Mark C. Posted August 29, 2020 Report Share Posted August 29, 2020 Much of reclaim is trimmings and they do not have the fines in them near as much.Also when clay drys and is rewetted the great organics need to start all over making bacteria which sets back clay (short) I only use wetter clay in my mixer. If it dry trimmings it out in the trash for me -usually 15 gallons per week before covid. I find my own fines in slop from water bucket and splash pan are enough to keep the clay have some legs for throwing. That additive A might be great in milkshakes as well. sounds like a cure for everything that ales you. Link to comment Share on other sites More sharing options...
CactusPots Posted August 29, 2020 Report Share Posted August 29, 2020 What ales me is not enough ale in me. Link to comment Share on other sites More sharing options...
Babs Posted August 29, 2020 Report Share Posted August 29, 2020 5 hours ago, CactusPots said: @CatcusPots. So you're reclaim.not short. Don't need anything but slops from.throwing bucket Link to comment Share on other sites More sharing options...
liambesaw Posted August 29, 2020 Report Share Posted August 29, 2020 I like veegumt in my clay body, I think additive A might be cheaper if it's only 75 bucks for a 50 pound bag! Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.