Mark C. Posted April 11, 2023 Report Share Posted April 11, 2023 (paid more attention to closing up damper for the cool down, and I fired on a fairly thick bed of silica. ) I think this really made the differeance Pres, Mudfish and Babs 3 Quote Link to comment Share on other sites More sharing options...
Pres Posted April 11, 2023 Report Share Posted April 11, 2023 Slow cooling is much better for wide flat forms, I fire all electric, and for years fired without a setter. . . .I wanted to be able to fire down. Firing down in electric is a big thing now, but with setters more difficult to do. best, Pres Mudfish 1 Quote Link to comment Share on other sites More sharing options...
Mudfish Posted June 21, 2023 Author Report Share Posted June 21, 2023 continued success with these large platters. Thanks again to all Hulk, Babs, Kelly in AK and 2 others 5 Quote Link to comment Share on other sites More sharing options...