Started to glaze the bowls but got an order for a dozen medium, tri-tube bud vases too...the first job for the extruder...
- Show previous comments 1 more
-
Pics please when you finish.
-
Pix of the latest glaze run...the customer bought 13 instead of 10 bowls. 18-54,55 2nd is the same glaze pattern after removal of a defect in each bowl and firing again. All are Amaco PC glazes layered for effects. In some cases Duncan's RG704 Shino Cream was banded to create the white edge runs...
-