  1. obvara today. will try to post if we get anything good

  2. Awesome stuff little rodent. i love the terra cotta look too. I am always trying to find a low fire glaze to use in raku that has that color. but so far the ones i have tried are just ugly brown. yep, museum quality. rakuku
  3. rakukuku

    027

    So deeply sorry for this loss. Beautiful beautiful work. Hoping for a new and bright future for you as you literally rise from the ashes. rakuku
  4. Hey, anybody just dump a beer in their obvara brew? seems like it might jack it up quickly but what do i know.

    1. Show previous comments  4 more
    2. Evelyne Schoenmann

      Evelyne Schoenmann

      yes, I have thrown a beer in the brew once or twice to make it fizz some more. It works! and it doesn't smell bad ;-)

    3. Marko

      Marko

      If you added beer, wouldn't that make it, obeera?

    4. rakukuku
  5. more obvara tomorrow. I am addicted

    1. Evelyne Schoenmann

      Evelyne Schoenmann

      Been there! Welcome to the club!!

    2. rakukuku

      rakukuku

      we got good stuff and learned more, will post

  6. well i loved loved loved doing the obvara. thanks marcia for advice. several of us did it and we have a bunch of addicts. others got some spectacular results.
  7. hey, two obvara hearts are in my gallery. we had more good results today. rakuku

    1. Evelyne Schoenmann

      Evelyne Schoenmann

      They look really good. Congrats!

  8. Yy, today's obvara was a total success. thanks Marica for the advice. will post pics when i can. rakuku

    1. Marcia Selsor

      Marcia Selsor

      looking forward to seeing the pieces. I will post some from my workshop in Las Cruces.

    2. Cavy Fire Studios
    3. Marcia Selsor

      Marcia Selsor

      I posted ics in Educational approaches. Let us know where you post them.

  9. wish i could get the whole piece into the picture. it has a large jeweled crown.
  10. mixed the brew. looks like it is going to grow out of the bucket this should be fun. rakuku

    1. Marcia Selsor

      Marcia Selsor

      obvara? just finished an intense workshop with the Las Cruces Potters Guild. Successful Obvara, Saggar,^1 Soda firingl, Raku, and horse feathers plus throwing demonstrations. Whew! heading home after a lecture on The Fulbright Experience at NMSU Las Cruces campus

       

       

    2. rakukuku

      rakukuku

      yep, gonna give it a try based on your video clip and article and other u tube stuff. hope it works.

    3. Evelyne Schoenmann

      Evelyne Schoenmann

      Oh great, a new Obvara follower. I wish you all the best! Post pictures please.

  11. today's the day I mix up obvara brew. some of us are going to try it on wed. we are going off of videos and Marcia;s article. hope we get some kind of results. rack

  12. How do I post photos from my new MAC?

    1. Show previous comments  1 more
    2. rakukuku

      rakukuku

      i had a pc before. can't find out how to do this from a mac. can't get it to choose a photo

    3. High Bridge Pottery

      High Bridge Pottery

      Not exactly sure on the problem. Does the finder window open? (think it is called explorer on windows) The choose photo button on the forum should still be in the same place.

    4. Mark C.

      Mark C.

      Send the photo to yourselfvia e-mail from I-photo in a smaller size -then I drag it to the decktop and then you follow the photo instructions on FAQ page

  13. Fabulous stuff. Love it, its gonna be a great hit. fyi i just made a slug sculpture with an evil grin called "I'm gonna eat your pansies". rakuku
  14. getting ready to try obvara. made some textured heart shapes. i am trying to get some other people interested so we can try it out. thanks Marcia for advice. as soon as the pieces get bisqued i will make the brew. rack

    1. Marcia Selsor

      Marcia Selsor

      have fun and post pictures.

       

  15. love this stuff. gonna have to try it. rakuku
  16. love the dragon but bunnies are best! rack
  17. From the album: rakukuku

    here is a product of yesterday's naked raku one step. pink terra sig. i added more alumina hydrate to the slip and we got the right amount of adherence. rakuku
×
×