Copper & cobalt oxide glazes applied to bisque fired (950oC) pieces. Fired in a dustbin raku kiln at recent kiln building workshop. (1000oC) then plunged into sawdust to reduce.


From the album:

July 2019

  • 6 images
  • 0 comments
  • 7 image comments

Photo Information for Raku fired stoneware

Taken with Apple iPhone SE

  • 4.2 mm
  • 1/33
  • f f/2.2
  • ISO 32
View all photo EXIF information
 Share


Recommended Comments

Thank you - it was all very experimental, but I did mix the glazes myself, so hopefully can reproduce the results when I fire my own raku kiln

I think the tile is my favourite too Johnny. 

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.