Jump to content

Anoka Sand Celadon Bowl


Recommended Posts

this is from my last firing, cone 8 reduction, needed just a bit more heat  but turned out good . This is my anoka sand Celadon glaze, and porcealin both made with the anoka sand  i use 56% anoka sand in the body and glaze, the anoka sand is an arkose sand having about 25% feldspar in it  the iron deoration around the rim is diabase basalt 100%

post-80534-0-03644400-1498923065_thumb.jpg