Porcelain vase with gold lustre accents
Celia UK commented on Celia UK's gallery image in Browse Member Galleries
- 2 comments
-
- porcelain
- gold lustre
-
(and 1 more)
Tagged with:
-
From the album: July 2019
Slip cast porcelain (own mould). Paper stencil (cut by me) applied when leather hard and wax resist painted over. Stencil removed and image water etched by wiping with damp sponge. Fired in electric kiln to cone 6/7. Battery tealight placed inside! -
Haven’t been active on CAD for a long time - life just became very busy! Thought I’d create a new album of some recent work.
-
From the album: July 2019
Thrown porcelain vase, cut vertically from rim. Textured slab attached with slip. Copper & cobalt oxide wash applied to bone dry greenware. Bisqued to 1000oC. Transparent glaze poured inside and brushed on textured addition. Fired to 1200oC (cone 6/7). Gold lustre highlights added then fired to 780oC.- 2 comments
-
- porcelain
- gold lustre
-
(and 1 more)
Tagged with:
-
From the album: July 2019
Thrown porcelain. Wax resist all over, carved when leather hard. Black underglaze inlay painted over and wiped back. Bisqued to 1000oC. Orange underglaze highlights added. Transparent glaze poured and dipped then fired to cone 6/7. -
Porcelain grasses vase with gold lustre highlights
Celia UK posted a gallery image in Browse Member Galleries
From the album: July 2019
Thrown porcelain. Wax resist all over, carved when leather hard. Black underglaze inlay painted over and wiped back. Bisqued to 1000oC. Transparent glaze poured and dipped then fired to cone 6/7. Gold lustre applied before third firing to 780oC. -
Miniature porcelain bottles with underglaze transfers
Celia UK posted a gallery image in Browse Member Galleries
From the album: July 2019
Thrown porcelain bottles (sometimes off the hump) - 3-4” tall. Underglaze transfer decoration applied to leather hard clay. Bisqued to 1000oC. Poured and dipped in transparent glaze. Fired to cone 6/7 (1200oC)- 1 comment
-
- porcelain
- miniature bottles
-
(and 1 more)
Tagged with:
-
From the album: July 2019
Copper & cobalt oxide glazes applied to bisque fired (950oC) pieces. Fired in a dustbin raku kiln at recent kiln building workshop. (1000oC) then plunged into sawdust to reduce. -
From the album: Winter 2016
-
Latest kiln opening - White earthenware with texture slabs and copper oxide and cobalt carbonate wash under transparent glaze. Fired to 1080oC.
-
White earthenware 'shell' bowl
Celia UK commented on Celia UK's gallery image in Browse Member Galleries
- 3 comments
-
- White earthenware
- carved
-
(and 2 more)
Tagged with:
-
From the album: Winter 2016
Thrown white earthenware, linear additions, Holes carved then dots added. Wash of copper oxide and cobalt carbonate airbrushed when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.- 3 comments
-
- White earthenware
- carved
-
(and 2 more)
Tagged with:
-
From the album: Winter 2016
Thrown white earthenware, linear additions, Holes carved then dots added. Wash of copper oxide and cobalt carbonate airbrushed when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.- 1 comment
-
- White earthenware
- cobalt carbonate
-
(and 2 more)
Tagged with:
-
From the album: Winter 2016
Thrown white earthenware, cut and altered. Slabs textured and added. Copper oxide and cobalt carbonate washes when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.-
- White earthenware
- texture
-
(and 2 more)
Tagged with:
-
From the album: Winter 2016
Thrown white earthenware, cut and altered. Slabs textured and added. Copper oxide and cobalt carbonate washes when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.-
- White earthenware
- texture
-
(and 2 more)
Tagged with:
-
From the album: Winter 2016
Thrown white earthenware, cut and altered. Slabs textured and added. Copper oxide and cobalt carbonate washes when bone dry. Bisqued to 1000oC. Transparent glaze poured over, fired to 1100oC.- 1 comment
-
- White earthenware
- texture
-
(and 2 more)
Tagged with:
-
- 4 comments
-
Shallow dish with tissue transfer motifs
Celia UK commented on Celia UK's gallery image in Browse Member Galleries
Yes that's about it Roberta. Stencils with the motif being the negative part (the holes). This one was actually some flower wrapping paper that was holey all over and I cut small pieces, laid them around the bowl, cut small pieces of tissue transfer paper, laid on top, sprayed lightly with water, rubbed them gently with a rubber tipped tool, left to dry then peeled off and removed the stencil. The creamer stencil I made myself on a Silhouette stencil machine, cut from thin plastic film (thin filing wallets) as it's flexible enough for the curves. Same process. Lots of potential and given the price of stencils - quite a good use of them.- 3 comments
-
- Tissue transfers
- stencil
-
(and 2 more)
Tagged with:
-
-
Small dish with homemade tissue transfers
Celia UK posted a gallery image in Browse Member Galleries
From the album: 2016
After reading CAD article about making your own transfers, I tried this using a rubber stamp with stain & frit 50:50 mix. Stamped on to tissue paper, applied to leather hard clay. Bisqued to 1000oC. Dipped in transparent glaze & fired to 1100oC in an electric kiln.-
- Tissue transfers
- white earthenware
-
(and 2 more)
Tagged with:
-
From the album: 2016
Experimenting with bought tissue transfers and stencils as resist. Thrown white earthenware. Dipped in transparent glaze & fired to 1100oC in an electric kiln.- 3 comments
-
- Tissue transfers
- stencil
-
(and 2 more)
Tagged with:
-
From the album: 2016
Made for a friend's 50th birthday. Various 'significant' words & phrases stamped inside and out with different letter styles, highlighted with oxide washes before bisque firing. Dipped in transparent glaze & fired to 1100oC in an electric kiln. -
White earthenware bowl with floral additions
Celia UK posted a gallery image in Browse Member Galleries
From the album: 2016
Small bowl with pinched floral additions. Stains added to transparent glaze painted on flowers. Whole piece dipped in transparent glaze. Fired to 1100oC in electric kiln.-
- White earthenware
- flowers
-
(and 2 more)
Tagged with:
-
From the album: 2016
Thrown bowls, cut at right angles to the rim. Thin slabs textured with bark, stamps, shells etc. - pieces attached to back part with front cut edge eased forwards to emphasise the contrast between the organic and engineered. Oxide washes applied at dry greenware stage, fixed in the bisqued firing. 3 back pieces were dipped in transparent glaze, front one dipped in tin white (to cover a repair that fired a different colour!). Fired to 1100oC in electric kiln.- 1 comment
-
- Earthenware
- Texture
-
(and 5 more)
Tagged with: