46 minutes ago, BobMagnuson said:
Does anyone out there have a successful reduction glaze recipe that includes zinc?
Yes. the college studio standard clear (and the base glaze for ~ four other glazes) cone 10 reduction glaze has 2-5% zinc and there is no evidence that the zinc evaporates. my memory says that some reduction crystalline glazes also have lots of zinc but i don't have the recipes.question: Has anyone set down and calculated zinc oxide decomposition to zinc vapor in a combustion kiln environment for the various oxygen levels at various kiln temperatures that the glaze mixture will see? All the data should be available in the CRC handbook or the NIST database.
LT -
My initiation to ceramics I: the semester started with specific cone 04 Earthenware with a choice of white or red; fired to cone 3 in an oxidation gas kiln producing fully matured ware. at mid-semester the clay body was changed to a specific cone 10 stoneware with a choice of white, tan to dark to be fired a cone 10 in reduction kiln.
Ceramics II was again cone 3 (earthenware) firing first half and cone 10 (stoneware) second half.
(several years later all classes was cone 10 stoneware reduction).
Some where along between earthenware to cone 10 was a semester or two it was all cone 5 (midware) fired in reduction.Today the studio is all stoneware at cone 10-ll reduction.
I now use cone 10 clay bodies (because that is the way the kiln is fired) -- any kind -- for structural purposes of an object and use a clay of any cone -- earthenware to wild clay bodies -- as exterior coatings supported by any available high fire rated clay body. Some of my ware uses a cone 04 clay body as a glaze. This works for me.
After determining the properties of the "earthenware" clay bodies fired at cone 10, I am comfortable with the way I am using the low fire clay bodies fired in the kiln I use and the way my ware is fired. I am making ceramic art even though the forms are often based on bowls and platters. The clay bodies are mature, the exterior surfaces are glazed with safe glazes.
Firing low fire to a higher fired temperature is not normal, but then "ik ben niet normaal!".
The cone 3 firing of earthenware was an easy way to make matured ware with bright simple studio glazes. If I were in the business of making drinking and eating ware with a bright strong color palette, cone 3 oxidation of earthenware clay bodies would be high on a choice list; but then I would not be making art, I would be making drinking and eating objects. I am making "interesting objects" with clay ceramics.Over the last five years and so, I have chosen to use any clay body easily available to me, and I make objects that I consider to be "interesting"; I use the term "container" for items that might be considered to be "mug" or some other use; the functionality decision is controlled by the user of the object not by the maker. Each batch of clay is different, and this reduces the boring tendency of making the same form over and over with the same appearance. The leftover low fire clay bodies from my early semesters was available, and I was given the latitude to experiment and to learn something. Improvise, Adapt, Overcome is the driving force for what I make and how I do it.
3 hours ago, Min said:Would be great if there was a commercial body that was in the cone 2-3 range that met those requirements.
Min, I suggest you take the available low fire commercial clay bodies and find the firing cone that will vitrify to the point that it won't leak without glaze. use that clay body to make your ware, take low fire glazes and fire them to that temperature. Start with firing low fire glazes at the mature temperature for the low fire clay.
LT
-
2 hours ago, Rick Wise said:
I would like to make a "reclaim bat", i.e. a tray on which I can lay wet clay/slip so that the water absorbs out of it for eventual re-use. Should I use pottery plaster or plaster of paris? And why?
Once upon a time, I had the same situation, how to reclaim clay and then dry the clay back to throwing moisture. I used a set of large red clay flower pot plates, or a large flower pot sitting on a flower pot plate. These remove water just like plaster, are not as heavy, and are cheap. And no, the red did not contaminate the white (aka porcelain) reclaim.LT
-
26 minutes ago, GEP said:
It wouldn’t be expensive, and not difficult at all.If they had to hire an outside editor/proofreader (which they probably don’t), it would cost them way less than the cost of one kiln. The entire manual is printed on a laser printer, not through a printing press. They wouldn’t have to edit the sections supplied by third parties, just the part that they wrote, which is what i was talking about.
Or L&L could just publish a pdf document on their website with "corrections". This is what the Oxford (and others majors) textbook press does. errors are encouraged to be sent to the editors of the books. The feedback is evidence that readers actually read and use the info in the books!
LT -
23 hours ago, Miriam Ash said:
I have always struggled with getting my pieces off the wheel cleanly. Here are some of my issues.
1) When I throw directly on the wheel the piece warps either when I try to lift it off or when I set it down. I've tried the pot lifters and I have issues with those too.
2) When I throw on my plastic bats I have a lot of trouble removing them when they are leather hard. They stick firmly to the bat.
1. when throwing on the wheel, use a tarpaper, canvas, or paper bat. ( https://www.vincepitelka.com/handoutsinformation/ and http://www.vincepitelka.com/wp-content/uploads/2019/02/Throwing-on-Canvas-Bats-as-an-Alternative-to-Rigid-Bats.pdf ). run the cutting wire under the bat, use the edge of the bat to slide the bat and clay form from the wheel onto a ware board; peal the canvas bat off at leather hard stage.2. for plastic bats: I let the pot dry until it is ready for trimming and trim as much as possible with the pot stuck to the bat, then let the pot dry until pops loose from the bat, then finish trimming the foot; or cut the pot off with the wire tool and the wheel turning slow.
3. remove as much extraneous clay from the pot as feasible (within the limits of the wet clay strength) while still wet and on the wheel; the pot dries quicker, and makes trimming easier.
LT
-
57 minutes ago, blackthorn said:
Eventually, I'll come up with a process I can apply to something other than a test slab or tile.
The "test slabs" are interesting forms and prints. well done!!!LT
-
3 hours ago, CactusPots said:
What kind of pugmill has speed adjustment?
A well designed one!
-
13 hours ago, liambesaw said:
I can't wall it in due to building code here
Don't build a wall, build a solid fence around it with a gate.
-
If the clay body requires any combustion, logic seems to prefer having separate incoming and outgoing openings for the gases. At least that’s what my physics and engineering schools recommended.
-
-
2 hours ago, Pres said:
QotW: How has your work progressed in terms of variety of form?
2 hours ago, Pres said:... I still have not been able to throw a sphere! Just don't seem to leave enough clay in the base to support the form, or can't get the form to go beyond a narrow base to a shoulder 2/3 of the way up going to a neck.
One answer to the "Thrown Sphere" problem is to first know how much clay is needed to make "the sphere", or to know how big will be "the sphere" for the known amount of clay being used. (gotta do some math here: get the volume of the sphere outside diameter and subtract the diameter of the inside sphere of air to find the minimum amount of clay needed. add about 1/3 more for trimming, etc). make a thick wall cylinder and expand the in the middle. rib the bottom of the cylinder to the shape of the inside.The top 3/4-th of the sphere is thrown directly from a cylinder using the skills of throwing the shoulder and spout of a bottle; close the bottle into a sphere; you now have a closed form of the top 3/4-th done. Let the form stiffen for a while; then trim the bottom 1/4-th to complete the sphere. [Practice by making hollow thrown doughnuts.]
Or take the approach I did in a class assignment for making a "thrown sphere": Take a 4x4x4 inch cube of wet clay; shape the cube into a smooth sphere; throw the sphere up in the air and let it fall onto a sheet of paper the floor (or on to your work table if you don't like to bend over); carefully lift the piece from the floor (table) add some decorative slip, dry, remove the paper, fire, and present on a pedestal with the title "Thrown Sphere". Others in the class made two half sphere bowls that were joined one over the other.
Seriously (and more on-topic) one must recognize that most thrown forms are monotonous unless we deliberately switch from being a throwing machine and use our artistic skills to produce something interesting. I have colleagues that uses simple plain thrown bottles and bowls as canvases for painting with slips and glazes. I use simple thrown forms with applied "dry slips" to produce random tactility textured canvases for a ground for "painting" with a glaze. The thrown form becomes an three dimensional canvas for making interesting marks. Look at the work by Tony Clennell ( http://smokieclennell.blogspot.com/ ) over the last five years. His forms are simple bowls, cylinders, platters, etc. are canvases to be used to apply handles, feet, and glaze. Or the work by Antonette Badenhorst: https://www.porcelainbyantoinette.com/ or https://www.aic-iac.org/en/member/antoinette-badenhorst/ the forms are simple bowls and cylinders. Look at the work of Voulkous, Paul Soldner, Marcia Selsor, etc. -- the thrown forms are just their starting point. But they were/are past the making bowls for food service; they were/are making art objects not bowls.
. i quit making "bowls" when the family said we've got enough "bowls"!!!!; switched to making "interesting 3-d stuff" out of clay -- some of which can be used as a food container (or napkin compressor, or sling-shot target, or ...); the owner chooses how to use it.
try making square bird-houses with slanted roofs using thrown lidded cylinders.
LT
-
26 minutes ago, liambesaw said:
Screw on top!? Now that would be something
years ago on clayart David Hendley wrote about his jars with ceramic screw-on lids aka “Homemade Dies”. Look it up on his website: http://farmpots.com/not as hard (or easy) to do as one might think.
LT
-
2 hours ago, Bill Kielb said:
First reduction test run was designed to calibrate and hopefully allow schedules to be created that are effective and finish in about eight hours. From an initial peek inside the kiln, All test tiles reduced everywhere as expected ……… they are on their way to creating cool stuff and sharing their results and new schedules / techniques. Next build I think we are gonna find a cool dressy enclosure though.
Bill,
good work!
what are the units in the reduction measurement vs time plot? Is the temperature measurement at the same location as the oxygen measurement? Do you convert the oxygen probe reading to oxygen fugacity ( which is the variable normally used in the thermodyamic approach to the chemistry of oxygen in silicate melts)?
LT
-
3 hours ago, MamaJenXO said:
This is the look I am seeking - Sean O'Connell and Dawn Candy pieces- I have reached out to them also to see if they would share their knowledge
I just really like the idea of the underglaze flowing
I wonder if the apparent 'bleeding' is a technique used at the time the blue colorant was applied to the pieces - that was the way I achieved similar effect on canvas with water color and pastel crayons. after lots of practice a "light" stroke with the "right" brush would produce the allusion of bleeding.
LT
- Bill Kielb, preeta and JohnnyK
- 3
-
-
-
-
12 minutes ago, liambesaw said:
Are you saying 10000 hours before someone will want to buy your work?
well, PT Barnum didn't think so.
My perspective is that the customer controls of what is bought, while the supplier controls what is offered for sale.
- PotterPutter and Hulk
- 2
-
Pres,
There is a lot to be said about the 10,000 hours of practice ... . I don't remember the rest of the story. Practice not only of throwing, but designing work that is interesting and desirable. Well thrown pots can be ruined with poor choices of glaze and glaze applications.
40 hours practice per week leads to about 5 years of practice (+/- a year or so).
LT -
According to my memory, there is a paragraph or two in Val Cushing's handbook on clay bodies for use in cold climates. Fully vitrified porcelain is not one of those clay bodies, as I remember; there is a optimum porosity for freeze - thaw requirements. Also check the Rhodes & Hopper book on clay bodies.Remember that roof tiles and bricks have been used in cold and snowy regions for several hundred years and they have survived lots of freeze thaw cycles.
LT -
About 10-15 years back (+/-), there were Clayart discussions on reduction in electric kilns. Mel Jacobson discussed his conversion of a small electric kiln to fire in reduction; Lee Love and John Baymore both discussed how the Japanese were routinely using large electric kilns for reduction. From what I remember from these discussions the customer base for electric reduction kilns is unwilling pay the cost of a well designed electric kiln for controlled reduction.
As a point of comparison, the heat treatment industry routinely uses electric furnaces for controlled atmosphere treatments of various metals where the atmosphere is in what a potter calls 'reduction'.
LT
-
I don't know for sure when I learned to throw clay, but it must have been about the time I started first grade at school. A new house was being built next door and my dad allowed the neighbor to level some of the hill we lived on. The part next to the house was a hard yellow clay and that was the material I learned to throw with. Took only a couple of days, with my dad as a teacher, to learn to throw straight. (I also learned to bat the clay 'balls' thrown at me). By high school time, I had given up throwing clay and was more interested in chemistry and engineering. Resumed my clay throwing around '05. The biggest difference now is that the clay is softer; back when I first started clay was always thrown dry; now the throwing clay is always wet, soft, and sticks to the bats.
-
My current fad is the use of soda ash, twenty-mule-team Borax, and TSP solutions sprayed on to raw clay surfaces - especially surfaces created from dry clay embedded in the moist surface of a clay body prior to the surface being stretched. Firing is cone 10 gas kiln. -
Art is in the mind of the observer.During the creation of an object the maker is the primary observer. After the object is completed and released, the decision regarding the "artness" of the object is determined by the observer. Different observers may (will) have different decisions on the placement of the object in the art ---- non-art spectrum.
The debate within the ceramic "art" domain between art and functional ware is a contrived debate. All ceramic articles have a function even if that function is to just take up space. The observers, owners, users, ... are the decision makers as to the specific functionality of the object. My tea mug has multiple functions. At this moment its (the mug) function is to keep a fan from blowing paper off the desk. The sculpture across the room functions as both a hat rack and a source of inspiration until I put on my hat and go to the studio, then its function is to be a piece of burnt dirt taking up space and keeping the table from drifting off into the ether while it waits for someone to return and take notice!
LT
QotW: All things considered, What coloring oxide would you not be able to work without?
in Int'l Ceramic Artists Network (ICAN) Operations and Benefits
Posted
Sodium;
soda ash/baking soda actually!
LT