It's 7AM; 1080 deg F on my first kiln firing in more than 4 years and the first ever ^04 bisque/glaze firing with my new Orton digital controller...The first 2 hours were a real disappointment when i saw the TCL message on the controller. The kiln didn't fire. I had ultimately realized that I hadn't pushed the reset button on the kiln sitter. Pushed the button and the kiln came to life!The firing took 12Hrs 18 min, but only reached 1941 degrees which is about halfway between ^...
-
Always hated when I just "fixed" something, and it does not work right.
-
You must be thrilled, after 4 years!