Jump to content

Joseph Fireborn

Members
  • Posts

    2,688
  • Joined

  • Last visited

3 Followers

About Joseph Fireborn

  • Birthday 08/12/1984

Profile Information

  • Location
    Georgia

Recent Profile Visitors

31,434 profile views

Joseph Fireborn's Achievements

Advanced Member

Advanced Member (3/3)

1.4k

Reputation

Single Status Update

See all updates by Joseph Fireborn

  1. Testing a new glaze firing schedule. Trying to rid myself of microdimples when working with good ole GB.

    1. Show previous comments  2 more
    2. Crusty

      Crusty

      i found a firing schedule from Perry at Skutt for ^5, just take it to your cone temp.. ill try to post it in my gallery..

       

       

    3. Crusty

      Crusty

      segment 1 rate 200 Temp 250 hold none

       

      Segment 2 Rate 400 Temp 1000 no hold

       

      Segment

       

      Segment 3 Rate 180 Temp 1150 no hold = adjust if you are need/want more burn off..

       

      Segment 4 Rate 300 Temp 1967 Hold none

       

      Segment 5 120 Temp 2160 {^5} adjustable =Hold 5 minutes

       

      Segment 6 Rate 125 Temp 1900 Hold 45 minutes

    4. Joseph Fireborn
×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.