Duncan Teacher Plus kiln start up help
neilestrick replied to Kiln technician help neede's topic in Equipment Use and Repair
Check out THIS THREAD. Lots of good Duncan info. -
Ah, an Electrositter. That makes sense. Diagnosing these Cress kilns can be difficult, so if you can do away with everything and just run the controller to the relays to the elements it will simplify things greatly.
-
I assumed the other manual controls were not there, that you had simply swapped out an older digital controller for the new Genesis. I'm with Bill, ditch all the manual controls and wire it up like an actual digital kiln. How/where is the controller mounted? Directly in place of the Sitter?
-
To be clear to everyone who may be reading this, we're talking about the L&L Dynatrol/ Bartlett V6-CF controller, which has two glaze settings and two bisque settings. This discussion does not apply to the Skutt controller, which has slow, medium, and fast settings. Fast Bisque and Slow Glaze work for most situations. For large or thick pieces you may want to use Slow Bisque, though. I do not recommend Fast Glaze in most situations, because it's generally too fast for low fire work, and most kilns can't actually ramp as fast as the program wants when going above low fire temps.
-
60 amp circuit? Shouldn't that be 30 amps? Assuming the thermocouple is good, the only other thing I would expect is a relay that's sticking when the kiln gets hot. I'd start with changing the thermocouple, though. At 18" wide and 22.5" deep, and pulling 24 amps, I'd say that kiln is not a very strong cone 10 kiln, more like maybe cone 8/9. But it should still get to cone 6 with the elements in spec. I would change that rate to 9999/hr. At 500/hr you're in the realm where we often see problems because the kiln can't cool that quickly.
-
We really need pictures to help figure this out. Try emailing the pics to yourself to resize them.
-
I recommend Fast Bisque to all of my customers. It's not really very fast, plenty slow for good burnout.
-
Envirovent Motor hot to touch—is it ok to run?
neilestrick replied to Windsong's topic in Equipment Use and Repair
Don't buy one from Skutt, they charge a fortune for them. Search online for a Dayton 1TDP7 or Fasco A166. -
Skutt Envirovent II - is it supposed to be so LOUD?
neilestrick replied to kristinanoel's topic in Equipment Use and Repair
The air going through the vent shouldn't be more than 140F degrees, but that's pretty hot to the touch. Make sure the cup that attaches to the kiln isn't clogged in any way so that it's not pulling in room air. The vent pulls a little bit of air from the kiln through the holes in the kiln floor, and and mixes it with a lot of air from the room through the holes in the side of the cup. As long as that's all good you're probably fine. Those motors typically fail due to everything corroding or the bearings wearing to the point that the motor can no longer make it turn. I've never seen one overheat to the point that it melts down or anything like that. They usually run very loud before failure.- 26 replies
-
- envirovent
- skutt
-
(and 2 more)
Tagged with:
-
Envirovent Motor hot to touch—is it ok to run?
neilestrick replied to Windsong's topic in Equipment Use and Repair
The air going through the vent shouldn't be more than 140F degrees, but that's pretty hot to the touch. Make sure the cup that attaches to the kiln isn't clogged in any way so that it's not pulling in room air. The vent pulls a little bit of air from the kiln through the holes in the kiln floor, and and mixes it with a lot of air from the room through the holes in the side of the cup. As long as that's all good you're probably fine. Those motors typically fail due to everything corroding or the bearings wearing to the point that the motor can no longer make it turn. I've never seen one overheat to the point that it melts down or anything like that. They usually run very loud before failure. -
How do I even out the kiln firing?
neilestrick replied to jrgpots's topic in Equipment Use and Repair
If they have gaps you could try closing up the gaps. Otherwise just a couple inches will probably make a difference. Slowing down the firing at the end can also help, like for the last 2-3 cones. Given that the kiln is built and you're not going to be adding insulation or moving the burners, at this point changing the bag wall and/or target brick and making adjustments to the burner settings are your only options. And honestly, if you're within one cone, then there's no reason to make and significant changes to the kiln design itself. Bag wall and settings should be able to dial it in just fine. -
How do I even out the kiln firing?
neilestrick replied to jrgpots's topic in Equipment Use and Repair
Raise the bag wall a few inches. -
Slipcasting with Paper Clay
neilestrick replied to Ryan M Miller's topic in Mold Making and Slip Casting
I don't think a typical paperclay has enough fiber in it to open up the body in a way that would affect how it the body handles thermal shock. It would take a lot more fiber than is usually used to increase building strength. Fibers are tiny but have a big effect on greenware strength. I also don't think that opening up the body is the best way to go about it. You'd be better off using a body that can handle the thermal shock from a formula standpoint, as Peter and Min have indicated. -
This. It takes forever for sealed forms to dry completely. The outside can be bone dry but the inside will still be leather hard. It also takes longer for the heat of the kiln to penetrate and drive off the last bit of moisture, so do a good long preheat and ramp slowly at first.
-
New skutt kiln - Best program for bisque firing
neilestrick replied to Amanda Hummes's topic in Equipment Use and Repair
Even bone dry pieces contain water. Clay can't be 0% moisture sitting in a room that's 50-70% humidity. That last bit of moisture has to evaporate in the kiln before turning to steam, which takes longer for thick pieces, so a preheat or slower ramp is necessary. What speed did you use for the first firings? Never use Fast, especially for a bisque. -
If the breaks are in the bottom row, just pin the big pieces in place, pin the elements to the floor if needed, and fire it up.
-
Congrats!
-
It all depends on how it goes together. Can you post some pics? You can cut the brick with a hand saw just fine, but you won't get very accurate cuts. For mortar joints you want very even surfaces for joining. It's generally easiest to just buy new wall sections.
-
Cracked thermocouple casing
neilestrick replied to LadyLumpsClay's topic in Equipment Use and Repair
What type of thermocouple? Does it have a metal sheath, or do you mean the ceramic beads, or a protection tube? Post a pic. -
New skutt kiln - Best program for bisque firing
neilestrick replied to Amanda Hummes's topic in Equipment Use and Repair
What Denice said. Explosions are caused by moisture. Even totally dry pots contain some moisture, which must evaporate out before it turns to steam and blows apart your work. When water turns to steam it expands 1700 times in size, so it's a powerful force. With thin pieces, the regular ramping rate of the kiln is slow enough to avoid explosions. But if you have large or thick pieces, it takes longer for that last bit of moisture to evaporate, so you need to do a preheat. -
New skutt kiln - Best program for bisque firing
neilestrick replied to Amanda Hummes's topic in Equipment Use and Repair
@Amanda Hummes What exactly made the first two firings unsuccessful? Explosions? Cracks? -
Recommendations for middle school wheel
neilestrick replied to Juhasz's topic in Equipment Use and Repair
Any wheel that is in your price range will work fine. Just don't get any of those cheap wheels on Amazon. -
Yes, it sounds like they need replacing.
-
@EarthToMatthew A gets the hot, D gets the neutral. 4 gets a wire from both elements (2 wires total). 2 and 1 each get a wire from one of the elements (1 wire each). You might have to swap 1 and 2 depending on which element heats up when on medium. I would have the top element on the top section and the bottom element on the bottom section heating on medium.
-
HERE. Unplug the kiln and test the element resistance. Check your manual to see what they should be. How hot does the kiln get before it errors?