  1. Hi All: When firing my kiln, I will wait until I have enough pieces to jam the kiln full. But the more that I thought about things, maybe this isn't the best practice. For example, if one piece blew up in the kiln, this could have the potential of ruining an entire shelf worth of sculptures. Just curious what others do. Do you wait for a full kiln or selectively fire based on the pieces? Thanks in advance for your input! Cheers!
  2. Cinat

    The Menagerie

    Cone 04 bisque. Glazed with Georgies interactive pigment "Tree Bark", then fired to Cone 6. No English bulldogs yet, but it sounds like an interesting project!
×
×