Cavy Fire Studios Posted December 18, 2015 Report Share Posted December 18, 2015 I've never seen a cone do this in a sitter! I just calibrated Fred's sitter, because he was underfiring, but I think I did it too much...lol... Ah, well! Better vitrification, huh? Link to comment Share on other sites More sharing options...
Marcia Selsor Posted December 18, 2015 Report Share Posted December 18, 2015 It looks about right to me. To calibrate the arm or rod on the sitter, there is a template to use that you slide onto the cone supports and the rod inside and adjust the lever on the outside. The lever can slip over time , so be sure to tighten the set screw well and check regularly. That cone looks like mine when I fire my test kiln. Marcia Link to comment Share on other sites More sharing options...
neilestrick Posted December 18, 2015 Report Share Posted December 18, 2015 90 degrees is perfect, so you're pretty darn close. Link to comment Share on other sites More sharing options...
oldlady Posted December 18, 2015 Report Share Posted December 18, 2015 looks normal to me, too. when you get minibars, they will look the same. forget the cone, show us the beautiful things you fired. Link to comment Share on other sites More sharing options...
Cavy Fire Studios Posted December 18, 2015 Author Report Share Posted December 18, 2015 I totally will! I just gotta edit the photos, heehee. You guys think it's right? Butttt it curls weird like a "J..." Should I leave his trigger plate be? This is kind of a mutated-looking 3 o'clock... O.o Link to comment Share on other sites More sharing options...
oldlady Posted December 18, 2015 Report Share Posted December 18, 2015 you have enough to worry about, stop. Link to comment Share on other sites More sharing options...
oldlady Posted December 19, 2015 Report Share Posted December 19, 2015 it is not fair to post all those wonderful pictures to the gallery without telling us. if it is 12/19 or later, anyone reading this stop and look at guinea's gallery. Link to comment Share on other sites More sharing options...
rayaldridge Posted December 25, 2015 Report Share Posted December 25, 2015 Her work really is terrific, isn't it? There's such a sense of vivid movement in her surfaces. Great stuff! Link to comment Share on other sites More sharing options...
Rae Reich Posted January 6, 2016 Report Share Posted January 6, 2016 Your mastery grows ever more masterful. Delicious terra cottas, juicy florals, critters are tastefully done and seem to be portraits. I'll take two of everything, lots of butter! Link to comment Share on other sites More sharing options...