Chilly Posted October 12, 2019 Report Share Posted October 12, 2019 On 10/10/2019 at 4:26 PM, Stephen said: The one problem I have with the sheetrock though is that stacking them right after mold release will result in my tiles being flattened to bigger dimensions and resulting thickness reduced. Have you tried using spacers between each sheet? Link to comment Share on other sites More sharing options...
Stephen Posted October 12, 2019 Report Share Posted October 12, 2019 1 hour ago, Chilly said: Have you tried using spacers between each sheet? well there's an idea, I will give that a go, thanks! Link to comment Share on other sites More sharing options...
Marcia Selsor Posted October 12, 2019 Report Share Posted October 12, 2019 I dry my large slabs between sheetrock boards lined with newsprint. I get end rolls from the local newspaper and have it on a gift wrap paper dispenser. I also was the edges as someone mentioned earlier that edges drying out first can cause warping. Marcia Link to comment Share on other sites More sharing options...
Mark C. Posted October 12, 2019 Report Share Posted October 12, 2019 I like to use the paper as stated above and also weight the pile so warpage cannot happen in the dry process. Link to comment Share on other sites More sharing options...
Stephen Posted October 12, 2019 Report Share Posted October 12, 2019 1 minute ago, Mark C. said: I lioke to use the paper as stated above and also weight the pile so warpage cannot happen in the dry process. That's what I left out, I plop a half kiln shelf on top the sheetrock. Link to comment Share on other sites More sharing options...