Raissas Posted November 28, 2021 Report Share Posted November 28, 2021 Hi, Newbie here! I was hoping I could get some help. I hope I’m posting in the right place. I have been taking ceramics classes for years (with the teacher firing my greenware and glazed items) but I’ve never had my own kiln. I now have an opportunity to purchase a used Paragon A88B kiln. The person is posting for an elderly family member in town and doesn’t know anything about the kiln. From the pictures the brick and elements look good but the kiln sitter looks really old. Can I replace that with an electronic version? Would I have to replace other electrical parts as well? Also the plate on the kiln lists 240 /120V what does that mean? I’ve added pictures. Any help would be appreciated. Thank you so much! Quote Link to comment Share on other sites More sharing options...
Marko Posted November 28, 2021 Report Share Posted November 28, 2021 (edited) Hi, your kiln looks in good shape. Have a go at it and try a firing before you get a, digital kiln controller. There are many available, but doing your research can narrow it down to what you want. The 240v is the power needed to run the kiln and get the element to the temperature your kiln is rated for. I wouldn't worry about the 120v. I have a Paragon A82B but never used the a 120v outlet on the control box. But you can call Paragon and ask. But more import than that is the amps. I see you have 25.9 amps. So the breaker must be at 30 amps or above. Best to ask Paragon or any qualified electrician. Get this done first then fire, then decide if you should spend the extra money on the digital kiln controller. Best of luck. ~marko Edited November 28, 2021 by Marko Quote Link to comment Share on other sites More sharing options...
Raissas Posted November 28, 2021 Author Report Share Posted November 28, 2021 14 minutes ago, Marko said: Hi, your kiln looks in good shape. Have a go at it and try a firing before you get a, digital kiln controller. There are many available, but doing your research can narrow it down to what you want. The 240v is the power needed to run the kiln and get the element to the temperature your kiln is rated for. I wouldn't worry about the 120v. I have a Paragon A82B but never used the a 120v outlet on the control box. But you can call Paragon and ask. But more import than that is the amps. I see you have 25.9 amps. So the breaker must be at 30 amps or above. Best to ask Paragon or any qualified electrician. Get this done first then fire, then decide if you should spend the extra money on the digital kiln controller. Best of luck. ~marko Thank you so much for your input! It is appreciated! Quote Link to comment Share on other sites More sharing options...
Dick White Posted November 28, 2021 Report Share Posted November 28, 2021 These old Paragon kilns are wired differently than most kilns these days. They are 120/240V, meaning some of the time the switches cause the elements to run on 120V and other times the elements use 240V. Consequently, the 4-wire plug and receptacle with a neutral is essential. The kiln will not operate properly on a conventional 3-wire 240V circuit. As Marko notes, a 30 amp circuit is minimum, but 40 amps is maximum. The outlet on the top of the control box is actually 120/240V, and was intended to power an extension ring if desired. Otherwise, it's not good for much else. As for digital controllers, the external wall-mount Skutt KM-1 is not suitable for this kiln. It will only work with a straight 240V 3-wire cord with no neutral. As noted, this kiln requires a neutral. The Orton AF4000 wall-mount controller can be special ordered with the 120/240V circuitry. If you are adventuresome and facile with electrical wiring, you could replace the kiln sitter mechanism with an Olympic ElectroSitter. Marko, Raissas and cadenrank 3 Quote Link to comment Share on other sites More sharing options...
oldlady Posted November 28, 2021 Report Share Posted November 28, 2021 brings back good memories, that is what i started out with in 1972. it worked very well, good luck to you with it. Marko and Raissas 2 Quote Link to comment Share on other sites More sharing options...
PotteryFarmer Posted December 13, 2021 Report Share Posted December 13, 2021 Did you ever fire it up? I just spent a ton of $ getting all my electric in. My electrician found it to be a doosy. Wound up special ordering 208v elements. Cleaned up all the relays. I test fired for 18+ hours and couldn't bend an 04 cone. I'm worried the settings are wired backwards. On low all 4 elements glow, medium every other, and high only the lowest element. I'm new to manual kilns, and I know theres a lit to learn. But not much info out there on this model kiln so any advice would be greatly appreciated! Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted December 13, 2021 Report Share Posted December 13, 2021 (edited) Go to the paragon website and get the wiring diagram for your model. Then you will need to check the wiring is appropriate for your house (If in a house, a neutral and two hots for 120v / 240v). 208 v does not make sense for a home installation it generally only occurs in three phase installations.. Then if all correct you will need to troubleshoot Edited December 13, 2021 by Bill Kielb Raissas and cadenrank 2 Quote Link to comment Share on other sites More sharing options...
Raissas Posted December 13, 2021 Author Report Share Posted December 13, 2021 On 11/28/2021 at 5:54 PM, Dick White said: These old Paragon kilns are wired differently than most kilns these days. They are 120/240V, meaning some of the time the switches cause the elements to run on 120V and other times the elements use 240V. Consequently, the 4-wire plug and receptacle with a neutral is essential. The kiln will not operate properly on a conventional 3-wire 240V circuit. As Marko notes, a 30 amp circuit is minimum, but 40 amps is maximum. The outlet on the top of the control box is actually 120/240V, and was intended to power an extension ring if desired. Otherwise, it's not good for much else. As for digital controllers, the external wall-mount Skutt KM-1 is not suitable for this kiln. It will only work with a straight 240V 3-wire cord with no neutral. As noted, this kiln requires a neutral. The Orton AF4000 wall-mount controller can be special ordered with the 120/240V circuitry. If you are adventuresome and facile with electrical wiring, you could replace the kiln sitter mechanism with an Olympic ElectroSitter. Thank you so very much for your input. While I am adventurous, I am a bit anxious to deal with older electronics. Quote Link to comment Share on other sites More sharing options...
Raissas Posted December 13, 2021 Author Report Share Posted December 13, 2021 On 11/28/2021 at 6:54 PM, oldlady said: brings back good memories, that is what i started out with in 1972. it worked very well, good luck to you with it. Ah, thank you! I haven't purchased. I'm just very anxious about not knowing if it will fire up or not. The person selling it does not have the right outlet to plug it in. :-( Quote Link to comment Share on other sites More sharing options...
Raissas Posted December 13, 2021 Author Report Share Posted December 13, 2021 8 hours ago, PotteryFarmer said: Did you ever fire it up? I just spent a ton of $ getting all my electric in. My electrician found it to be a doosy. Wound up special ordering 208v elements. Cleaned up all the relays. I test fired for 18+ hours and couldn't bend an 04 cone. I'm worried the settings are wired backwards. On low all 4 elements glow, medium every other, and high only the lowest element. I'm new to manual kilns, and I know theres a lit to learn. But not much info out there on this model kiln so any advice would be greatly appreciated! Actually no, I didn't buy it. I was afraid of what you are going through happening to me!! I'm so sorry, that really stinks. I think I'm going to just buy a new one. This is a great place to get a lot of information and make informed decisions. Best of luck to you. Quote Link to comment Share on other sites More sharing options...
Raissas Posted December 13, 2021 Author Report Share Posted December 13, 2021 3 hours ago, Bill Kielb said: Go to the paragon website and get the wiring diagram for your model. Then you will need to check the wiring is appropriate for your house (If in a house, a neutral and two hots for 120v / 240v). 208 v does not make sense for a home installation it generally only occurs in three phase installations.. Then if all correct you will need to troubleshoot Thank you for the info. Quote Link to comment Share on other sites More sharing options...
jhb Posted September 22, 2022 Report Share Posted September 22, 2022 I just bought an old dusty A88B ($40 + gas) with ok ceramics but with a creamed power box. It appears to have fallen onto its side (the 4 way switches are crushed and unrecognizable). At $40-60 ea, I"m hesitant to buy new ones only to encounter other problems. The sitter looks weary as well but only seems a bit rusty. Could I finesse the funky 50 year old electronics by simply operating the two element sets as two separate 120 V (30A) circuits each driven by its own modern 'infinite' power controller (variacs or TBD) per the attached jpg? Obviously each would have to be on it's own dedicated 120 v circuit. In addition, since there would now be two circuits, the sitter would have to drive a relay to switch both. A timer would be nice but I could live with cones (& vigilance) since I only need 1100F or so. If practical, can anyone suggest some low cost but adequate controllers and relays (and a timer)? Thx J Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted September 22, 2022 Report Share Posted September 22, 2022 (edited) 1 hour ago, jhb said: Could I finesse the funky 50 year old electronics by simply operating the two element sets as two separate 120 V (30A) circ I think I would opt for wiring the elements in series (high power) for each ring and feed them with their own infinite switch 240 v no nuetral. Fix up the sitter and use it to feed everything as a safety. Clearly remark everything for 240v operation with a ground. (3 wire). Just like more modern kilns that do not use a neutral. There are no 120v auxiliary loads this way so no need to run the neutral. The infinite switches will provide variability for firing. Safe neat wiring practices for load and temperature rating is also a must though IMO. 4 way switch below to give you an idea of typical operation. If you wire two elements in series they can be driven by 240 v without a neutral at their junction. Edited September 22, 2022 by Bill Kielb Quote Link to comment Share on other sites More sharing options...
PeterH Posted September 22, 2022 Report Share Posted September 22, 2022 For what it's worth, a firing schedule by original 4-way switch positions and the resultant power to the elements. Quote Link to comment Share on other sites More sharing options...
neilestrick Posted September 22, 2022 Report Share Posted September 22, 2022 Bill's solution is the simplest and best way to go, because that box isn't set up for relays. There's no heat shield, and it may or may not be deep enough or have enough ventilation for them. Quote Link to comment Share on other sites More sharing options...
oldlady Posted September 23, 2022 Report Share Posted September 23, 2022 to anyone seeing a kiln like the photo in the original post, that is a really good kiln for a first one. notice how little firing has been done in it. look at the shiny metal above the peepholes. nobody fired that thing to 2300 degrees as it says on the label. if they had, there would be smoky burn marks at the top of the peepholes. the very clean top bricks show minimal heating. the floor is pristine, nobody ran glazes all over it. the elements may be original to the date of purchase. i would bet it was used by someone whose hobby was painting bisqued ware from a " ceramics shop" that today we would call a "paint your own pottery". that would mean it was only used to cone 06, about 1800 degrees F if i remember it right. the sitter is not as clean as it could be, a damp rag would remove that white stuff. the tiny bits of surface rust i see here and there are nothing to worry about. yes, it is not in sections for easy moving but it is only 18 inches deep and not that heavy. it is not so wide that going through a normal door will be a problem. it gave good service to someone back in the 1970s and would continue to give good service today with the proper electrical connections. it would be a definite buy for me. Quote Link to comment Share on other sites More sharing options...
neilestrick Posted September 23, 2022 Report Share Posted September 23, 2022 I've got two kilns in my shop right now that I'm converting to digital systems. One is 35+ years old and never been fired, the other is 33 years old and has only been fired a handful of times and only to low fire temps. I only paid $1000 for the pair. Old kilns can be a great value! Quote Link to comment Share on other sites More sharing options...
jhbb Posted October 4, 2022 Report Share Posted October 4, 2022 Bill K Thanks for your insight on my A88B rewiring (22Sep comment). I had hoped to simplify the circuitry (dropping the 'funky' neutral) by using two 120V/30A infinity switches, to drive two separate 120V line circuits (easier to access in my garage) - one circuit for each pair of elements. Thus, this drove the need to modify the sitter relay to drive two separate circuits. But they (high amp switches) don't seem to exist (lots of dryer infinity switches at 120/240-15A but nothing apparent for the 30A I'd need). And an extra sitter relay adds unnecessary complication Thus your recom to stay with the sitter 240V relay makes sense. j Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted October 5, 2022 Report Share Posted October 5, 2022 (edited) Your kiln appears to be 6226 watts or 25.9 amps, let’s call it 26 amps. 1/2 the power is from the top ring and 1/2 the power is from the bottom ring. So 26 amps/2 = 13 amps load on each infinite switch. The elements must stay in series (No neutral connected at this junction) and each series group gets fed from the infinite switch. H1 to one side of the element group and H2 to the other side. Sketch it up and post it just to be sure - folks here will double check. Notice a 40 amp fuse was required, today the breaker size is 125% of the load not to exceed 150% meaning 35 amps for todays breakers. This is a special requirement for kilns to make sure the breaker doesn’t overheat and wear out. You 30 amp breaker is undersized and this ought to have #8 wire run to it as well. Edited October 5, 2022 by Bill Kielb Quote Link to comment Share on other sites More sharing options...
Dana Stripe Posted October 7, 2022 Report Share Posted October 7, 2022 On 9/22/2022 at 10:33 PM, neilestrick said: I've got two kilns in my shop right now that I'm converting to digital systems. One is 35+ years old and never been fired, the other is 33 years old and has only been fired a handful of times and only to low fire temps. I only paid $1000 for the pair. Old kilns can be a great value! Neil, Be sure and post some pictures when you get them completed, would like to see how you did it. Quote Link to comment Share on other sites More sharing options...
Ann E. V. Posted April 17, 2023 Report Share Posted April 17, 2023 Hello, I was given a nearly identical Paragon A88B kiln but it is rated for 230 Volts, instead of 120/240V, 25 Amps instead of 25.9A, 5750 Watts instead of 6226 W, and the plug is a different configuration. It must be an earlier or later version. I would like to add a computerized controller to make it easier for me to use. I am looking at the Bartlett V6-CF control board as it is much more reasonably priced than the Skutt wall mount controller. Since this kiln does not use both 120 and 240V this should work, I think?? I definitely would have my electrician do the re-wiring. Any information on the best controller and how to go about the retrofit would be greatly appreciated. Thank you! Quote Link to comment Share on other sites More sharing options...
neilestrick Posted April 17, 2023 Report Share Posted April 17, 2023 2 hours ago, Ann E. V. said: I am looking at the Bartlett V6-CF control board as it is much more reasonably priced than the Skutt wall mount controller. The Bartlett V6-CF is just a controller, whereas the Skutt wall mount has a controller and also has all the parts that make the controller work- relays, thermocouple, etc. The controller is just one part of the system that makes a digital kiln function. There are cheaper versions of wall mount controllers out there, though. Check out Orton and Olympic. Your kiln will pull 26 amps on 240 volt service (what you have at your house), and it will need a 35 or 40 amp breaker with 8 gauge wiring. Quote Link to comment Share on other sites More sharing options...
Ann E. V. Posted April 17, 2023 Report Share Posted April 17, 2023 Many thanks, Neil! I wondered about the relays etc. but manufacturers descriptions were pretty vague. I'll check that the a88B is wired correctly! Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.