  1. I will conquer this black clay bloating problem if its the last thing I do on this earth!

    1. Show previous comments  5 more
    2. Cavy Fire Studios

      Cavy Fire Studios

      Seattle Pottery claims their vashon series goes to ^6, as well as their crystal white porcelain. All of those bodies bloat like a gassed-up politician. Sooooo...either the clay's being over-fired, or your kiln might be a bit too hot. :P

    3. Joseph Fireborn

      Joseph Fireborn

      Maybe, but others have stated they have fired to cone 6. I use self supporting witness cones. I am not over firing, if anything under firing. I go to about 5.5.

    4. High Bridge Pottery

      High Bridge Pottery

      Good luck :D I have no idea about bloating.

×
×