5th night in a row firing. I will figure out this celadon thickness if its the death of my elements.
- Show previous comments 11 more
-
What seems to be the problem? Those pictures look great!
-
Thanks Benzine. It is just a very difficult application issue. If I don't apply it thick I get a pale blue clearish.
-
I am going to try using a deflocculant to thin the glaze out when I am mixing it instead of using as much water, then I will use a some vinegar or epsom salt to thicken it to where I want it. I think this will help with my application issues.