Lbraddock Posted January 21, 2023 Report Share Posted January 21, 2023 I was wedging Clay on my board without realizing there was a dusting of sawdust on the surface. As I wedged I realized the presence of fine sawdust particles in the clay. Should I dispose of this clay or could it be used? Quote Link to comment Share on other sites More sharing options...
Denice Posted January 21, 2023 Report Share Posted January 21, 2023 The sawdust will burn out, it depends on how coarse it is on the texture the clay is after firing. It depends on how sensitive your skin is when it comes to throwing it, I threw a large bowl with large grain sawdust in it, wasn't to bad. I had a teacher that demonstrated throwing clay with broken flourescent bulbs in it. He got the vase thrown and had tiny cuts all over his hand that were bleeding. He wiped off the blood and said no big deal. Denice Quote Link to comment Share on other sites More sharing options...
Min Posted January 21, 2023 Report Share Posted January 21, 2023 1 hour ago, Denice said: I had a teacher that demonstrated throwing clay with broken flourescent bulbs in it. He got the vase thrown and had tiny cuts all over his hand that were bleeding. He wiped off the blood and said no big deal. Maybe not the brightest bulb? glazenerd 1 Quote Link to comment Share on other sites More sharing options...
Bam2015 Posted January 22, 2023 Report Share Posted January 22, 2023 21 hours ago, Denice said: I had a teacher that demonstrated throwing clay with broken flourescent bulbs in it. He got the vase thrown and had tiny cuts all over his hand that were bleeding. He wiped off the blood and said no big deal. Denice But, why?!?!? Quote Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted January 22, 2023 Report Share Posted January 22, 2023 That kind of move right there is why Gen z isn’t wrong for thinking the Elders need therapy*! Hi and welcome to the forum, @Lbraddock! We don’t usually lead with stories like that, but it’s never dull here. After my left eyelid stops twitching, we should get back to the sawdust. Okay. A little bit of fine sawdust that you hadn’t initially noticed on the board likely won’t hurt anything. If it’s wedged in thoroughly, it might not even leave noticeable voids. Unless there was a lot of it and it was from something like pressure treated lumber or MDF, I can’t even see it being an issue burning out in the bisque. If you’re handbuilding and not throwing, I wouldn’t even worry about it. If you’re throwing, it depends on your tolerance for gritty textures. If you’re really concerned about it and it’s just a few pounds, you could use it for waster cookies under glaze tests, or cone packs. *edited to add: I’m making a broad generalization with that statement, based on the comments my kids make to me when I tell them similar stories from my life. I’m 20-30 years older than Gen Z myself, and am included in their “elder” category. Getting therapy doesn’t mean someone is crazy, and I think that therapy and good mental health is for everyone. Pres 1 Quote Link to comment Share on other sites More sharing options...
Denice Posted January 22, 2023 Report Share Posted January 22, 2023 This was part of a demonstration on how broken bulbs fired in the clay create a clear glaze. He had us find old bulbs and break them over a trash can outdoors because the powder in side of them was dangerous to breathe. We washed them and brought them to class, this was part of our assignment. I handbuilt my pot, we had only one wheel in the class, my teacher would pick one boy to teach him how to throw. Girls weren't given this honor we were too weak, I was a head taller than my teacher. had broad shoulders and large hands. The glaze it made was a ugly dingy clear. In the late 60's many of the psychodelic albums were played during class and I am pretty sure my teacher was smoking marijuana in his pipe. After I left he somehow managed to burn down the classroom, they rewarded him by replacing the electric kilns with a big gas kiln. It was a interesting and fun time of my life and I didn't do drugs, smoke or drink. Denice Hulk 1 Quote Link to comment Share on other sites More sharing options...
Pres Posted January 23, 2023 Report Share Posted January 23, 2023 I once was throwing with some clay I have wedged in college. Seems someone put an old rib in the slop bucket that got broken up in the pug mill. . . I did have cuts after doing the cone up and down the second time. . . . really was not comfortable throwing for a while, and it taught me to bread stack the clay after cutting a couple of times before hand wedging or throwing the clay. Larger pieces takes time for the small bits to show up. Felt like an idiot, but lesson learned. best, Pres Quote Link to comment Share on other sites More sharing options...
Min Posted January 24, 2023 Report Share Posted January 24, 2023 On 1/21/2023 at 7:58 AM, Denice said: I had a teacher that demonstrated throwing clay with broken flourescent bulbs in it. On 1/22/2023 at 9:13 AM, Denice said: He had us find old bulbs and break them over a trash can outdoors because the powder in side of them was dangerous to breathe. We washed them and brought them to class, Just in case someone thinks this would be something to try, apart from the obvious risks of cutting hands with broken glass there is also the hazard of mercury exposure from florescent bulbs. This practice is not recommended. https://www.osha.gov/sites/default/files/publications/mercuryexposure_fluorescentbulbs_factsheet.pdf Quote Link to comment Share on other sites More sharing options...
Denice Posted January 25, 2023 Report Share Posted January 25, 2023 We were told not to breathe the dust buy not why. This is a good topic for people with flourescent bulbs in their studio's, I am about to replace my bulbs with LED's and my husband is also replacing the ones in his garage. Now we know to take them to hazardous waste instead of our trash can. Thank you Min for your information and help, not questioning some ones sanity. I am glad I mentioned that class I have learned something new that helps prevent soil contamination. Denice Quote Link to comment Share on other sites More sharing options...
Pres Posted January 25, 2023 Report Share Posted January 25, 2023 I replaced all of the old fluorescent bulbs in the shop within the last 5 years. The amount of light the new ones put out and the quality of the light is astounding. I much prefer the LED's and wonder why I waited so long. best, Pres Kelly in AK and akilpots 2 Quote Link to comment Share on other sites More sharing options...
SmokerX Posted June 27, 2023 Report Share Posted June 27, 2023 (edited) 9 out of 10 dentists agree mercury is good for your teeth since mercury amalgam fillings and Anderson Cooper says mercury in vaccines is all organic. I replace my bulbs with LED because of high efficiency. Because a 60 watt equivalent incandescent is running 10 true watts power consumption. The true 17 watt LED bulbs are the best but expensive like sometimes 30 bucks each and the led chips weaken so by the end of the year theyre pobably producing a single candle worth of lumens it seems. Something is up with mercury in flourescent. When you google mercury vapor in google images it just shows you a bunch of light bulbs. I said show me mercury vapor not light bulbs. Thats a good indication something is up. Since I imagine mercury vapor is an odorless colorless gas you can plug right into the atmosphere. Thats the kind of mercury in mercury vapor bulbs,Gaseous mercury. One time I was in New Orleans and a Giant truck filled with flourescent tube lights dropped their load and 1000's of bulbs broke in front of the tourists. None the less I held my breath walking by that, because whatever stuff those things put into the environment when they break. I wouldnt be ball milling glass from the risk of silicosis, and the guy just said its not a good looking glaze. Like maybe if its the apocalypse and were trying to waterproof our primitive pottery I would start ball milling glass with extreme precautions. You can write the concept of glaze as glass on a chalkboard. Then do the lightbulb glass trick as glaze and take a picture one time. Just so everyone can see it(i want to see it)...Sounds like a cool professor though. Alright I tried everything. They wont show me light bulbs as glaze or light bulbs in a clay body. The closest I got was speckled cup-recycled glass clay body, Sorry, It looks like trash. It looks like a cup id be drinking out of 11,000 years from now in the peak of the next warm age. Edited June 27, 2023 by SmokerX Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.