I just reviewed the results of my ^5 test tiles of my repertoire of Amaco glazes and am totally disappointed with the outcomes on one hand and happy on the other hand.

Disappointed because the results were less than I had hoped for to use on the Laguna black clay pots that I made. I had glazed 4 pieces of the black clay just to see how they would come out of a ^5 firing. The black clay was grogged and when they came out of the kiln, the result looked almost like a textured matte finish, even though the glaze was a gloss. The color was also more muted which was probably due to the base color of the black clay. Though, too, the colors on the test tiles, which were a grogged white clay, seemed more muted than the work I've done at ^6, but didn't have the texture of the black clay...

Happy because I only have 10 more bisqued black clay pieces to glaze and fire and will probably just trash them to save the glaze and price of electricity for the firing. and just stay away from the black clay in the future as a result of these tests.

I'll post photos of the finished pieces later...

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.