Kiln cooling. Happy tomorrow? LOL
- Show previous comments 2 more
-
pics brother- pics!
-
Gonna put them up later this evening.
-
glazenerd, there in the gallery.
-
I just started working with a ^5 laguna that I took to ^6. got some translucency. but not overall. Guess I need to go thinner. Help
- Show previous comments 9 more
-
I have been teaching myself to use less water. I set out one cup of water to throw 3-5lbs of porcelain. It forces you to use less water.
-
Going with the original question .. which Laguna clay are you trying to get translucent?? Not all Cone 5/6 porcelain will be no matter how you fire them.
-
Chris, TBH, I don't remember. I had thrown the box away and without thinking about what clay it was. I know it was porcelain because I maked it on the bag that I had soaked in a 5 gal bucket. Mystery Porcelain:P. I like working with it. I get my clay from either, http://www.roadrunnerceramics.com/ in San Antonio or http://www.armadilloclay.com/ in Austin, Tx. This clay has some translucency in some parts. I would love a recommendation.