Posted 23 May 2013 - 12:42 PM


MAY 27- new image added
JUNE 22- new image added

JULY 23- new image added


As I develop as a potter, I'm becoming increasingly sensitive to proportion and flow in my work.

I'll often create a piece these days, and have an instantaneous, overwhelming sense of dissatisfaction with the form I just generated. Sometimes this leads to smashing things in a fit of pique... but other times I second-guess my own instincts.

Overall, I think it's a healthy process... but I'm not always able to completely quantify why I'm dissatisfied with a particular piece.

Anyhow, I may post an example here once in awhile, in hopes of an objective opinion or two.

Here's a garden lantern I assembled a couple days ago. Something about this piece strikes me as a bit off... but I can't quite pin down whether the stand is too narrow for the top elements, or or whether I don't like the depth and curve of the top piece.

Or... maybe I'm just a bit too twitchy these days.

Thoughts?

IMG_1521_zpsd5a08374.jpg


Not all who wander are lost

#2 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 23 May 2013 - 01:15 PM

As I develop as a potter, I'm becoming increasingly sensitive to proportion and flow in my work.

I'll often create a piece these days, and have an instantaneous, overwhelming sense of dissatisfaction with the form I just generated. Sometimes this leads to smashing things in a fit of pique... but other times I second-guess my own instincts.

Overall, I think it's a healthy process... but I'm not always able to completely quantify why I'm dissatisfied with a particular piece.

Anyhow, I may post an example here once in awhile, in hopes of an objective opinion or two.

Here's a garden lantern I assembled a couple days ago. Something about this piece strikes me as a bit off... but I can't quite pin down whether the stand is too narrow for the top elements, or or whether I don't like the depth and curve of the top piece.

Or... maybe I'm just a bit too twitchy these days.

Thoughts?

Posted Image



You already said it. I think base is needs more strength. But don't go wrecking it yet. Maybe sippmple as adding platform below legs. Or "earth ring" if you will. I think that the the designs strength is weakened by weaker base. At first glance I'd be weary of it toppling over.
The top is on point design wise.

The traditional legged lanterns I've seen all had beefier legs.

I'd be proud to own it as is. But if I had to pick between one with stronger base I'd pick stronger base.

Your work is very much organic..... visualizing the following may be difficult.....
On flip side of coin this composition will work in a non traditional setting, house with simple open lines, modern, steel and glass, inorganic design, Horizon pool..... (In this case a single glaze finish letting composition do all the talking).

LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#3 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 23 May 2013 - 01:36 PM

You already said it. I think base is needs more strength. But don't go wrecking it yet. Maybe sippmple as adding platform below legs. Or "earth ring" if you will. I think that the the designs strength is weakened by weaker base. At first glance I'd be weary of it toppling over.
The top is on point design wise.

The traditional legged lanterns I've seen all had beefier legs.

I'd be proud to own it as is. But if I had to pick between one with stronger base I'd pick stronger base.

Your work is very much organic..... visualizing the following may be difficult.....
On flip side of coin this composition will work in a non traditional setting, house with simple open lines, modern, steel and glass, inorganic design, Horizon pool..... (In this case a single glaze finish letting composition do all the talking).


Thanks... that backs up some of my own thinking. Much obliged.

The funny thing is that it's almost a direct translation from my sketch book... and I liked it just fine as a drawing. Odd how the extra dimension can change your thinking...
Not all who wander are lost

#4 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 23 May 2013 - 02:50 PM

I like it. For me the weak parts are where you make cut-outs. The bowl shape is strong, the donut in the center is strong and the piece on top is strong. The decoration is nice. The two pieces that have cut-outs, especially the bottom one are weak. By weak I don't mean they need to be bigger, thicker or stronger (even though Big Lou is right about the bottom), I mean a stronger form for the eye. It's the edges of the cut-out that are a problem. Even smoothing and rounding those edges would help some, but it needs more than that. With that said, let me repeat that I like it.

Don't over think it. Walk away from it for at least a day and look at it with fresh eyes.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#5 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,111 posts
  • LocationRaleigh, NC

Posted 23 May 2013 - 03:14 PM

Is that top curled object a hollow extrusion? If so, I see it filling with water when it rains then either stinking with algae or growing mosquitoes.

If those legs were wider apart on your next one, it would make a visually stronger base. Right now the width difference between them and the bowl shape is what throws it off, but I would not make the bowl form smaller. They could also look good shorter, wider and studier.
I think you are onto a very good form ... I like the top pieces and the base is definitely on its way to being there.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#6 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,303 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 23 May 2013 - 03:41 PM

I think the base is to weak-the form seems top heavy-mening the legs seem to little. I think it would fall over easy.
I also ope drainage is built in otherwise its someones problem.
I agree with Jim that the cut outs are the main issue .
Mark
Mark Cortright
www.liscomhillpottery.com

#7 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,430 posts
  • LocationThe Hawkeye State

Posted 23 May 2013 - 06:38 PM

That's a very nice design. I do agree with the others, regarding the base. A bit wider, would help with the overall appearance.
"Anything worth believing, is worth questioning"

#8 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 23 May 2013 - 09:39 PM

Thanks everyone- lots of comments here in line with what I've been thinking.

Chris- the top piece was thrown and cut, with caps... so no algal gardens, hopefully.

Aside from the width of the base, I agree that the cutouts are wrong. Apart from other considerations, the shape is almost moorish- doesn't really fit with the overall Japanese aesthetic.
Not all who wander are lost

#9 Denice

Denice

    Advanced Member

  • Members
  • PipPipPip
  • 1,266 posts
  • LocationWichita, Kansas

Posted 23 May 2013 - 10:51 PM

I agree with Chris and BigLou but I wouldn't trash it yet make two more and try modifications on each one and then compare. See what modifications you want to keep or throw out and then make another with your new changes. Denice

#10 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,303 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 24 May 2013 - 12:37 AM

Thanks everyone- lots of comments here in line with what I've been thinking.

Chris- the top piece was thrown and cut, with caps... so no algal gardens, hopefully.

Aside from the width of the base, I agree that the cutouts are wrong. Apart from other considerations, the shape is almost moorish- doesn't really fit with the overall Japanese aesthetic.


If the Japanese aesthetic is what you are after check out the book -Japanese Homes and their Surroundings by Edward S. Morse
I have had this book since the early 70s it a good resource.
Mark
Mark Cortright
www.liscomhillpottery.com

#11 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 24 May 2013 - 01:01 PM


Thanks everyone- lots of comments here in line with what I've been thinking.

Chris- the top piece was thrown and cut, with caps... so no algal gardens, hopefully.

Aside from the width of the base, I agree that the cutouts are wrong. Apart from other considerations, the shape is almost moorish- doesn't really fit with the overall Japanese aesthetic.


If the Japanese aesthetic is what you are after check out the book -Japanese Homes and their Surroundings by Edward S. Morse
I have had this book since the early 70s it a good resource.
Mark


Cool- thanks. I need to dive into that world more deeply, since it's definitely an influence.

Looking at the design (and re-visiting images of some traditional lanterns that I like) one thing that's very consistent across the trad designs is that the 'plinth' (the doughnut-like piece that the actual lantern element rests on) is generally quite robust- often broader than the actual lantern element.

As the piece stands, I worry that broadening the base would mar the vertical flow... but I can see that a fatter plinth element might solve this. Something to incorporate for the next one.
Not all who wander are lost

#12 Diane Puckett

Diane Puckett

    Advanced Member

  • Members
  • PipPipPip
  • 398 posts
  • LocationAsheville, NC

Posted 24 May 2013 - 06:32 PM

I love your design, enough to copy it for inspiration for my own garden. I agree with what has been said about the base. The one you made, especially with the cut outs, gives the base a lot of lift.

Robin Hopper's book on functional pottery has at least one chapter on form and proportion. I took some drawing and design classes hoping to get more information on this topic but did not find the classes helpful. If anyone knows of a good book about this just for potters, I would love to know about it.
Diane Puckett
Dry Ridge Pottery

#13 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 27 May 2013 - 02:16 PM

I love your design, enough to copy it for inspiration for my own garden. I agree with what has been said about the base. The one you made, especially with the cut outs, gives the base a lot of lift.

Robin Hopper's book on functional pottery has at least one chapter on form and proportion. I took some drawing and design classes hoping to get more information on this topic but did not find the classes helpful. If anyone knows of a good book about this just for potters, I would love to know about it.


Thanks Diane... I'd love to see the piece that you generate when it's finished.

In the meantime, here's another recent effort (below).

I love making these complex assemblages.. but again, I don't feel like my sense of proportion and flow is 100% calibrated. I generally know when a piece 'works' (I can look at a Hans Coper vessel and swoon)... whereas I can look at some of my work and see that it's not entirely 'there'... but not feel confident as to the exact reason.

I generally like this lantern... (I was able to restrain myself from smashing it)... but I think there are some areas for improvement. Rather than outlining these, however, I'm interested to hear what other people think...

Posted Image
Not all who wander are lost

#14 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 27 May 2013 - 03:11 PM


I love your design, enough to copy it for inspiration for my own garden. I agree with what has been said about the base. The one you made, especially with the cut outs, gives the base a lot of lift.

Robin Hopper's book on functional pottery has at least one chapter on form and proportion. I took some drawing and design classes hoping to get more information on this topic but did not find the classes helpful. If anyone knows of a good book about this just for potters, I would love to know about it.


Thanks Diane... I'd love to see the piece that you generate when it's finished.

In the meantime, here's another recent effort (below).

I love making these complex assemblages.. but again, I don't feel like my sense of proportion and flow is 100% calibrated. I generally know when a piece 'works' (I can look at a Hans Coper vessel and swoon)... whereas I can look at some of my work and see that it's not entirely 'there'... but not feel confident as to the exact reason.

I generally like this lantern... (I was able to restrain myself from smashing it)... but I think there are some areas for improvement. Rather than outlining these, however, I'm interested to hear what other people think...

Posted Image


Nice. Much stronger shape. Solved my complaint about the cut-outs elegantly! The cut-out here works.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#15 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 27 May 2013 - 03:47 PM

Nice. Much stronger shape. Solved my complaint about the cut-outs elegantly! The cut-out here works.

Jim


Cool- thanks Jim.

Mind you- I'm not sure that I solved your complaint so much as side stepped it. I definitely want to make lanterns with a more traditional tripod base... that's where I'll definitely need to work on a stronger base...
Not all who wander are lost

#16 Biglou13

Biglou13

    Advanced Member

  • Members
  • PipPipPip
  • 1,258 posts
  • LocationNorth Florida

Posted 27 May 2013 - 04:26 PM

Ok I'm going on first impression....

Bottom circle / wheel. A bit too strong. The lantern house or top should be dominant feature with base and legs supporting. Here my eye goes to wheel shape vs. moving with in composition. The wheel shape ends up demanding to much attention .....
Side view works.
Again it's a lantern I would not be ashamed of. I would be proud to own it.

Your first one had to delicate legs this one a little to beefy.......

First thought is thinner wheel, larger open circle. Possibly larger feet.

On second look while compositionally sound d side view . An issue with this is support system is linear, as in there is no leg support tipping forward or backward. you still have three point attachment however linear.

I'm imagining same design with four foot base. Or a three foot base upon wheel sits. Which leans towards traditional designs .

I think base must be strong (like in martial arts). It is light for both proverbial and literal pathway.

LEC potttery  on facebook, instagram

 

The true sign of intelligence is not knowledge but imagination.
-Albert Einstein


#17 oldlady

oldlady

    single firing an electric kiln to cone 6

  • Members
  • PipPipPip
  • 3,448 posts
  • Locationharpers ferry west va and pinellas park fl

Posted 27 May 2013 - 04:47 PM

if you hold a ruler against the photo, side view, you will notice that the center line is not in the center of the piece. otherwise looks ok. what do the local mosquitoes say about the top swimming pool for their larva? i bet they like it.
"putting you down does not raise me up."

#18 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 27 May 2013 - 04:50 PM

Ok I'm going on first impression....

Bottom circle / wheel. A bit too strong. The lantern house or top should be dominant feature with base and legs supporting. Here my eye goes to wheel shape vs. moving with in composition. The wheel shape ends up demanding to much attention .....
Side view works.
Again it's a lantern I would not be ashamed of. I would be proud to own it.

Your first one had to delicate legs this one a little to beefy.......

First thought is thinner wheel, larger open circle. Possibly larger feet.

On second look while compositionally sound d side view . An issue with this is support system is linear, as in there is no leg support tipping forward or backward. you still have three point attachment however linear.

I'm imagining same design with four foot base. Or a three foot base upon wheel sits. Which leans towards traditional designs .

I think base must be strong (like in martial arts). It is light for both proverbial and literal pathway.


Thanks. You seem to have an affinity for eastern forms, so this carries a lot of weight.

You're quite right about the lack of support on the front-back axis. I though about making the base a disc, but was concerned that doing so would add one element too many (I'm not a big fan of the 'frosty the snowman' look). As it is, this one is definitely going to have to be an interior piece (probably put glass and a soft electric bulb in the lantern).

I sketched a whole range of ideas, with the 'lantern house' varying in size. This one was intermediate... but I definitely think I might have done better to make it larger.

Cheers...

David
Not all who wander are lost

#19 Kohaku

Kohaku

    Huffing cobalt over a Raku kiln

  • Members
  • PipPipPip
  • 331 posts
  • LocationMoscow, Idaho

Posted 27 May 2013 - 04:56 PM

if you hold a ruler against the photo, side view, you will notice that the center line is not in the center of the piece. otherwise looks ok. what do the local mosquitoes say about the top swimming pool for their larva? i bet they like it.


I think this one is going to be staying indoors... as Biglou noted, the base lacks the kind of tri-point support you'd want for an outdoor feature. It'll be about 16 inches high when fired.

If I was going to market it as a garden piece, I'd cap the swimming pool.

Mind you, I live in Northern Idaho, where the mosquitos are sparse and lily-livered. Nonetheless, as a canoeist with multiple trips above the Arctic circle, I should be a bit less complacent.

Thanks for the feedback!
Not all who wander are lost

#20 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,111 posts
  • LocationRaleigh, NC

Posted 27 May 2013 - 08:55 PM

I think you have to focus on the relationship between the inverted bowl shape and the base. The rest will fall into place when those two are in balance.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman




0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users