouring off the water to get remaining sig. Yes, this is not the official method, but it has worked just fine for the clay I take from my ponds and roads to them. I have also used that same method for making sig from scrap commerical clay bodies.If you are able to get wet clay from the backyard just start with that; add water and mix well; if you have sand, it will sink along with the heavy particles. I have a pond that collects fine clay every time there is a decent rain. After the rain there will be a thin layer of fine clay above the big paricles. My first round on terra-sigillata I followed the "official" method; it worked ok. After noting what was happening in the ponds and just getting a bucket of pond mud and water I begin to make my own method which has worked just as good as the textbook.
The best "official" recipe I have found (beyond my own) is Vince Pitelka's version:
http://www.vincepitelka.com/wp-content/uploads/2022/10/Super-Refined-Terra-Sig.pdf/*/
-
when wondering around the property this week I notice a rotting stomp of a large pine tree that was blown down a few years ago; the dried yellow clay still on the bottom of the stomp was simular to the color of the plastic cat litter buckets; the clay on the stump contains iron oxides. Long ago while solving problems for plastics, fine particles of iron oxides were used to produce colors to the plastics.
My point is you should think about the iron being taken from the plastic. Test using a plastic bucket that is not yellow.
LT
- Babs and Bill Kielb
- 2
-
I have been down a similar route long ago: make a round object (a piece of stiff flat tarpaper); place on the soft clay; use a sharp cutting tool (I used a small sharp pointed kitchen knife) to cut the circle of clay. Start with a large flat sheet of clay on a piece of dry paper or cardboard, use the round object and the knife to cut the clay with the knife; when all of the coasters are cut, then remove the clay between the coasters leaving the coasters on the cardboard. The coasters are allowed to flat all the time. smoothed the sharp edges of the coaster after the bisque.
LT
-
To get a "blue" shino:
Take your own plain shino glaze recipe.
Add a "pinch" of cobalt to that glaze; make a test to see if you like the "blue";
If not enough blue, add another "pinch" of cobalt; if to much blue, use "half a pinch" (this is just like finding how much sugar you need in you coffee).
warning: too much cobalt will produce black blue (or a blue black).the images are for cone 10 reduction on a studio clay body.
one is plain shino, the other is shino with cobalt (aka blue):
LT -
40 minutes ago, JBT said:
Have you found one way creates a stronger bond?
nope
-
I have done what you are doing. The application of the glaze is one of the main variables. The glaze composition and the "stiff ness" of the melted glaze is also an important variable. There will be a difference between raw clay ware joining and bisque ware joining. Both are possible; important variables: application of the glaze, porosity of the bisque surfaces, and the thickness of the glaze slurry. Always make sure that weights and gravity are working for you at all of the joints. the glazes used for my work was a shino glaze (very stiff) and a clear or celadon glaze (not very stiff); all cone 10 reduction. It works also at lower temperatures, just use glazes to fit the temperature.
LT
-
Do you have a clear glaze that works OK all the time?
if so, just add some Zircopax to your clear glaze and you will have a white glaze.
the amount of Zircopax will probably be somewhere between 4 and 8 %.LT
-
4 hours ago, Rosie S said:
The texture looks like there is a lot of sand but did the artist use a slip and then added a grog/chamotte to it and then covered the piece to create this type of texture? Would love to understand your thoughts on how I can go about to creating this texture on one of my pieces. I just love the organic look of natural clay used and it's texture. Any advise would be greatly appreciated.
I have created this texture by dipping the bowl in glaze, and immediately roll the bowl in a container of dry sand or crushed white dried claybody. The wet glaze will capture the dry material and "glue" the dry material to the surface during the firing. A similar effect using a slip of the bowl's claybody on the bowl surface followed by the dry material. My experience has been that the a "stiff" melted glaze works better than a runny one, but both will work if the ratios of glaze and dry material are worked out by testing.
LT
-
13 hours ago, ingrid houchin said:
I was wondering if anyone uses kaolin wash to coat the bisque ceramic work with?
I have been making exterior surface coatings of all form of items, bowls, vases, bottles, and sculpture using a paste (think toothpaste or soft butter) of various kaolins. The paste is applied to the clay body (prior to bisque) and compressed with a spatula; . I have also used dry kaolins, ball clays, and "wild clay" dust to rub into rough surfaces of bisqued (and bone dry surfaces) to change the color of the fired ware. I used paste and dry materials to avoid having to deal with extra moisture that a slip produces.
my work is fired to cone 10+ reduction; some sculpture is only fired to bisque.LT
-
A good "BAT" discussion can be found at:
How to Make Throwing Bats
https://www.vincepitelka.com/wp-content/uploads/2019/02/How-to-Make-Throwing-Bats.pdf
an alternate to hard bats try the flexible ones:
https://www.vincepitelka.com/wp-content/uploads/2019/02/Throwing-on-Canvas-Bats-as-an-Alternative-to-Rigid-Bats.pdfI use both kinds depending on why, what, where, and when the "bat" is needed.
LT
-
My mark tool started a square shaped piece of soft clay with a carved design on that piece; had it bisqued and start using the then hard stamp. I have made many over time; it took more time thinking about the "design" than it took to actually make the item. I now have different sizes for different sized objects.Just prior to sending all objects to the bisque firing, I also mark the bottom of the objects with an "iron oxide and water ink" applied with a fine tipped brush; the iron oxide mark has shown on all clay bodies from white porcelain to red clays for low temperature (cone 08) to cone 12 electric, gas, wood, and Raku firings; this homemade "ink" works better than any other material.
LT
-
an alternate approach to remove "gloss":
place the object in a container of sharp sand then vibrate the container for a few minutes; the sharp sand will create scratch the glaze surface and remove some the "gloss"; take the object out evaluate the "gloss"; repeat as needed.
You can also use fine emery paper and change the "gloss".LT
-
20 hours ago, njabeid said:
I wonder how much that would be per weight of slip or of dry clay before making the slip?
my assumption is that you are looking for the amount of sodium in the slip. the amount of sodium in: sodium bicarbonate is Na-H-CO3 (molar mass = 84). sodium carbonate is Na-Na-CO3 (molar mass =106) therefore:to get the same amount of sodium you need to 168 grams of baking soda to get the same amount of sodium if you used 106 grams of sodium carbonate.
In other words you need 1.58 times of sodium bicarb instead of than the amount of sodium carbonate in your slurry recipe.All of this is based on the assumption that both the sodium carbonate and the sodium bicarbonate are "dry" solids; that is they have no water attached to the molecule. Sodium carbonate is more likely to absorb water than baking soda but both can /and will/ pickup water and still be a "dry" solid. Both are white powders that will absorb water vapor from the air if not stored in a sealed container.
I have no useful insight if the reason for using sodium carbonate is adjust the pH of a slurry to control suspension of the solids. I seldom care about suspension as I apply "paste" instead of "slip" on surfaces. I add the sodium to get the effect of the sodium in the fired surface.
Regarding @PeterH question: yes. long ago I began using a water spray of sodium carbonate as a means of controlling the fired effect of surfaces.
I ran out of sodium carbonate but had baking soda in the cupboard and used it instead; saved a trip to the store and the results were equivalent. I have been using baking soda more often as it is less damaging to my skin and is available at the grocery store near home.A footnote: once the sodium carbonates are dissolved in water they are no longer "sodium carbonates" but are sodium ions and carbonate ions. the pH is determined by the total collections of ions in the liquid phase. Soluble ingredients other than the sodium carbonates also must be considered.
LT
-
3 hours ago, njabeid said:
I think soda ash is the (nearly) one ingredient I haven't got, but I'll go along to the shops and have a look. I do have bicarb, so I could bake that.
no need to "bake" the bicarb, just add more of the bicarb to equal the amount of sodium that you want to have in the mixtrue.
LT
-
1 hour ago, Gonen said:
no its just nickel metal "High purity, ultra-fine, conductive, metallic nickel powder for experimental research"
my comment:
I have applied copper wire and iron wire (wire size was between 0.1-0.2 mm diameter) both over and under glazes in both 1000 C oxidation raku firing and cone 10 reduction firing. The copper wire melts, runs, and is practically "dissolved" into the glazes and makes color between black and red. The iron wire reacted with the glaze "corroded" the wire and did not "melt"; the glaze color was what you expect if applied as iron oxide; but the wire was not totally reacted because of the wire size. these data are results of applications of the metal on to the bisque both before and after the glaze slurry applied.
I have not added metal dust to a glaze slurry; I expect suspension problems and reaction problems between the metal particles and the water part of the glaze slurry. some metal dusts are flammable; I have no data here.I have also used zinc coated iron nails as decorative treatments for objects and the zinc along with the iron work together (and/or against)
From these examples I concluded the following:
metal particle size is a major variable;
the composition of the glaze will also control the solubility into the glaze melt;
firing temperature is a variable, some metals melt, some don't before the final temperature is reached;I also have used metal filings sprinkled over glazes and marks were produced. I have not used aluminum metals but I think they would also produce marks. Application will be important - as is always for glazes.
Also keep in mind that most pure metals will have some form of an oxide coating unless the particles are not treated with a oxygen barrier of some sort.
also filings from many "metals" will be a alloy instead of pure elemental metal.all together, Go for it. Assume something, but not a specific something;
the worst thing would be nothing happening.LT
-
mixing two glazes:
call them glaze A and B.This is a standard glaze assignment for the college Ceramics II.
There are various combinations A over B; B over A; A mixed with B;
Expect three different fired outcomes.The above assumes that the amounts of glaze per area of A and B are applied equally.
The forth set is to use different amounts of glaze per area also, which will also provide even more different outcomes.
my recommendation: make a large set of test pieces and find the outcome you prefer.
LT
-
13 hours ago, PaulineNL said:
I have made a bunch of conical tree ornaments, I bisque fired them and glazed them today. I would like to glaze the interior of the cone as well as the bottom rim. But that leaves no place for it to sit on a kiln shelf. What is the solution?
place three small sea shells (filled with wadding [mixture half alumina half kaolin wet to a stiff paste); shell side up touching each cone ware item. the wadding supports the weight of the ware;
The fired ware will have three small rough spots where each shell meets with the glaze that can be pollished with emery paper. if the ware item is quite heavy, used larger shells.
I have used this method for many years at firing temperatures from cone 011 to cone 12+ with 100% results at oxidation and reduction firing.LT
- Min, Rae Reich, Kelly in AK and 1 other
- 4
-
Take your clear glaze ; add some Zircopax. Do some testing to find the amount needed to meet your own amount of white ness in the fired glaze. Start at around 4 % +/- as a start.
LT
-
-
19 hours ago, TaraB said:
My question is why would these be non vitrified if the correct cone was used and the sitter dropped at the right temp? The firing was no different to any other...? The only new thing I have done with these mugs, compared to my usual firing, was add a gold lustre.
my thoughts are more about thinking about the clay body, the glaze, and the firing might be causing the variable appearances when the mug contains liquids such as water or coffee.
1. if the glaze is completely covering the clay body on the mug and is completed melted and not crazed; how does liquids (water) get past the glaze and cause a change in the appearance of the glaze? The first approach would be to make sure the application produces a good solid coating.
2. assuming that the clay body might not be completely vitrified throughout I would fire some mugs without glaze and see if the mugs absorbs water. @Min used the cooking of cookies analogy on what temperature to fire the clay body in the kiln. I want to extend the analogy to point out that the mass of a mug is several more than ten times the mass of a "cone" and requires a longer time at the peak temperature than a "cone". The correction is to either hold longer time at peak temperature, or just shoot for a higher "cone" temperature.
3. The glaze is supposed to have a "gold luster" visual effect after firing. Is the "gold" uniformly distributed throughout the glaze? in other words: is the differences are about the "gold" rather than about the other possible reasons? easy test is to fire several mugs with and without the "gold" located in the kiln side by side see what happens?
4. my ceramics professor long ago pointed out that application is 99% of the glazing; therefore think about how application of this set of mugs was different from those made previously.
LT
-
On 10/13/2022 at 10:21 AM, Zeynep Gedikoglu Sculpture said:
I like to build tall sculptures that are thin at the bottom and larger at the top. Therefore I am looking for a way to glaze my sculptures so that all Sides look great!
I have made similar tall sculpture with small base of the sculpture part. The solution was to make a clay base big enough to prevent the sculpture from falling and attach such base to the sculpture; that is the base is a part of the sculpture. some were just a half inch thick flat piece of clay. If the final base is to be wood, provide holes in the clay base to attach the wood foot.LT
Wood ash glaze conundrum
in Clay and Glaze Chemistry
Posted
Sam:
If I were doing what you are trying to do: I would do the following:
1. Use all of the dry ashes and the water that is use to suspend the solids in the glaze slurry. I would also add some strong clear vinegar to convert the potassium and sodium caustics to netural that becomes dissolved into the glaze slurry. I would also measure the amount I use so that I would know the amount to use next time.
2. Add about 4 grams of sugar for ever 100 grams of dry ash that is used for the glaze. The sugar will help keep the calcium in the dry ash from converting the glaze slurry to a solid lumps of concrete after setting for a day or so. If the slurry goes solid over night I would know I did not add enough sugar. The 4% is based on the assumption that the calcium compound is about half of the total weight of the ash. If the calcium were less than half I would use less sugar, and if more than half, use more sugar.
My reasoning: Loosing the potassium and sodium components is a waste; both helps melting of the glaze (think American Shino). Calcium is a main ingredient for concrete and sugar slows setting of concretes; I learned that from a university professor that studied concretes; a bucket of such glaze with sugar survived half a year before I got bored with it and switched to a different base glaze.
It is the potassium and sodium that creates the great coatings in wood fired ware along with the other elements released from the buring wood that also get cared to the surfaces of the wood fired wares. If done right, using wood ash as a applied glaze one can almost make pots in a non-wood fired kiln that will appear to have been wood fired.
LT